Abstract

Abstract A test method for characterizing retention performance, both same state and opposite state performance, of ferroelectric capacitors includes the steps of writing an original complementary data state into first and second ferroelectric capacitors after the ferroelectric capacitors have been initialized into an initial valid data state. The first and second ferroelectric capacitors are then subjected to time and temperature stress. The original complementary data state from the first and second ferroelectric capacitors is then read, and same state charge (Q SS ) information is collected. An opposite complementary data state is then written in the first and second capacitors. After a short time interval, possibly at an elevated temperature, the opposite complementary data state from the first and second ferroelectric capacitors is read to gather opposite state charge (Q OS ) information. The original complementary data state is then written into the first and second ferroelectric capacitors. The first and second ferroelectric capacitors are then subjected to further stress cycles, after which the same state and opposite state charge values are recorded. A plot of the same state charge (Q SS ) and opposite state charge (Q OS ) versus log time can be generated, which has great value for fully characterizing a ferroelectric capacitor and for predicting the performance of a ferroelectric capacitor in a memory circuit.

Inventors

  • 👤 Steven Traynor

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 09:10
CPC Classifications
G; G11; G11C; G11C11/00; G11C11/21; G11C11/22

Claims Analysis

Total Claims: 25
Claim 1
Independent Claim 93 words
A method for measuring retention performance in ferroelectric capacitors, the method comprising the steps of: (a) collecting same state charge values from a pair of ferroelectric capacitors formed of a first ferroelectric capacitor and a second ferroelectric capacitor; (b) collecting opposite state charge values from respective ones of the first and second ferroelectric capacitors, respectively, of the pair of ferroelectric capacitors; (c) subjecting both the first and second of the pair of ferroelectric capacitors to time and temperature stress; and (d) plotting the same state charge and opposite state charge values versus time.
Claim 2
Independent Claim 93 words
A method for measuring retention performance in ferroelectric capacitors, the method comprising the steps of: (a) collecting same state charge values from a pair of ferroelectric capacitors formed of a first ferroelectric capacitor and a second ferroelectric capacitor; (b) collecting opposite state charge values from respective ones of the first and second ferroelectric capacitors, respectively, of the pair of ferroelectric capacitors; (c) subjecting both the first and second of the pair of ferroelectric capacitors to time and temperature stress; and (d) plotting the same state charge and opposite state charge values versus time.
Claim 3
Independent Claim 153 words
A method for characterizing retention in ferroelectric capacitors, the method comprising the steps of: (a) writing an original complementary data state into a pair of ferroelectric capacitors formed of a first ferroelectric capacitor and a second ferroelectric capacitor; (b) subjecting the first and second ferroelectric capacitors, respectively, to time and temperature stress; (c) reading the original complementary data state from the pair of ferroelectric capacitors and recording the same state charge value; (d) writing an opposite complementary data state into the pair of ferroelectric capacitors; (e) waiting for a predetermined time interval; (f) reading the opposite complementary data state from the pair of ferroelectric capacitors and recording the opposite state charge value; (g) writing the original complementary data state into the pair of ferroelectric capacitors; and (h) repeating steps (b) through (g) for a plurality of cycles to gather same state and opposite state charges values as a function of time and temperature.
Claim 4
Independent Claim 153 words
A method for characterizing retention in ferroelectric capacitors, the method comprising the steps of: (a) writing an original complementary data state into a pair of ferroelectric capacitors formed of a first ferroelectric capacitor and a second ferroelectric capacitor; (b) subjecting the first and second ferroelectric capacitors, respectively, to time and temperature stress; (c) reading the original complementary data state from the pair of ferroelectric capacitors and recording the same state charge value; (d) writing an opposite complementary data state into the pair of ferroelectric capacitors; (e) waiting for a predetermined time interval; (f) reading the opposite complementary data state from the pair of ferroelectric capacitors and recording the opposite state charge value; (g) writing the original complementary data state into the pair of ferroelectric capacitors; and (h) repeating steps (b) through (g) for a plurality of cycles to gather same state and opposite state charges values as a function of time and temperature.
Claim 5
Dependent Claim 20 words
The method of claim 1 further comprising the step of initializing the pair of capacitors to a valid data state.
Claim 6
Independent Claim 152 words
A method for characterizing retention in ferroelectric capacitors, the method comprising the steps of: (a) reading/writing an original complementary data state into a pair of ferroelectric capacitors formed of a first ferroelectric capacitor and a second ferroelectric capacitor; (b) subjecting the first and second ferroelectric capacitors, respectively, to time and temperature stress; (c) reading/restoring the original complementary data state from the pair of ferroelectric capacitors and recording the same state charge value; (d) reading/writing an opposite complementary data state into the pair or ferroelectric capacitors; (e) waiting for a predetermined time interval; (f) reading/restoring the opposite complementary data state from the pair of ferroelectric capacitors and recording the opposite state charge value; (g) reading/writing the original complementary data state into the pair of ferroelectric capacitors; and (h) repeating steps (b) through (g) for a plurality of cycles to gather same state and opposite state charges as a function of time and temperature.
Claim 7
Independent Claim 152 words
A method for characterizing retention in ferroelectric capacitors, the method comprising the steps of: (a) reading/writing an original complementary data state into a pair of ferroelectric capacitors formed of a first ferroelectric capacitor and a second ferroelectric capacitor; (b) subjecting the first and second ferroelectric capacitors, respectively, to time and temperature stress; (c) reading/restoring the original complementary data state from the pair of ferroelectric capacitors and recording the same state charge value; (d) reading/writing an opposite complementary data state into the pair or ferroelectric capacitors; (e) waiting for a predetermined time interval; (f) reading/restoring the opposite complementary data state from the pair of ferroelectric capacitors and recording the opposite state charge value; (g) reading/writing the original complementary data state into the pair of ferroelectric capacitors; and (h) repeating steps (b) through (g) for a plurality of cycles to gather same state and opposite state charges as a function of time and temperature.
Claim 8
Dependent Claim 21 words
The method of claim 4 further comprising the step of initializing the pair of ferroelectric capacitors to a valid data state.
Claim 9
Dependent Claim 31 words
The method of claim 5 in which the initializing step comprises the step of applying a PUND pulse sequence to each of the first and second ferroelectric capacitors in the pair.
Claim 10
Dependent Claim 40 words
The method of claim 4 in which step (a) comprises the steps of applying a PU pulse sequence to the first ferroelectric capacitor in the pair and applying a PN pulse sequence to the second ferroelectric capacitor in the pair.
Claim 11
Dependent Claim 21 words
The method of claim 4 in which step (b) lasts for about an hour at a temperature of about 150° C.
Claim 12
Dependent Claim 40 words
The method of claim 4 in which step (c) comprises the steps of applying a UU pulse sequence to the first ferroelectric capacitor in the pair and applying a PN pulse sequence to the second ferroelectric capacitor in the pair.
Claim 13
Dependent Claim 40 words
The method of claim 4 in which step (d) comprises the steps of applying a UN pulse sequence to the first ferroelectric capacitor in the pair and applying a PU pulse sequence to the second ferroelectric capacitor in the pair.
Claim 14
Dependent Claim 14 words
The method of claim 4 in which step (e) lasts for about thirty seconds.
Claim 15
Dependent Claim 14 words
The method of claim 4 in which step (e) lasts for about five minutes.
Claim 16
Dependent Claim 21 words
The method of claim 4 further comprising the step of applying an elevated temperature to the ferroelectric capacitors during step (e).
Claim 17
Dependent Claim 40 words
The method of claim 4 in which step (f) comprises the steps of applying a PN pulse sequence to the first ferroelectric capacitor in the pair and applying a UU pulse sequence to the second ferroelectric capacitor in the pair.
Claim 18
Dependent Claim 40 words
The method of claim 4 in which step (g) comprises the steps of applying a PU pulse sequence to the first ferroelectric capacitor in the pair and applying a PN pulse sequence to the second ferroelectric capacitor in the pair.
Claim 19
Dependent Claim 29 words
The method of claim 4 further comprising the step of applying a PUND pulse sequence to both of the ferroelectric capacitors in the pair between steps (f) and (g).
Claim 20
Independent Claim 98 words
A method for characterizing the reference charge level for a 1T-1C ferroelectric memory cell, the method comprising the steps of: (a) collecting opposite state switched charge information over time and temperature form a pair of ferroelectric capacitors formed of a first ferroelectric capacitor and a second ferroelectric capacitor; (b) collecting opposite state non-switched charge information over time and temperature from the pair of ferroelectric capacitors; (c) determining an "end of life" charge level from the opposite state switched and non-switched charge information; and (d) setting the reference charge level approximately equal to the "end of life" charge level.
Claim 21
Independent Claim 98 words
A method for characterizing the reference charge level for a 1T-1C ferroelectric memory cell, the method comprising the steps of: (a) collecting opposite state switched charge information over time and temperature form a pair of ferroelectric capacitors formed of a first ferroelectric capacitor and a second ferroelectric capacitor; (b) collecting opposite state non-switched charge information over time and temperature from the pair of ferroelectric capacitors; (c) determining an "end of life" charge level from the opposite state switched and non-switched charge information; and (d) setting the reference charge level approximately equal to the "end of life" charge level.
Claim 22
Dependent Claim 23 words
The method of claim 17 in which the charge information in steps (a) and (b) is generated according to the "up-down" sensing method.
Claim 23
Dependent Claim 23 words
The method of claim 17 in which the charge information in steps (a) and (b) is generated according to the "up-only" sensing method.
Claim 24
Independent Claim 46 words
A method for measuring retention performance in ferroelectric capacitors comprising the steps of collecting a plurality of same state and opposite state charge values from a pair of ferroelectric capacitors formed of a first ferroelectric capacitor and a second ferroelectric capacitor during time and temperature stress.
Claim 25
Independent Claim 46 words
A method for measuring retention performance in ferroelectric capacitors comprising the steps of collecting a plurality of same state and opposite state charge values from a pair of ferroelectric capacitors formed of a first ferroelectric capacitor and a second ferroelectric capacitor during time and temperature stress.

References Cited (Backward Citations)

DE1089475B Cited
US3492662A Cited
SU731406A1 Cited
SU917149A1 Cited
US5254482A Cited
US5751628A Cited
US5661730A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 2002-12-27 2003-06-28 2003-12-28 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2006-12-27 2007-06-28 2007-12-28 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2010-12-27 2011-06-28 2011-12-28 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag