US4121983A Expired / Lapsed US ⏱️ 0.0 years remaining

Metal production

Assignee: Alcoa Corp
•
Filing: 1977-12-21
•
Granted: 1978-10-24
•
Expires: 1997-12-21
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A process is provided for producing aluminum in an electrolytic cell containing aluminum chloride dissolved in a molten solvent of higher decomposition potential. The cell has a terminal anode, a terminal cathode and a bipolar electrode arranged to operate with the anode and the cathode, providing interelectrode spaces therebetween. On electrolyzing the cell chlorine is produced on each anode surface thereof and aluminum on each cathode surface, the aluminum being swept from the cathode surface by bath material. In the process, carbonaceous material is provided for use as the electrode. The direction of grain flow constituting the carbonaceous material is determined and the electrode is arranged in the cell such that the direction of electrolysis current flow through the cell is in a direction substantially perpendicular to the direction of grain flow in the electrode.

Inventors

  • 👤 Donald L. Kinosz
  • 👤 Subodh K. Das
  • 👤 Robert L. Coffman

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-28 21:07
CPC Classifications
C; C25; C25C; C25C3/00; C25C3/06; C25C3/08; C25C7/00; C25C7/02; C25C7/025

Claims Analysis

Total Claims: 15
Claim 1
Independent Claim 133 words
A process for producing metal in an electrolytic cell containing metal halide dissolved in a molten solvent of higher decomposition potential, the cell having a terminal anode, a terminal cathode and at least one bipolar electrode arranged to operate with the anode and the cathode providing inter-electrode spaces therebetween, the process which comprises the steps of: (a) providing at least one electrode comprised of carbonaceous material; (b) determining the direction of grain flow in the carbonaceous material constituting the electrode; (c) arranging said electrode in said cell such that the direction of electrolyzing current flow through the cell is in a direction substantially perpendicular to the direction of grain flow in the electrode; and (d) electrolyzing the cell, thereby producing halogen gas on each anode surface thereof and metal on each cathode surface.
Claim 2
Dependent Claim 133 words
A process for producing metal in an electrolytic cell containing metal halide dissolved in a molten solvent of higher decomposition potential, the cell having a terminal anode, a terminal cathode and at least one bipolar electrode arranged to operate with the anode and the cathode providing inter-electrode spaces therebetween, the process which comprises the steps of: (a) providing at least one electrode comprised of carbonaceous material; (b) determining the direction of grain flow in the carbonaceous material constituting the electrode; (c) arranging said electrode in said cell such that the direction of electrolyzing current flow through the cell is in a direction substantially perpendicular to the direction of grain flow in the electrode; and (d) electrolyzing the cell, thereby producing halogen gas on each anode surface thereof and metal on each cathode surface.
Claim 3
Dependent Claim 16 words
The process according to claim 1 wherein the electrode in step (a) is a bipolar electrode.
Claim 4
Dependent Claim 25 words
The process according to claim 1 wherein the electrode in step (a) has a density in the range of 1400 to 2000 kg/m 3 .
Claim 5
Dependent Claim 25 words
The process according to claim 1 wherein the electrode in step (a) has a density in the range of 1700 to 1880 kg/m 3 .
Claim 6
Dependent Claim 34 words
The process according to claim 1 wherein the carbonaceous material in the electrode in step (a) has a grain size in the range of 1.0 × 10 -6 to 1.0 × 10 -2 m.
Claim 7
Dependent Claim 36 words
The process according to claim 1 wherein the carbonaceous material in the electrode in step (a) has a coefficient of thermal expansion in the range of 1.0 × 10 -6 to 7.0 × 10 -6 in/in/°C.
Claim 8
Dependent Claim 25 words
The method according to claim 1 wherein the carbonaceous material in step (a) has an ash content in the range of 0.02 to 3.0 wt.%.
Claim 9
Dependent Claim 31 words
The method according to claim 1 wherein the carbonaceous material in step (a) has an electrical resistivity in the direction of grain flow in the range of 5.0 to 30 μΩm.
Claim 10
Dependent Claim 209 words
A process for producing aluminum in an electrolytic cell containing aluminum chloride dissolved in a molten solvent of higher decomposition potential, the cell having a terminal anode, a terminal cathode and at least one bipolar electrode arranged to operate with the anode and the cathode providing inter-electrode spaces therebetween, the process which comprises the steps of: (a) providing at least one electrode comprised of carbonaceous material having a density in the range of 1400 to 2000 kg/m 3 , a grain size in the range of 2.0 × 10 -6 to 6.6 to 10 -3 m, a coefficient of thermal expansion of 1.0 × 10 -6 to 7.0 × 10 -6 in/in/°C., an ash content of 0.02 to 3.0 wt.% and an electrical resistance in the range of 5.0 to 30 μΩm; (b) determining the direction of grain flow in the carbonaceous material constituting the electrode; (c) arranging said electrode in said cell such that the direction of electrolyzing current flow through the cell is in a direction substantially perpendicular to the direction of grain flow in the electrode; and (d) electrolyzing the cell, thereby producing chlorine on each anode surface thereof and aluminum on each cathode surface, the aluminum being swept from the cathode surface by bath material.
Claim 11
Dependent Claim 209 words
A process for producing aluminum in an electrolytic cell containing aluminum chloride dissolved in a molten solvent of higher decomposition potential, the cell having a terminal anode, a terminal cathode and at least one bipolar electrode arranged to operate with the anode and the cathode providing inter-electrode spaces therebetween, the process which comprises the steps of: (a) providing at least one electrode comprised of carbonaceous material having a density in the range of 1400 to 2000 kg/m 3 , a grain size in the range of 2.0 × 10 -6 to 6.6 to 10 -3 m, a coefficient of thermal expansion of 1.0 × 10 -6 to 7.0 × 10 -6 in/in/°C., an ash content of 0.02 to 3.0 wt.% and an electrical resistance in the range of 5.0 to 30 μΩm; (b) determining the direction of grain flow in the carbonaceous material constituting the electrode; (c) arranging said electrode in said cell such that the direction of electrolyzing current flow through the cell is in a direction substantially perpendicular to the direction of grain flow in the electrode; and (d) electrolyzing the cell, thereby producing chlorine on each anode surface thereof and aluminum on each cathode surface, the aluminum being swept from the cathode surface by bath material.
Claim 12
Dependent Claim 137 words
In a process for producing aluminum in an electrolytic cell containing aluminum chloride dissolved in a molten solvent of higher decomposition potential, the cell having a terminal anode, a terminal cathode and a bipolar electrode arranged to operate with the anode and the cathode providing inter-electrode spaces therebetween, wherein chlorine is produced on each anode surface thereof and aluminum on each cathode surface by electrolyzing the cell, the aluminum being swept from the cathode surface by bath material, the process wherein the improvement comprises utilizing an electrode comprised by carbonaceous material wherein the direction of grain flow constituting the carbonaceous material has been determined and the electrode is arranged in the cell such that the direction of current flow through the cell is in a direction substantially perpendicular to the flow of the grains in the electrode.
Claim 13
Dependent Claim 137 words
In a process for producing aluminum in an electrolytic cell containing aluminum chloride dissolved in a molten solvent of higher decomposition potential, the cell having a terminal anode, a terminal cathode and a bipolar electrode arranged to operate with the anode and the cathode providing inter-electrode spaces therebetween, wherein chlorine is produced on each anode surface thereof and aluminum on each cathode surface by electrolyzing the cell, the aluminum being swept from the cathode surface by bath material, the process wherein the improvement comprises utilizing an electrode comprised by carbonaceous material wherein the direction of grain flow constituting the carbonaceous material has been determined and the electrode is arranged in the cell such that the direction of current flow through the cell is in a direction substantially perpendicular to the flow of the grains in the electrode.
Claim 14
Dependent Claim 201 words
In a process for producing aluminum in an electrolytic cell containing aluminum chloride dissolved in a molten solvent of higher decomposition potential, the cell having a terminal anode, a terminal cathode and a bipolar electrode arranged to operate with the anode and the cathode providing inter-electrode spaces therebetween, wherein chlorine is produced on each anode surface thereof and aluminum on each cathode surface by electrolyzing the cell, the aluminum being swept from the cathode surface by bath material, the process wherein the improvement comprises utilizing an electrode comprised of carbonaceous material wherein the direction of grain flow constituting the carbonaceous material has been determined and the electrode is arranged in the cell such that the direction of current flow through the cell is in a direction substantially perpendicular to the flow of the grains in the electrode, the carbonaceous material characterized by having a density in the range of 1550 to 1900 kg/m 3 , a grain size in the range of 2.0 × 10 -6 to 6.6 × 10 -3 m, a coefficient of thermal expansion of 1.5 × 10 -6 to 6.0 × 10 -6 in/in/° C. and an ash content in the range of 0.02 to 3.0 wt.%.
Claim 15
Dependent Claim 201 words
In a process for producing aluminum in an electrolytic cell containing aluminum chloride dissolved in a molten solvent of higher decomposition potential, the cell having a terminal anode, a terminal cathode and a bipolar electrode arranged to operate with the anode and the cathode providing inter-electrode spaces therebetween, wherein chlorine is produced on each anode surface thereof and aluminum on each cathode surface by electrolyzing the cell, the aluminum being swept from the cathode surface by bath material, the process wherein the improvement comprises utilizing an electrode comprised of carbonaceous material wherein the direction of grain flow constituting the carbonaceous material has been determined and the electrode is arranged in the cell such that the direction of current flow through the cell is in a direction substantially perpendicular to the flow of the grains in the electrode, the carbonaceous material characterized by having a density in the range of 1550 to 1900 kg/m 3 , a grain size in the range of 2.0 × 10 -6 to 6.6 × 10 -3 m, a coefficient of thermal expansion of 1.5 × 10 -6 to 6.0 × 10 -6 in/in/° C. and an ash content in the range of 0.02 to 3.0 wt.%.

References Cited (Backward Citations)

US1569606A Cited
US4046650A Cited
US3822195A Cited
US3960696A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1981-10-23 1982-04-24 1982-10-24 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1985-10-23 1986-04-24 1986-10-24 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1989-10-23 1990-04-24 1990-10-24 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag