Fabrication method of semiconductor integrated circuit device
Assignee: NEC Electronics Corp
•
Filing: 2002-07-16
•
Granted: 2003-12-02
•
Expires: 2022-07-16
Abstract
Abstract A pattern accuracy of a semiconductor integrated circuit device is to be improved. When an ordinary photomask is to be replaced with a resist mask, in setting a planar size of a shielding pattern formed by resist film, a correction quantity L is subtracted from a planar size of a corresponding shielding pattern formed of metal. Conversely, when the resist mask is to be replaced with the ordinary mask, in setting a planar size of the shielding pattern formed of metal, the correction quantity L is added to the planar size of the corresponding shielding pattern formed by resist film.
Inventors
- 👤 Shoji Hotta
- 👤 Norio Hasegawa
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-07 17:47
CPC Classifications
G; G03; G03F; G03F1/00; G03F1/36; H; H10; H10P; H10P76/00; G03F1/54; G03F1/56
Claims Analysis
Total Claims: 21
Claim 1
Independent Claim
172 words
A method of fabricating a semiconductor integrated circuit device, comprising the steps of: (a) providing a first photomask having a first light-shielding film having a first thickness, said first light-shielding film having first light-transmitting portions and first light-shielding portions arranged to produce a first predetermined projected exposure pattern corresponding to an integrated circuit, said first light-shielding portions having first transverse dimensions; (b) making a projection exposure through said first photomask onto a first photosensitive substrate; (c) providing a second photomask having a second light-shielding film having a second thickness different from said first thickness, said second light-shielding film having second light-transmitting portions and second light-shielding portions arranged to produce a second predetermined projected exposure pattern corresponding to said integrated circuit, said second light-shielding portions having second transverse dimensions different from said first transverse dimensions; and (d) making a projection exposure through said second photomask onto a second photosensitive substrate; wherein said second transverse dimensions are selected such that said second photomask produces essentially the same projection exposure pattern as said first photomask.
Claim 2
Independent Claim
172 words
A method of fabricating a semiconductor integrated circuit device, comprising the steps of: (a) providing a first photomask having a first light-shielding film having a first thickness, said first light-shielding film having first light-transmitting portions and first light-shielding portions arranged to produce a first predetermined projected exposure pattern corresponding to an integrated circuit, said first light-shielding portions having first transverse dimensions; (b) making a projection exposure through said first photomask onto a first photosensitive substrate; (c) providing a second photomask having a second light-shielding film having a second thickness different from said first thickness, said second light-shielding film having second light-transmitting portions and second light-shielding portions arranged to produce a second predetermined projected exposure pattern corresponding to said integrated circuit, said second light-shielding portions having second transverse dimensions different from said first transverse dimensions; and (d) making a projection exposure through said second photomask onto a second photosensitive substrate; wherein said second transverse dimensions are selected such that said second photomask produces essentially the same projection exposure pattern as said first photomask.
Claim 3
Dependent Claim
29 words
The method according to claim 1 , wherein said projection exposures are made using a KrF excimer laser beam having a wavelength of 248 nm as a light source.
Claim 4
Dependent Claim
15 words
The method according to claim 1 , wherein said photosensitive substrates are photoresist-coated semiconductor wafers.
Claim 5
Dependent Claim
76 words
The method according to claim 3 , wherein in a first operation where the production volume is relatively large there is performed a reducing projection exposure process using the photomask with the shield member formed by a metallic film, while in a second operation where the production volume is smaller than in the first operation there is performed a reducing projection exposure process using the photomask with the shield member formed by a photosensitive organic film.
Claim 6
Dependent Claim
25 words
The method according to claim 3 , wherein said projection exposures are made using a KrF excimer laser beam having a wavelength of 248 nm.
Claim 7
Dependent Claim
16 words
The method according to claim 1 , wherein said second light-shielding film is an organic film.
Claim 8
Dependent Claim
16 words
The method according to claim 6 , wherein said first light-shielding film is a metallic film.
Claim 9
Dependent Claim
71 words
A method according to claim 1 , for fabricating a semiconductor integrated circuit device, comprising the steps of: (b1) after step (b), inspecting a first pattern produced by said first projection exposure; (b2) if said first pattern does not meet a predetermined criterion, repeating steps (a) through (c), with adjustments to said first transverse dimensions, until said first projection exposure meets said predetermined criterion, and thereafter performing steps (c) and (d).
Claim 10
Dependent Claim
30 words
The method according to claim 8 , wherein steps (a) to (b2) are mask debugging steps, and steps (c) to (d) are steps of mass-producing the semiconductor integrated circuit device.
Claim 11
Dependent Claim
29 words
The method according to claim 8 , wherein said projection exposures are made using a KrF excimer laser beam having a wavelength of 248 nm as a light source.
Claim 12
Dependent Claim
21 words
The method according to claim 8 , wherein each first light-shielding film is organic, and said second light-shielding film is inorganic.
Claim 13
Dependent Claim
16 words
The method according to claim 8 , wherein said second light-shielding film is a metallic film.
Claim 14
Independent Claim
177 words
A method of fabricating a semiconductor integrated circuit device, comprising the steps of: (a) transferring a pattern onto a first photoresist layer over a semiconductor substrate by a reducing projection exposure process using a first photomask having an inorganic first light-shielding film having a first thickness, said first light-shielding film having first light-transmitting portions and first light-shielding portions arranged to produce a first predetermined projected exposure pattern corresponding to an integrated circuit, said first light-shielding portions having first transverse dimensions; and (b) transferring a second pattern onto a second photoresist layer over the semiconductor substrate by a reducing projection exposure process using an organic second light-shielding film having a second thickness greater than said first thickness, said second light-shielding film having second light-transmitting portions and second light-shielding portions arranged to produce a second predetermined projected exposure pattern corresponding to said semiconductor integrated circuit, wherein for a given pattern dimension on said semiconductor substrate said second light-shielding portions have second transverse dimensions smaller than said first transverse dimensions of said first light-shielding portions of said first light-shielding film.
Claim 15
Independent Claim
177 words
A method of fabricating a semiconductor integrated circuit device, comprising the steps of: (a) transferring a pattern onto a first photoresist layer over a semiconductor substrate by a reducing projection exposure process using a first photomask having an inorganic first light-shielding film having a first thickness, said first light-shielding film having first light-transmitting portions and first light-shielding portions arranged to produce a first predetermined projected exposure pattern corresponding to an integrated circuit, said first light-shielding portions having first transverse dimensions; and (b) transferring a second pattern onto a second photoresist layer over the semiconductor substrate by a reducing projection exposure process using an organic second light-shielding film having a second thickness greater than said first thickness, said second light-shielding film having second light-transmitting portions and second light-shielding portions arranged to produce a second predetermined projected exposure pattern corresponding to said semiconductor integrated circuit, wherein for a given pattern dimension on said semiconductor substrate said second light-shielding portions have second transverse dimensions smaller than said first transverse dimensions of said first light-shielding portions of said first light-shielding film.
Claim 16
Dependent Claim
25 words
The method according to claim 13 , wherein said projection exposures are made using a KrF excimer laser beam having a wavelength of 248 nm.
Claim 17
Dependent Claim
16 words
The method according to claim 13 , wherein said first light-shielding film is a metallic film.
Claim 18
Independent Claim
174 words
A method of fabricating an integrated circuit device, comprising the steps of: transferring a predetermined pattern onto a photosensitive substrate by a reducing projection exposure process using a photomask having first and second mask regions; said first mask region having a first light-shielding film comprising an inorganic film having a first thickness, said first light-shielding film having first light-transmitting portions and first light-shielding portions arranged to produce a first predetermined projected exposure pattern corresponding to a first portion of an integrated circuit, said first light-shielding portions having first transverse dimensions; said second mask region having a second light-shielding film comprising an organic film having a second thickness greater than said first thickness, said second-light-shielding film having second light-transmitting portions and second light-shielding portions arranged to produce a second predetermined projected exposure pattern corresponding to a second portion of the integrated circuit, wherein for a given pattern dimension on the substrate, said second light-shielding portions have second transverse dimensions smaller than said first transverse dimensions of said first light-shielding portions of said first mask region.
Claim 19
Independent Claim
174 words
A method of fabricating an integrated circuit device, comprising the steps of: transferring a predetermined pattern onto a photosensitive substrate by a reducing projection exposure process using a photomask having first and second mask regions; said first mask region having a first light-shielding film comprising an inorganic film having a first thickness, said first light-shielding film having first light-transmitting portions and first light-shielding portions arranged to produce a first predetermined projected exposure pattern corresponding to a first portion of an integrated circuit, said first light-shielding portions having first transverse dimensions; said second mask region having a second light-shielding film comprising an organic film having a second thickness greater than said first thickness, said second-light-shielding film having second light-transmitting portions and second light-shielding portions arranged to produce a second predetermined projected exposure pattern corresponding to a second portion of the integrated circuit, wherein for a given pattern dimension on the substrate, said second light-shielding portions have second transverse dimensions smaller than said first transverse dimensions of said first light-shielding portions of said first mask region.
Claim 20
Dependent Claim
28 words
The method according to claim 16 , wherein said projection exposures are made using a KrF excimer laser having a wavelength of 248 nm as a light source.
Claim 21
Dependent Claim
16 words
The method according to claim 16 , wherein said first light-shielding film is a metallic film.
References Cited (Backward Citations)
JPS5630129A
Cited
US4684971A
Cited
JPS5922050A
Cited
US5389474A
Cited
US5378585A
Cited
US5418092A
Cited
JPH05289307A
Cited
JPH0619115A
Cited
US5556724A
Cited
US5376483A
Cited
US5741613A
Cited
US6327022B1
Cited
JPH1115133A
Cited
US5948572A
Cited
US5989760A
Cited
WO2001002908A1
Cited
US6346427B1
Cited
WO2002005032A1
Cited
JP2002023340A
Cited
US20020022185A1
Cited
WO2002015242A1
Cited
JP2002062634A
Cited
US6426168B1
Cited
JP2002118049A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 2006-12-01 | 2007-06-02 | 2007-12-02 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 2010-12-01 | 2011-06-02 | 2011-12-02 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2014-12-01 | 2015-06-02 | 2015-12-02 | $7700.00 | Window Closed / Lapsed |