Patent US3042494A successfully refreshed from Google Patents.
← Back to Patent Explorer
US3042494A Expired / Lapsed US ⏱️ 0.0 years remaining

Method for producing highest-purity silicon for electric semiconductor devices

Assignee: Siemens Schuckertwerke AG
•
Filing: 1958-05-23
•
Granted: 1962-07-03
•
Expires: 1978-05-23
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Gutsche Heinrich

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-23 18:15
CPC Classifications
H; H10; H10P; H10P14/00; H10P14/20; H10P14/34; H10P14/3402; H10P14/3404; H10P14/3411; C; C01; C01B; C01B33/00; C01B33/02; C01B33/021; C01B33/027; C01B33/035; C23; C23C; C23C16/00; C23C16/06; C23C16/22; C30; C30B; C30B13/00; C30B25/00; C30B25/02; C30B33/00; H10P14/24; H10P95/00; Y; Y02; Y02T; Y02T50/00; Y02T50/60

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 134 words
IN A METHOD OF PRODUCING SILICON OF HIGH PURITY, FOR USE IN ELECTRICAL SEMICONDUCTING DEVICES, IN WHICH METHOD SILICON IS PRECIPITATED ONTO A HOT CARRIER BODY OF SILICON BY GAS-PHSES CHEMICAL CONVERSION OF A HALOGEN COMPOUND OF SILICON BY CONTACT THEREOF WITH THE HOT BOODY, THE IMPROVEMENT COMPRISIING CARRYING OUT SAID METHOD IN AN AT LEAST PARTLY TRANSPARENT REACTION VESSEL AT LEAST PARTLY COMPRISED OF A SILICEOUS MATERIAL OF THE GROUP CONSISTING OF GLASS AND QUARTZ, THE HOT BODY BEING HEATED TO ABOUT 1100* TO 1200* C. BY PASSAGE OF AN ELECTRIC CURRENT THERETHROUGH, AND MAINTAINING THE TEMPERATURE OF THE INNER WALLS OF THE VESSEL AT BETWEEEN ABOUT 300*C. AND 800*C. DURING THE PRECIPITATION PERIOD, TO MINIMIZE FORMATION OF A COATING OF HIGH MOLECULAR WEIGHT SILICON HALOGENIDE ON THE SURFACE OF THE REACTION VESSEL.
Claim 2
Dependent Claim 134 words
IN A METHOD OF PRODUCING SILICON OF HIGH PURITY, FOR USE IN ELECTRICAL SEMICONDUCTING DEVICES, IN WHICH METHOD SILICON IS PRECIPITATED ONTO A HOT CARRIER BODY OF SILICON BY GAS-PHSES CHEMICAL CONVERSION OF A HALOGEN COMPOUND OF SILICON BY CONTACT THEREOF WITH THE HOT BOODY, THE IMPROVEMENT COMPRISIING CARRYING OUT SAID METHOD IN AN AT LEAST PARTLY TRANSPARENT REACTION VESSEL AT LEAST PARTLY COMPRISED OF A SILICEOUS MATERIAL OF THE GROUP CONSISTING OF GLASS AND QUARTZ, THE HOT BODY BEING HEATED TO ABOUT 1100* TO 1200* C. BY PASSAGE OF AN ELECTRIC CURRENT THERETHROUGH, AND MAINTAINING THE TEMPERATURE OF THE INNER WALLS OF THE VESSEL AT BETWEEEN ABOUT 300*C. AND 800*C. DURING THE PRECIPITATION PERIOD, TO MINIMIZE FORMATION OF A COATING OF HIGH MOLECULAR WEIGHT SILICON HALOGENIDE ON THE SURFACE OF THE REACTION VESSEL.

References Cited (Backward Citations)

US1019392A Cited
US1601931A Cited
US1671213A Cited
US1829756A Cited
US2441603A Cited
US2654657A Cited
US2753280A Cited
US2763581A Cited
US2804377A Cited
US2851342A Cited
US2909411A Cited
US2912311A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1965-07-02 1966-01-01 1966-07-03 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1969-07-02 1970-01-01 1970-07-03 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1973-07-02 1974-01-01 1974-07-03 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag