Claims Analysis
Total Claims: 25
Claim 1
Independent Claim
164 words
A method for the production of aluminum in an electrolytic cell containing a halide of said aluminum dissolved in a molten solvent bath of higher decomposition potential, the cell including a plurality of interelectrode spaces between opposed anode and graphite cathode electrode surfaces wherein: (a) said bath is moved through a plurality of said interelectrode spaces where said bath is electrolyzed to deposit molten aluminum at the cathode surface thereof, the bath moving through at least one first interelectrode space at a velocity of 11/2 feet per second or less; (b) said first interelectrode space being provided with a graphite cathode surface which is wetted by said aluminum produced from said bath as it is deposited at said cathode surface; (c) such interelectrode spaces through which said bath moves through a velocity of over 11/2 feet per second are provided with a graphite cathode surface which is not wetted by said aluminum produced from said bath as it is deposited at said cathode surface.
Claim 2
Independent Claim
164 words
A method for the production of aluminum in an electrolytic cell containing a halide of said aluminum dissolved in a molten solvent bath of higher decomposition potential, the cell including a plurality of interelectrode spaces between opposed anode and graphite cathode electrode surfaces wherein: (a) said bath is moved through a plurality of said interelectrode spaces where said bath is electrolyzed to deposit molten aluminum at the cathode surface thereof, the bath moving through at least one first interelectrode space at a velocity of 11/2 feet per second or less; (b) said first interelectrode space being provided with a graphite cathode surface which is wetted by said aluminum produced from said bath as it is deposited at said cathode surface; (c) such interelectrode spaces through which said bath moves through a velocity of over 11/2 feet per second are provided with a graphite cathode surface which is not wetted by said aluminum produced from said bath as it is deposited at said cathode surface.
Claim 3
Dependent Claim
12 words
The method according to claim 1 wherein said halide comprises aluminum chloride.
Claim 4
Dependent Claim
28 words
The method according to claim 1 wherein the bath velocity over said wetted graphite cathode surface in said first interelectrode space is 1/2 to 11/2 feet per second.
Claim 5
Dependent Claim
22 words
The method according to claim 1 wherein said first interlectrode space is greater than 1/2 inch between opposed anode and cathode surfaces.
Claim 6
Dependent Claim
33 words
The method according to claim 1 wherein such interelectrode space through which said bath moves at greater than 11/2 feet per second is 1/2 inch or less between opposed anode and cathode surfaces.
Claim 7
Dependent Claim
47 words
The method according to claim 1 wherein a terminal anode is situated in the upper region of the electrolytic cell and a terminal cathode is in the lower region and wherein substantially horizontal bipolar electrodes therebetween define substantially horizontal interelectrode spaces between opposed anode and cathode surfaces.
Claim 8
Dependent Claim
18 words
The method according to claim 6 wherein said first interelectrode space is situated close to the terminal cathode.
Claim 9
Dependent Claim
22 words
The method according to claim 7 wherein said first interelectrode space is greater than 1/2 inch between opposed anode and cathode surfaces.
Claim 10
Independent Claim
168 words
A method for the production of aluminum in an electrolytic cell containing a chloride of aluminum dissolved in a molten solvent bath of higher decomposition potential, the cell including a plurality of interelectrode spaces between spaced opposed anode and graphite cathode electrode surfaces, comprising: (a) moving a portion of said bath through at least one first interelectrode space at a velocity of 11/2 feet per second or less while electrolyzing said bath in said first interelectrode space to deposit aluminum at the graphite cathode surface for said first interelectrode space, said graphite cathode surface for said first interelectrode space being wetted by said aluminum there deposited; (b) moving a portion of said bath through at least one second interelectrode space at a velocity of greater tha 11/2 feet per second while electrolyzing said bath in said second interelectrode space to deposit aluminum at the graphite cathode surface for said second interelectrode space, said graphite cathode surface for said second interelectrode space being non-wetted by said aluminum there deposited.
Claim 11
Independent Claim
168 words
A method for the production of aluminum in an electrolytic cell containing a chloride of aluminum dissolved in a molten solvent bath of higher decomposition potential, the cell including a plurality of interelectrode spaces between spaced opposed anode and graphite cathode electrode surfaces, comprising: (a) moving a portion of said bath through at least one first interelectrode space at a velocity of 11/2 feet per second or less while electrolyzing said bath in said first interelectrode space to deposit aluminum at the graphite cathode surface for said first interelectrode space, said graphite cathode surface for said first interelectrode space being wetted by said aluminum there deposited; (b) moving a portion of said bath through at least one second interelectrode space at a velocity of greater tha 11/2 feet per second while electrolyzing said bath in said second interelectrode space to deposit aluminum at the graphite cathode surface for said second interelectrode space, said graphite cathode surface for said second interelectrode space being non-wetted by said aluminum there deposited.
Claim 12
Dependent Claim
28 words
The method according to claim 9 wherein the bath velocity over said wetted graphite cathode surface in said first interelectrode space is 1/2 to 11/2 feet per second.
Claim 13
Dependent Claim
22 words
The method according to claim 9 wherein said first interelectrode space is greater than 1/2 inch between opposed anode and cathode surfaces.
Claim 14
Dependent Claim
22 words
The method according to claim 9 wherein said second interelectrode space is 1/2 inch or less between opposed anode and cathode surfaces.
Claim 15
Dependent Claim
47 words
The method according to claim 9 wherein a terminal anode is situated in the upper region of the electrolytic cell and a terminal cathode is in the lower region and wherein substantially horizontal bipolar electrodes therebetween define substantially horizontal interelectrode spaces between opposed anode and cathode surfaces.
Claim 16
Dependent Claim
22 words
The method according to claim 13 wherein said first interelectrode space is closer to the terminal cathode than said second interelectrode space.
Claim 17
Dependent Claim
22 words
The method according to claim 14 wherein said first interelectrode space is greater than 1/2 inch between opposed anode and cathode surfaces.
Claim 18
Independent Claim
154 words
A method for the production of aluminum in an electrolytic cell containing a halide of aluminum dissolved in a molten solvent bath of higher decomposition potential, the cell including a plurality of interelectrode spaces between opposed spaced anode and graphite cathode electrode surface comprising: (a) moving said bath through at least one such interelectrode space at a relatively low velocity, the distance between the anode and cathode surfaces defining said space being greater than 1/2 inch, the graphite cathode surface of said interelectrode space being wetted by said aluminum there deposited by electrolysis from said bath in said space; (b) moving said bath through at least one such interelectrode space at a relatively high velocity, the distance between the anode and cathode surfaces defining said space being 1/2 inch or less, the graphite cathode surface of said interelectrode space being non-wetted by said aluminum there deposited by electrolysis from said bath in said space.
Claim 19
Independent Claim
154 words
A method for the production of aluminum in an electrolytic cell containing a halide of aluminum dissolved in a molten solvent bath of higher decomposition potential, the cell including a plurality of interelectrode spaces between opposed spaced anode and graphite cathode electrode surface comprising: (a) moving said bath through at least one such interelectrode space at a relatively low velocity, the distance between the anode and cathode surfaces defining said space being greater than 1/2 inch, the graphite cathode surface of said interelectrode space being wetted by said aluminum there deposited by electrolysis from said bath in said space; (b) moving said bath through at least one such interelectrode space at a relatively high velocity, the distance between the anode and cathode surfaces defining said space being 1/2 inch or less, the graphite cathode surface of said interelectrode space being non-wetted by said aluminum there deposited by electrolysis from said bath in said space.
Claim 20
Independent Claim
168 words
A method for the production of aluminum in an electrolytic cell by electrolysis of a halide of aluminum dissolved in a molten solvent bath of higher decomposition potential, the cell including a terminal anode in its upper region, a terminal cathode in its lower region, and a plurality of substantially horizontal bipolar graphite electrodes therebetween and a plurality of substantially horizontal interelectrode spaces between opposed anode and cathode electrode surfaces comprising: (a) moving said bath through at least one first interelectrode space at a velocity of 11/2 feet per second or less, said interelectrode space having a graphite cathode surface which is wetted by said aluminum; (b) moving said bath through at least one second interelectrode space at a velocity of over 11/2 feet per second, said interelectrode space having a graphite cathode surface which is nonwetted by said aluminum; (c) said first interelectrode space being situated closer to the terminal cathode and having a greater distance separating opposed anode and cathode spaces than said second interelectrode space.
Claim 21
Independent Claim
168 words
A method for the production of aluminum in an electrolytic cell by electrolysis of a halide of aluminum dissolved in a molten solvent bath of higher decomposition potential, the cell including a terminal anode in its upper region, a terminal cathode in its lower region, and a plurality of substantially horizontal bipolar graphite electrodes therebetween and a plurality of substantially horizontal interelectrode spaces between opposed anode and cathode electrode surfaces comprising: (a) moving said bath through at least one first interelectrode space at a velocity of 11/2 feet per second or less, said interelectrode space having a graphite cathode surface which is wetted by said aluminum; (b) moving said bath through at least one second interelectrode space at a velocity of over 11/2 feet per second, said interelectrode space having a graphite cathode surface which is nonwetted by said aluminum; (c) said first interelectrode space being situated closer to the terminal cathode and having a greater distance separating opposed anode and cathode spaces than said second interelectrode space.
Claim 22
Dependent Claim
28 words
The method according to claim 17 wherein the bath velocity over said wetted graphite cathode surface in said first interelectrode space is 1/2 to 11/2 feet per second.
Claim 23
Dependent Claim
22 words
The method according to claim 17 wherein said first interelectrode space is greater than 1/2 inch between opposed anode and cathode surfaces.
Claim 24
Dependent Claim
22 words
The method according to claim 17 wherein said second interelectrode space is 1/2 inch or less between opposed anode and cathode surfaces.
Claim 25
Dependent Claim
12 words
The method according to claim 17 wherein said halide comprises aluminum chloride.