Abstract

Abstract A fabrication method is disclosed for providing self-aligned (i.e., misregistration tolerant or "borderless") contact vias for electrical connections between metal interconnection lines and underlying doping semiconductive regions of an integrated circuit. The described method utilizes an oxidation barrier layer material which is patterned twice to provide, first, the recessed oxide isolation regions and, later, the self-aligned contact vias. An example of an n-channel FET embodiment is described wherein self-aligned contact vias are provided between aluminum interconnection lines and n-type doped source and drain regions. In the described method, at least a portion of the normally present misregistration region or border is eliminated between the boundary of a recessed isolation oxide and the boundary of the via. The latter is ultimately coincident with the boundary of an underlying doped region. Elimination of contact borders advantageously reduces the overall area required for the contact, and consequently, reduces the overall surface area of the integrated circuit chip. Additionally, the metal step coverage at the contact edges is improved over prior art etched contact vias. The self-aligned contact via is achieved by repeated patterning of an oxidation barrier coupled with the intermediate step of thermally growing a thick insulation oxide layer over areas wherein devices such as FET's or bipolar transistors will be formed.

Inventors

  • 👤 Robert H. Dennard
  • 👤 Vincent L. Rideout

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-27 15:43
CPC Classifications
H; H10; H10D; H10D30/00; H10D30/01; H10D30/021; H10D30/0223; H10P; H10P14/00; H10P14/60; H10P14/61; H10P76/00; H10P76/40; H10W; H10W10/00; H10W10/01; H10W10/011; H10W10/012; H10W10/0125; H10W10/0126; H10W10/10; H10W10/13

Claims Analysis

Total Claims: 17
Claim 1
Independent Claim 152 words
In a process for fabricating semiconductor integrated circuits on a semiconductor substrate containing at least an oxidation barrier covered region on the surface thereof, said oxidation barrier covered region being formed by patterning and etching an oxidation barrier layer, which steps expose the remainder of said substrate surface, said remainder of said substrate surface being covered with a thermally grown recessed oxide region the latter being formed by thermally oxidizing said remainder of said substrate surface, the steps of: masking a portion of said oxidation barrier, applying an etchant to the unmasked oxidation barrier to etch it away and expose a portion of said substrate surface, reoxidizing said exposed portion of said substrate surface to form insulation oxide therein, removing said portion of said oxidation barrier to expose another portion of said substrate surface and form a via which is self-aligned to only a portion of said thermally grown recessed oxide region.
Claim 2
Dependent Claim 152 words
In a process for fabricating semiconductor integrated circuits on a semiconductor substrate containing at least an oxidation barrier covered region on the surface thereof, said oxidation barrier covered region being formed by patterning and etching an oxidation barrier layer, which steps expose the remainder of said substrate surface, said remainder of said substrate surface being covered with a thermally grown recessed oxide region the latter being formed by thermally oxidizing said remainder of said substrate surface, the steps of: masking a portion of said oxidation barrier, applying an etchant to the unmasked oxidation barrier to etch it away and expose a portion of said substrate surface, reoxidizing said exposed portion of said substrate surface to form insulation oxide therein, removing said portion of said oxidation barrier to expose another portion of said substrate surface and form a via which is self-aligned to only a portion of said thermally grown recessed oxide region.
Claim 3
Dependent Claim 35 words
In a process for fabricating semiconductor integrated circuits according to claim 1 further including the step of: introducing conductive material into said self-aligned via to contact the thus exposed another portion of said substrate surface.
Claim 4
Dependent Claim 59 words
In a process for fabricating semiconductor integrated circuits according to claim 2 wherein the step of introducing conductive material into said self-aligned via to contact the thus-exposed another portion of said substrate surface includes the steps of depositing conductive material in at least said self-aligned via to contact the thus-exposed another portion of said substrate surface and delineating it.
Claim 5
Dependent Claim 18 words
In a process for fabricating semiconductor integrated circuits according to claim 2 wherein said conductive material is aluminum.
Claim 6
Dependent Claim 56 words
In a process for fabricating semiconductor integrated circuits according to claim 1 further including the step of: forming a transistor device after the step of applying an etchant in the exposed said a portion of said substrate surface while retaining said portion of said oxidation barrier in a state unaffected by said transistor device forming step.
Claim 7
Dependent Claim 18 words
In a process for fabricating semiconductor integrated circuits according to claim 1 wherein said semiconductor substrate is silicon.
Claim 8
Dependent Claim 38 words
In a process for fabricating semiconductor integrated circuits according to claim 1 wherein said oxidation barrier is made of a material selected from the group consisting of silicon nitride, aluminum nitride, boron nitride, aluminum oxide and silicon carbide.
Claim 9
Dependent Claim 19 words
In a process for fabricating semiconductor integrated circuits according to claim 1 wherein said oxidation barrier is silicon nitride.
Claim 10
Dependent Claim 39 words
In a process for fabricating semiconductor integrated circuits according to claim 1 wherein said reoxidizing step includes the step of thermally regrowing an oxide of the semiconductor of said semiconductor substrate on said exposed portion of said substrate surface.
Claim 11
Dependent Claim 47 words
In a process for fabricating semiconductor integrated circuits according to claim 1 wherein the step of removing said portion of said oxidation barrier includes the step of etching said portion of said oxidation barrier to form a self-aligned via over said another portion of said substrate surface.
Claim 12
Dependent Claim 26 words
In a process for fabricating semiconductor integrated circuits according to claim 1 further including the step of providing oxide layers above and below said oxidation barrier.
Claim 13
Dependent Claim 55 words
In a process for fabricating semiconductor integrated circuits according to claim 1 further including the step of: forming a memory cell after the step of applying an etchant in the thus-exposed said portion of said substrate surface while retaining said portion of said oxidation barrier in a sate unaffected by said memory cell forming step.
Claim 14
Dependent Claim 49 words
In a process for fabricating semiconductor integrated circuits according to claim 1 further including the step of: forming at least a doped region in said semiconductor substrate the boundary of which is self-aligned to the edges of said thermally grown recessed oxide region and extends beneath said oxidation barrier.
Claim 15
Dependent Claim 32 words
In a process for fabricating semiconductor integrated circuits according to claim 13 wherein the step of forming at least a doped region is carried out after the step of applying an etchant.
Claim 16
Dependent Claim 37 words
In a process for fabricating semiconductor integrated circuits according to claim 13 wherein the step of forming at least a doped region is carried out prior to the step of masking a portion of said oxidation barrier.
Claim 17
Dependent Claim 45 words
In a process for fabricating semiconductor integrated circuits according to claim 1 wherein said self-aligned via has at least a portion elsewhere than where it is self-aligned to only a portion of said thermally grown recessed oxide regions which is bounded by said insulation oxide.

References Cited (Backward Citations)

US3752711A Cited
US3751722A Cited
US3834959A Cited
US3869322A Cited
US3899363A Cited
US4023195A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1983-01-07 1983-07-09 1984-01-08 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1987-01-07 1987-07-09 1988-01-08 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1991-01-07 1991-07-09 1992-01-08 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag