Pyrolytic deposition of silicon dioxide on semiconductors using a shrouded boat
Assignee: Motorola Solutions Inc
•
Filing: 1976-06-07
•
Granted: 1978-07-04
•
Expires: 1996-06-07
Abstract
Abstract Silicon dioxide is pyrolytically deposited by the reaction of silane with oxygen on vertically mounted substrates in an evacuated system. A standard diffusion furnace equipped with a furnace tube which is vacuum tight is used. Injection tubes having multiple injection ports are positioned within the furnace tube to distribute the silane and the oxygen uniformly across a plurality of substrates which are positioned perpendicular to the furnace tube axis in a boat covered with a perforated shroud. The process is particularly useful in providing for the low temperature deposition of uniform layers of silicon dioxide on silicon wafers to be used in the fabrication of semiconductor devices.
Inventors
- 👤 Robert Stanley Alberti
- 👤 Jon Charles Goldman
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-01 21:45
CPC Classifications
H; H10; H10P; H10P14/00; H10P14/60; H10P14/69; H10P14/692; H10P14/6921; H10P14/6922; H10P14/6923; C; C23; C23C; C23C16/00; C23C16/22; C23C16/30; C23C16/40; C23C16/401; C23C16/402; C23C16/44; C23C16/458; C23C16/4582; C23C16/4587; H10P14/63; H10P14/6326; H10P14/6328; H10P14/6334; H10P14/66; H10P14/668; H10P14/6681; H10P14/6682; H10P14/69215; Y; Y10; Y10S; Y10S118/00; Y10S118/90
Claims Analysis
Total Claims: 13
Claim 1
Independent Claim
154 words
A method for pyrolytically depositing silicon dioxide on the surfaces of semiconductor substrates comprising the steps of: (a) loading said substrates in a boat; (b) surrounding said boat with a cylindrical shroud of perforated metal; (c) positioning said shrouded boat in the interior region of a furnace tube such that broad surfaces of said substrates are perpendicular to the longitudinal axis of said furnace tube and the cylindrical axis of said shroud is in the same direction as said longitudinal axis; (d) heating said substrate; (e) evacuating said furnace tube; and (f) injecting oxygen and reactant gas comprising silane into said evacuated furnace tube, each through separate injection tubes positioned in said interior region with said injection tubes having multiple ports located adjacent said shrouded boat to restrict the injection to occur in the vicinity of said shrouded boat and to enhance the mixing of said oxygen and said reactant gas in said vicinity.
Claim 2
Independent Claim
154 words
A method for pyrolytically depositing silicon dioxide on the surfaces of semiconductor substrates comprising the steps of: (a) loading said substrates in a boat; (b) surrounding said boat with a cylindrical shroud of perforated metal; (c) positioning said shrouded boat in the interior region of a furnace tube such that broad surfaces of said substrates are perpendicular to the longitudinal axis of said furnace tube and the cylindrical axis of said shroud is in the same direction as said longitudinal axis; (d) heating said substrate; (e) evacuating said furnace tube; and (f) injecting oxygen and reactant gas comprising silane into said evacuated furnace tube, each through separate injection tubes positioned in said interior region with said injection tubes having multiple ports located adjacent said shrouded boat to restrict the injection to occur in the vicinity of said shrouded boat and to enhance the mixing of said oxygen and said reactant gas in said vicinity.
Claim 3
Dependent Claim
20 words
The method of claim 1 wherein said reactant gases further comprise phosphine such that phosphorous doped silicon dioxide is deposited.
Claim 4
Dependent Claim
22 words
The method of claim 2 wherein said heating of said substrate is to a temperature from about 400° to about 500° C.
Claim 5
Dependent Claim
20 words
The method of claim 1 wherein said reactant gases further comprise diborane such that boron doped silicon dioxide is deposited.
Claim 6
Dependent Claim
22 words
The method of claim 4 wherein said heating of said substrate is to a temperature from about 400° to about 500° C.
Claim 7
Independent Claim
110 words
A method for the pyrolytic deposition of silicon dioxide upon a substrate mounted vertically with respect to the longitudinal axis of a furnace tube which comprises contacting a mixture of silane and oxygen with said vertically mounted substrate which is positioned in a boat surrounded by a shroud of perforated metal located in said furnace tube in a vacuum at an elevated temperature wherein said mixture of silane and oxygen is formed by injecting said silane through a first injection tube and injecting said oxygen through a second injection tube and wherein said first and second injection tubes restrict said injecting to the vicinity of said substrate within said vacuum.
Claim 8
Independent Claim
110 words
A method for the pyrolytic deposition of silicon dioxide upon a substrate mounted vertically with respect to the longitudinal axis of a furnace tube which comprises contacting a mixture of silane and oxygen with said vertically mounted substrate which is positioned in a boat surrounded by a shroud of perforated metal located in said furnace tube in a vacuum at an elevated temperature wherein said mixture of silane and oxygen is formed by injecting said silane through a first injection tube and injecting said oxygen through a second injection tube and wherein said first and second injection tubes restrict said injecting to the vicinity of said substrate within said vacuum.
Claim 9
Dependent Claim
17 words
The method of claim 6 wherein a temperature from about 400° to about 500° C. is employed.
Claim 10
Dependent Claim
18 words
The method of claim 5 wherein a vacuum of about 300 millitorr to about 10 torr is employed.
Claim 11
Dependent Claim
19 words
The method of claim 6 wherein said mixture further comprises phosphine such that said silicon dioxide is phosphorous doped.
Claim 12
Dependent Claim
26 words
The method of claim 6 wherein said first and said second injecting tubes have multiple injection ports through which said silane and said oxygen are injected.
Claim 13
Dependent Claim
57 words
The method of claim 10 wherein said multiple injection ports of said first and said second injection tubes face the longitudinal centerline of said furnace tube whereby said perforated shroud, said first and said second injection tubes, and said furnace tube create a fluid flow environment which enhances the mixing of said mixture of silane and oxygen.
References Cited (Backward Citations)
US3098763A
Cited
US3481781A
Cited
US3598082A
Cited
US3706597A
Cited
US4018183A
Cited
US3854443A
Cited
US3900597A
Cited
US3934060A
Cited
US4005240A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1981-07-03 | 1982-01-02 | 1982-07-04 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1985-07-03 | 1986-01-02 | 1986-07-04 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1989-07-03 | 1990-01-02 | 1990-07-04 | $7700.00 | Window Closed / Lapsed |