Claims Analysis
Total Claims: 10
Claim 1
Independent Claim
72 words
In a process for imparting durable-press properties to cellulosic textiles, said process of the type wherein the textile is impregnated with an aqueous formulation containing a formaldehyde-amide adduct crosslinking agent and aluminum chlorhydroxide catalyst, and is dried and cured, the improvement characterized by: adding hydrogen peroxide to the formulation to provide a more efficient, activated catalyst system that promotes the finishing reaction through synergistic interaction of the aluminum chlorhydroxide and hydrogen peroxide.
Claim 2
Dependent Claim
72 words
In a process for imparting durable-press properties to cellulosic textiles, said process of the type wherein the textile is impregnated with an aqueous formulation containing a formaldehyde-amide adduct crosslinking agent and aluminum chlorhydroxide catalyst, and is dried and cured, the improvement characterized by: adding hydrogen peroxide to the formulation to provide a more efficient, activated catalyst system that promotes the finishing reaction through synergistic interaction of the aluminum chlorhydroxide and hydrogen peroxide.
Claim 3
Dependent Claim
89 words
An improved process for imparting durable-press properties to cotton and other cellulose-containing textiles, the process comprising: a. impregnating a textile which contains at least 50% cellulose with an aqueous formulation consisting of: 1. about 7-a 20%, by weight, of a formaldehydeamide adduct crosslinking agent, 2. about from 0.35% to 1.75%, by weight (about 2 to 10 mmol. per 100 g. of formulation), of aluminum chlorhydroxide, 3. an amount of hydrogen peroxide so that the molar ratio of aluminum chlorhydroxide to hydrogen peroxide is about from 1:4 to 1:0.25, and
Claim 4
Dependent Claim
89 words
An improved process for imparting durable-press properties to cotton and other cellulose-containing textiles, the process comprising: a. impregnating a textile which contains at least 50% cellulose with an aqueous formulation consisting of: 1. about 7-a 20%, by weight, of a formaldehydeamide adduct crosslinking agent, 2. about from 0.35% to 1.75%, by weight (about 2 to 10 mmol. per 100 g. of formulation), of aluminum chlorhydroxide, 3. an amount of hydrogen peroxide so that the molar ratio of aluminum chlorhydroxide to hydrogen peroxide is about from 1:4 to 1:0.25, and
Claim 5
Dependent Claim
28 words
water, as the remainder of the formulation, and b. drying and curing the wet impregnated textile of (a) by heat treatment, to obtain durable press-properties in the textile.
Claim 6
Dependent Claim
28 words
water, as the remainder of the formulation, and b. drying and curing the wet impregnated textile of (a) by heat treatment, to obtain durable press-properties in the textile.
Claim 7
Dependent Claim
27 words
The process of claim 2 wherein a flash-curing step is achieved by heat treatment at about from 175° to 215° C. for about 10 to 45 seconds.
Claim 8
Dependent Claim
23 words
The process of claim 2 wherein curing is achieved by heat treatment at about from 120° to 175° C. for about 3 minutes.
Claim 9
Dependent Claim
14 words
The process of claim 2 wherein the formaldehydeamide adduct crosslinking agent is dimethylol dihydroxyethyleneurea.
Claim 10
Dependent Claim
15 words
The process of claim 2 wherein the formaldehydeamide adduct crosslinking agent is dimethylol methyl carbamate.