Abstract

Abstract Through the use of a uniquely constructed molybdenum frame, a completely additive fabrication method may advantageously be employed to form an array of minute interconnecting circuit crossovers directly on the frame, using photolithographic and plating processes, with the requisite arches of the crossovers being directly formed within specially configured grooves of the frame during the plating operation. The frame is thereafter initially used as a temporary crossover carrier member, and subsequently as a bonding member during the thermo-compression bonding of the individual crossovers to respectively associated bond sites of the circuit, which typically may be of the integrated thin or thick film type. Such a simplified additive crossover generating technique advantageously obviates the need of not only potentially circuit-damaging chemical etching operations, but the many associated processing and handling steps associated therewith.

Inventors

  • 👤 Richard P. Debiec
  • 👤 William T. Wydra

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 09:26
CPC Classifications
H; H10; H10W; H10W70/00; H10W70/60; H10W70/62; H10W70/65; H05; H05K; H05K3/00; H05K3/46; H05K3/4685; Y; Y10; Y10T; Y10T29/00; Y10T29/49; Y10T29/49002; Y10T29/49117; Y10T29/49121; Y10T29/49124; Y10T29/49147; Y10T29/49155; Y10T29/49156

Claims Analysis

Total Claims: 18
Claim 1
Independent Claim 130 words
A method of forming a circuit crossover, with an arched intermediate region, for subsequent use in crossing over an intervening circuit element of a substrate-supported circuit, comprising the steps of: forming a mask-defined, exposed area on one planar surface of a frame member such that said exposed area extends across and a predetermined distance beyond opposite sides of a groove, previously formed with a concave base, in the one surface of the frame member; plating said exposed surface area of said frame member to form a metallic crossover, of predetermined thickness, with two planar end regions interconnected by an intermediate arched region, the latter being formed within the concave base of said groove, said completely formed crossover thereafter remaining on the frame member until subsequently transferred to an associated circuit.
Claim 2
Independent Claim 130 words
A method of forming a circuit crossover, with an arched intermediate region, for subsequent use in crossing over an intervening circuit element of a substrate-supported circuit, comprising the steps of: forming a mask-defined, exposed area on one planar surface of a frame member such that said exposed area extends across and a predetermined distance beyond opposite sides of a groove, previously formed with a concave base, in the one surface of the frame member; plating said exposed surface area of said frame member to form a metallic crossover, of predetermined thickness, with two planar end regions interconnected by an intermediate arched region, the latter being formed within the concave base of said groove, said completely formed crossover thereafter remaining on the frame member until subsequently transferred to an associated circuit.
Claim 3
Dependent Claim 29 words
A method in accordance with claim 1 further comprising the step of removing said mask prior to the time when said formed crossover is transferred to an associated circuit.
Claim 4
Dependent Claim 97 words
A method in accordance with claim 1 wherein a predetermined mask-defined, patterned array of exposed areas are formed on said one planar surface of the frame member such that each exposed area extends across and a predetermined distance beyond opposite sides of a different one of a plurality of spaced, parallel extending grooves, previously formed with concave bases, in the one surface of the frame member, and wherein a metallic crossover is plated on each exposed surface area of said frame member so as to simultaneously form an array thereof for subsequent transfer to an associated circuit.
Claim 5
Dependent Claim 36 words
A method in accordance with claim 3 further comprising the step of removing said mask-defined pattern from said frame member prior to the time when said arrray of formed crossovers are transferred to an associated circuit.
Claim 6
Dependent Claim 97 words
A method in accordance with claim 2 further comprising the steps of: aligning the terminating end regions of said plated crossover formed on the frame member with spaced and respectively associated circuit elements forming bond sites of a substrate-supported circuit; bonding the terminating end regions of the crossover to the respectively aligned bond sites of the circuit such that the bond strength between the crossover and the circuit is considerably greater than the plated bond strength initially established between the crossover and the frame member, and removing the frame member from the circuit bonded crossover, for reuse.
Claim 7
Dependent Claim 98 words
A method in accordance with claim 4 further comprising the steps of: aligning the terminating end regions of each of the array of plated crossovers formed on said frame member with spaced and respectively associated bond sites of the circuit; bonding the terminating end regions of each crossover to the respectively aligned bond sites of the circuit such that the bond strength between each crossover and the circuit is considerably greater than the plated bond strength initially established between each crossover and the frame member, and removing the frame member from the array of circuit-bonded crossovers, for reuse.
Claim 8
Dependent Claim 49 words
A method in accordance with claim 6 wherein said mask-defined pattern is formed by a photolithographic process, and wherein said plating step comprises a series of plating operations that form a composite multi-layered crossover, each layer being comprised of a different metallic material, with the outer layer being gold.
Claim 9
Dependent Claim 34 words
A method in accordance with claim 7 wherein said frame member is made of a thin sheet of molybdenum, and said circuit comprises a thin film circuit fabricated on a high alumina ceramic substrate.
Claim 10
Independent Claim 208 words
A method of fabricating an array of circuit crossovers, with arched intermediate regions, on a substrate-supported circuit, comprising the steps of: forming a predetermined mask-defined, patterned array of exposed areas on one surface of a frame member such that each exposed area extends across and a predetermined distance beyond opposite sides of a different one of a plurality of grooves, each previously formed with a concave base, in the one surface of the frame member; plating each exposed surface area of said frame member to form a metallic crossover, of predetermined thickness, with two planar end regions interconnected by an intermediate arched region, the latter being formed within the concave base of each groove; removing said mask-defined pattern from said frame member; aligning the terminating end regions of each of the array of plated crossovers formed on said frame member with spaced and respectively associated bond sites of the circuit; bonding the terminating end regions of each crossover to the respectively aligned bond sites of the circuit such that the bond strength between each crossover and the circuit is considerably greater than the plated bond strength initially established between each crossover and the frame member, and removing the frame member from the array of circuit-bonded crossovers, for reuse.
Claim 11
Independent Claim 208 words
A method of fabricating an array of circuit crossovers, with arched intermediate regions, on a substrate-supported circuit, comprising the steps of: forming a predetermined mask-defined, patterned array of exposed areas on one surface of a frame member such that each exposed area extends across and a predetermined distance beyond opposite sides of a different one of a plurality of grooves, each previously formed with a concave base, in the one surface of the frame member; plating each exposed surface area of said frame member to form a metallic crossover, of predetermined thickness, with two planar end regions interconnected by an intermediate arched region, the latter being formed within the concave base of each groove; removing said mask-defined pattern from said frame member; aligning the terminating end regions of each of the array of plated crossovers formed on said frame member with spaced and respectively associated bond sites of the circuit; bonding the terminating end regions of each crossover to the respectively aligned bond sites of the circuit such that the bond strength between each crossover and the circuit is considerably greater than the plated bond strength initially established between each crossover and the frame member, and removing the frame member from the array of circuit-bonded crossovers, for reuse.
Claim 12
Dependent Claim 17 words
A method in accordance with claim 9 wherein said mask-defined pattern is formed by a photolithographic process.
Claim 13
Dependent Claim 34 words
A method in accordance with claim 10 wherein said frame member is made of a thin sheet of molybdenum, and said circuit comprises a thin film circuit fabricated on a high alumina ceramic substrate.
Claim 14
Dependent Claim 38 words
A method in accordance with claim 9 wherein said plating step comprises a series of plating operations that form composite multi-layered crossovers, each crossover layer being comprised of a different metallic material, with the outer layer being gold.
Claim 15
Dependent Claim 38 words
A method in accordance with claim 9 wherein said crossover plating step involves plating a first layer of nickel, an intermediate layer of copper and an outer exposed layer of gold on each mask-exposed area of said frame.
Claim 16
Dependent Claim 29 words
A method in accordance with claim 12 wherein said crossover plating step further includes the step of plating a thin layer of indium on the outer layer of gold.
Claim 17
Dependent Claim 47 words
A method in accordance with claim 9 wherein said bonding step involves the application of predetermined heat and pressure to said aligned and contacting frame and circuit so as to effect thermo-compression bonds between each of said crossovers and the respectively associated bond sites of said circuit.
Claim 18
Dependent Claim 51 words
A method in accordance with claim 15 wherein a compensating member is interposed between the backside of said circuit substrate and a driving member of a bonder so as to compensate for dimensional variations in said substrate and to, thereby, impart substantially uniform bonding pressure to all of said crossovers simultaneously.

References Cited (Backward Citations)

US2629907A Cited
US3461524A Cited
US3562040A Cited
US3597839A Cited
US3667988A Cited
USB231416I5 Cited
US4000054A Cited
US3729816A Cited
US4054484A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1983-05-06 1983-11-05 1984-05-06 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1987-05-06 1987-11-05 1988-05-06 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1991-05-06 1991-11-05 1992-05-06 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag