Abstract An improved method of fabricating a flash memory cell is disclosed. A tunnel oxide film is formed on active regions. A first conductive film and a protective film are sequentially formed on the tunnel oxide film. The protective film on the isolation film is selectively etched, thus forming a protective film pattern on the tunnel oxide film. A sacrificial conductive film is formed on the resultant structure. The sacrificial conductive film and the first conductive film pattern are over-etched until the sidewalls and the upper surface of the protective film pattern are exposed, thereby exposing the center of the isolation film and simultaneously forming a first conductive film pattern having sloped sidewalls. With the present invention, an electrical field is prevented from being concentrated in an area between a control gate electrode and a floating gate because the floating gate have a sloped sidewall profile instead of sharp edges. Also, the recession of an isolation film between adjacent floating gates can be significantly avoided, consequently suppressing the deterioration of isolation between adjacent cells.

Inventors

  • 👤 Jae-sun Yun
  • 👤 Jeong-Hyuk Choi
  • 👤 Chan-jo Lee

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 08:51
CPC Classifications
H; H10; H10B; H10B69/00; H10B41/00; H10B41/30

Claims Analysis

Total Claims: 24
Claim 1
Independent Claim 205 words
A method of fabricating a cell of a flash memory device, comprising the steps of: forming an isolation film for defining a plurality of parallel active regions on a semiconductor substrate; forming a tunnel oxide film on the active regions; sequentially forming, overlying the tunnel oxide film, a semiconductor film, a protective film, and a first conductive film; etching the first conductive film above the isolation film to form a first conductive film pattern above the tunnel oxide, thereby defining a first gap above the isolation film between a pair of sidewalls in the first conductive film pattern; forming spacers on the sidewalls of the first conductive film pattern; etching the protective film exposed between the spacers to form a protective film pattern, thereby defining, in the protective film, a second gap, the second gap being narrower than the first gap; etching the semiconductor film beneath the second gap to form a semiconductor film pattern, thereby exposing the center portion of the isolation film; removing the first conductive film pattern, thereby exposing the protective film pattern; removing the exposed protective film pattern, thereby exposing the semiconductor film pattern; and sequentially forming, overlying the semiconductor film pattern, an interlayer insulative film and a second conductive film.
Claim 2
Independent Claim 205 words
A method of fabricating a cell of a flash memory device, comprising the steps of: forming an isolation film for defining a plurality of parallel active regions on a semiconductor substrate; forming a tunnel oxide film on the active regions; sequentially forming, overlying the tunnel oxide film, a semiconductor film, a protective film, and a first conductive film; etching the first conductive film above the isolation film to form a first conductive film pattern above the tunnel oxide, thereby defining a first gap above the isolation film between a pair of sidewalls in the first conductive film pattern; forming spacers on the sidewalls of the first conductive film pattern; etching the protective film exposed between the spacers to form a protective film pattern, thereby defining, in the protective film, a second gap, the second gap being narrower than the first gap; etching the semiconductor film beneath the second gap to form a semiconductor film pattern, thereby exposing the center portion of the isolation film; removing the first conductive film pattern, thereby exposing the protective film pattern; removing the exposed protective film pattern, thereby exposing the semiconductor film pattern; and sequentially forming, overlying the semiconductor film pattern, an interlayer insulative film and a second conductive film.
Claim 3
Dependent Claim 41 words
The method of fabricating a cell of a flash memory device as claimed in claim 1, wherein the step of etching the semiconductor film beneath the second gap and the step of removing the first conductive film pattern are performed simultaneously.
Claim 4
Dependent Claim 25 words
The method of fabricating a cell of a flash memory device as claimed in claim 1, wherein the semiconductor film is an undoped polysilicon film.
Claim 5
Dependent Claim 28 words
The method of fabricating a cell of a flash memory device as claimed in claim 1, wherein the protective film is an insulative film containing a nitrogen component.
Claim 6
Dependent Claim 40 words
The method of fabricating a cell of a flash memory device as claimed in claim 4, wherein the insulative film containing a nitrogen component is selected from the group consisting of a silicon nitride film and a silicon oxynitride film.
Claim 7
Dependent Claim 31 words
The method of fabricating a cell of a flash memory device as claimed in claim 1, wherein the first conductive film is the same thickness or thinner than the semiconductor film.
Claim 8
Dependent Claim 26 words
The method of fabricating a cell of a flash memory device as claimed in claim 1, wherein the first conductive film is a doped polysilicon film.
Claim 9
Dependent Claim 39 words
The method of fabricating a cell of a flash memory device as claimed in claim 1, wherein the spacers are formed of a material selected from the group consisting of a doped silicon film and a silicon nitride film.
Claim 10
Dependent Claim 38 words
The method of fabricating a cell of a flash memory device as claimed in claim 8, wherein the doped silicon film is selected from the group consisting of a doped polysilicon film and a doped amorphous silicon film.
Claim 11
Dependent Claim 32 words
The method of fabricating a cell of a flash memory device as claimed in claim 1, wherein the exposed protective film pattern is removed by wet etching using a phosphoric acid solution.
Claim 12
Dependent Claim 26 words
The method of fabricating a cell of a flash memory device as claimed in claim 1, wherein the semiconductor film pattern is doped by ion implantation.
Claim 13
Dependent Claim 37 words
The method of fabricating a cell of a flash memory device as claimed in claim 1, wherein the interlayer insulative film is selected from the group consisting of an oxide/nitride/oxide (O/N/O) film and a nitride/oxide (N/O) film.
Claim 14
Dependent Claim 40 words
The method of fabricating a cell of a flash memory device as claimed in claim 1, wherein the second conductive film is selected from the group consisting of a doped polysilicon film and a polycide film containing a refractory metal.
Claim 15
Dependent Claim 40 words
The method of fabricating a cell of a flash memory device as claimed in claim 13, wherein the polycide film containing the refractory metal is selected from the group consisting of a tungsten polycide film and a titanium polycide film.
Claim 16
Independent Claim 171 words
A method of fabricating a cell of a flash memory device, comprising the steps of: forming an isolation film, for defining a plurality of parallel active regions, on a semiconductor substrate; forming a tunnel oxide film on the active regions; sequentially forming a first conductive film and a protective film on the entire surface of the semiconductor substrate on which the tunnel oxide film is formed; forming a protective film pattern above the tunnel oxide film by selectively etching the protective film above the isolation film; forming a sacrificial conductive film on the entire surface of the semiconductor substrate on which the protective film pattern is formed; exposing the center of the isolation film and simultaneously forming a first conductive film pattern having sloped sidewalls, by over-etching the sacrificial conductive film and the first conductive film until the sidewalls and an upper surface of the protective film pattern are exposed; removing the protective film pattern; and sequentially forming an interlayer insulative film and a second conductive film on the resultant structure.
Claim 17
Independent Claim 171 words
A method of fabricating a cell of a flash memory device, comprising the steps of: forming an isolation film, for defining a plurality of parallel active regions, on a semiconductor substrate; forming a tunnel oxide film on the active regions; sequentially forming a first conductive film and a protective film on the entire surface of the semiconductor substrate on which the tunnel oxide film is formed; forming a protective film pattern above the tunnel oxide film by selectively etching the protective film above the isolation film; forming a sacrificial conductive film on the entire surface of the semiconductor substrate on which the protective film pattern is formed; exposing the center of the isolation film and simultaneously forming a first conductive film pattern having sloped sidewalls, by over-etching the sacrificial conductive film and the first conductive film until the sidewalls and an upper surface of the protective film pattern are exposed; removing the protective film pattern; and sequentially forming an interlayer insulative film and a second conductive film on the resultant structure.
Claim 18
Dependent Claim 20 words
The method of claim 15, wherein the first conductive film is a doped silicon film or an undoped silicon film.
Claim 19
Dependent Claim 14 words
The method of claim 15, wherein the protective film is a silicon nitride film.
Claim 20
Dependent Claim 18 words
The method of claim 15, further comprising the step of forming an anti-reflective film on the protective film.
Claim 21
Dependent Claim 14 words
The method of claim 18, wherein the anti-reflective film is a silicon oxynitride film.
Claim 22
Dependent Claim 20 words
The method of claim 15, wherein the sacrificial conductive film is a doped silicon film or an undoped silicon film.
Claim 23
Independent Claim 223 words
A method of fabricating a cell of a flash memory device, comprising the steps of: forming an isolation film for defining a plurality of parallel active regions on a semiconductor substrate; forming a tunnel oxide film on the active regions; sequentially forming, overlying the tunnel oxide film, an undoped polysilicon film, a protective film, and a first conductive film; etching the first conductive film above the isolation film to form a first conductive film pattern above the tunnel oxide, thereby defining a first gap above the isolation film between a pair of sidewalls in the first conductive film pattern; forming spacers on the sidewalls of the first conductive film pattern; etching the protective film exposed between the spacers to form a protective film pattern, thereby defining, in the protective film, a second gap, the second gap being narrower than the first gap; etching the undoped polysilicon film beneath the second gap to form an undoped polysilicon film pattern, thereby exposing the center portion of the isolation film; removing the first conductive film pattern, thereby exposing the protective film pattern; removing the exposed protective film pattern, thereby exposing the undoped polysilicon film pattern; after removing the exposed protective film pattern, doping the undoped polysilicon film pattern; and sequentially forming, overlying the doped polysilicon film pattern, an interlayer insulative film and a second conductive film.
Claim 24
Independent Claim 223 words
A method of fabricating a cell of a flash memory device, comprising the steps of: forming an isolation film for defining a plurality of parallel active regions on a semiconductor substrate; forming a tunnel oxide film on the active regions; sequentially forming, overlying the tunnel oxide film, an undoped polysilicon film, a protective film, and a first conductive film; etching the first conductive film above the isolation film to form a first conductive film pattern above the tunnel oxide, thereby defining a first gap above the isolation film between a pair of sidewalls in the first conductive film pattern; forming spacers on the sidewalls of the first conductive film pattern; etching the protective film exposed between the spacers to form a protective film pattern, thereby defining, in the protective film, a second gap, the second gap being narrower than the first gap; etching the undoped polysilicon film beneath the second gap to form an undoped polysilicon film pattern, thereby exposing the center portion of the isolation film; removing the first conductive film pattern, thereby exposing the protective film pattern; removing the exposed protective film pattern, thereby exposing the undoped polysilicon film pattern; after removing the exposed protective film pattern, doping the undoped polysilicon film pattern; and sequentially forming, overlying the doped polysilicon film pattern, an interlayer insulative film and a second conductive film.

References Cited (Backward Citations)

US5688705A Cited
US5661053A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 2003-11-28 2004-05-29 2004-11-28 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2007-11-28 2008-05-29 2008-11-28 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2011-11-28 2012-05-29 2012-11-28 $7700.00 Window Closed / Lapsed