← Back to Patent Explorer
US4048347A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of coating lamp envelope with heat reflecting filter

Assignee: GTE Sylvania Inc
•
Filing: 1976-11-24
•
Granted: 1977-09-13
•
Expires: 1996-11-24
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A dichroic coating is deposited on a cylindrical lamp envelope from an evaporation source while the envelope is heated and rotated. The thickness of the coating is monitored by measuring the intensity of light beamed on and reflected from a flat plate in line of sight with the evaporation source.

Inventors

  • 👤 Martin P. Schrank
  • 👤 Richard M. Coppola

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-07 05:32
CPC Classifications
C; C23; C23C; C23C14/00; C23C14/22; C23C14/54; C23C14/542; C23C14/545; C23C14/547; C03; C03C; C03C17/00; C03C17/34; C03C17/3411; C03C17/3417; H; H01; H01K; H01K3/00; H01K3/005

Claims Analysis

Total Claims: 3
Claim 1
Independent Claim 150 words
The method of depositing a dichroic coating on the tubular envelope of an incandescent lamp comprising the steps of disposing said envelope in an evacuable bell jar and in line of sight with an evaposating source therein; evacuating said bell jar; heating and rotating said envelope while two different materials are alternately evaporated and deposited on the envelope, the envelope being heated during deposition to a temperature of at least about 300° C by energizing the lamp filament; and monitoring the thickness of said coating by beaming light on a plate located in the bell jar in line of sight with the evaporating source, recording the intensity of light reflected from said plate, determining the thickness of coating on said plate by means of said intensity of reflected light and multiplying said thickness of coating on said plate by a predetermined ratio to determine the coating thickness on said envelope.
Claim 2
Independent Claim 150 words
The method of depositing a dichroic coating on the tubular envelope of an incandescent lamp comprising the steps of disposing said envelope in an evacuable bell jar and in line of sight with an evaposating source therein; evacuating said bell jar; heating and rotating said envelope while two different materials are alternately evaporated and deposited on the envelope, the envelope being heated during deposition to a temperature of at least about 300° C by energizing the lamp filament; and monitoring the thickness of said coating by beaming light on a plate located in the bell jar in line of sight with the evaporating source, recording the intensity of light reflected from said plate, determining the thickness of coating on said plate by means of said intensity of reflected light and multiplying said thickness of coating on said plate by a predetermined ratio to determine the coating thickness on said envelope.
Claim 3
Dependent Claim 25 words
The method of claim 1 wherein the dichroic coating comprises Ti0 2 and Si0 2 and oxygen is admitted to the bell jar during deposition.

References Cited (Backward Citations)

US2920002A Cited
US2784115A Cited
US3225243A Cited
US3188513A Cited
US3650815A Cited
US3637294A Cited
US3752691A Cited
US3926508A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1980-09-12 1981-03-14 1981-09-13 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1984-09-12 1985-03-14 1985-09-13 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1988-09-12 1989-03-14 1989-09-13 $7700.00 Window Closed / Lapsed