Method for producing a semiconductor device having a semiconductor layer of SiC
Assignee: ABB Research Ltd Switzerland
•
Filing: 1995-05-08
•
Granted: 1998-09-08
•
Expires: 2015-05-08
Abstract
Abstract A method for producing a semiconductor device, having a semiconductor layer of a SiC comprises the steps of a) supplying dopants to the surface of the SiC layer during heating thereof for diffusion of the dopants into the SiC layer, and b) highly doping at least a portion of the surface layer of the SiC layer prior to step a) to control diffusion of the dopants into the SiC layer under the surface layer portion.
Inventors
- 👤 Andrei Konstantinov
- 👤 Erik Janzen
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-27 07:38
CPC Classifications
H; H10; H10D; H10D8/00; H10D8/01; H10D8/051; C; C23; C23C; C23C8/00; C23C8/02; C23C8/04; H10D62/00; H10D62/80; H10D62/83; H10D62/832; H10D62/8325; H10D8/043; H10P; H10P30/00; H10P30/20; H10P30/22; H10P32/00; H10P32/10; H10P32/17; H10P32/171; H10P32/172; Y; Y10; Y10S; Y10S438/00; Y10S438/931
Claims Analysis
Total Claims: 18
Claim 1
Independent Claim
158 words
A method for producing a semiconductor device having a semiconductor layer of a SiC, said method comprising the steps of a) supplying dopants to the surface of the SiC layer during heating thereof for diffusion of said dopants into the SiC layer, and b) prior to step a) highly doping at least a portion of the surface layer in the peripheral regions of the SiC layer with dopants of the same conductivity type as that of the dopants for said diffusion for obtaining enhanced diffusion of dopants at the periphery of the SiC layer under said surface layer portion, and wherein the heat treatment and thereby the diffusion in step a) is carried out under such conditions that the dopants may penetrate through a junction thereby creating the space charge region of said device for creating a guard ring arranged to smooth out the electric field in the peripheral region during a blocking state of the power device.
Claim 2
Independent Claim
158 words
A method for producing a semiconductor device having a semiconductor layer of a SiC, said method comprising the steps of a) supplying dopants to the surface of the SiC layer during heating thereof for diffusion of said dopants into the SiC layer, and b) prior to step a) highly doping at least a portion of the surface layer in the peripheral regions of the SiC layer with dopants of the same conductivity type as that of the dopants for said diffusion for obtaining enhanced diffusion of dopants at the periphery of the SiC layer under said surface layer portion, and wherein the heat treatment and thereby the diffusion in step a) is carried out under such conditions that the dopants may penetrate through a junction thereby creating the space charge region of said device for creating a guard ring arranged to smooth out the electric field in the peripheral region during a blocking state of the power device.
Claim 3
Independent Claim
192 words
A method for producing a semiconductor device having a semiconductor layer of a SiC, said method comprising the steps of a) supplying dopants to the surface of the SiC layer during heating thereof for diffusion of said dopants into the SiC layer, and b) highly doping at least a portion of the surface layer of the SiC layer prior to step a) with dopants of an opposite conductivity type to that of the dopants supplied for said diffusion, to control diffusion of dopants into the SiC layer under said surface layer portion, whereby said surface layer portion in step a) functions as a diffusion mask and wherein said mask is first created by epitaxial growth of a highly doped layer followed by a patterning thereof for removing said mask layer in the peripheral regions of the SiC layer, an ion implantation is then carried out for creating a thin highly doped surface layer in said peripheral regions, then the SiC layer is annealed so as to re-crystallize the ion-implanted layer, said diffusion step is carried out for forming a guard ring, and then the mask layer is removed in a non-mechanical way.
Claim 4
Independent Claim
192 words
A method for producing a semiconductor device having a semiconductor layer of a SiC, said method comprising the steps of a) supplying dopants to the surface of the SiC layer during heating thereof for diffusion of said dopants into the SiC layer, and b) highly doping at least a portion of the surface layer of the SiC layer prior to step a) with dopants of an opposite conductivity type to that of the dopants supplied for said diffusion, to control diffusion of dopants into the SiC layer under said surface layer portion, whereby said surface layer portion in step a) functions as a diffusion mask and wherein said mask is first created by epitaxial growth of a highly doped layer followed by a patterning thereof for removing said mask layer in the peripheral regions of the SiC layer, an ion implantation is then carried out for creating a thin highly doped surface layer in said peripheral regions, then the SiC layer is annealed so as to re-crystallize the ion-implanted layer, said diffusion step is carried out for forming a guard ring, and then the mask layer is removed in a non-mechanical way.
Claim 5
Dependent Claim
39 words
A method according to claim 1, wherein in step b) first surface layer portions of the SiC layer are highly doped with P-type dopants, whereas second surface layer portions of the SiC layer are highly doped with N-type dopants.
Claim 6
Dependent Claim
31 words
A method according to claim 1, wherein in step b) a very thin highly doped layer of the same conductivity type is applied, said layer having a thickness below 0.5 μm.
Claim 7
Dependent Claim
23 words
A method according to claim 2, wherein said surface layer portion of the opposite or same conductivity type is applied by ion implantation.
Claim 8
Dependent Claim
30 words
A method according to claim 5, wherein said ion implantation is carried out with an energy of 50-100 KeV and at a dose of 2-3×10 16 per cm 2 .
Claim 9
Dependent Claim
19 words
A method according to claim 2, wherein said highly doped surface layer portion is obtained by doping with aluminum.
Claim 10
Dependent Claim
26 words
A method according to claim 5, wherein the SiC layer is annealed through heating after the ion implantation for re-crystallizing the ion implanted surface layer portion.
Claim 11
Dependent Claim
26 words
A method according to claim 4, wherein the dopants supplied for said diffusion are of P-type and said highly doped surface layer portion is of N-type.
Claim 12
Dependent Claim
46 words
A method according to claim 9, wherein said surface layer portion of said opposite conductivity type is created by epitaxially growing a thin SiC layer highly doped with N-type dopants on top of the SiC layer at a doping concentration above 5×10 19 cm 3 .
Claim 13
Dependent Claim
21 words
A method according to claim 1 or 2, wherein the SiC layer is heated above 1500° C. during said diffusion step.
Claim 14
Dependent Claim
17 words
A method according to claim 1 or 2, wherein the dopant supplied for the diffusion is boron.
Claim 15
Dependent Claim
33 words
A method according to claim 1, wherein said SiC layer is made of at least two sub-layers, a first uppermost layer of P-type and a second layer of N-type supporting the first layer.
Claim 16
Dependent Claim
37 words
A method according to claim 2 wherein in step b) different surface layer portions are doped with dopants having opposite conductivity so as to obtain different diffusivities of the dopants in different portions of the SiC layer.
Claim 17
Dependent Claim
19 words
A method according to claim 2 wherein the SiC layer is heated above 1500° C. during said diffusion step.
Claim 18
Dependent Claim
15 words
A method according to claim 1 wherein the dopant supplied for the diffusion is boron.
References Cited (Backward Citations)
US3510369A
Cited
US4560642A
Cited
EP0380340A2
Cited
US5313078A
Cited
US5286660A
Cited
US5322802A
Cited
US5543637A
Cited
US5654208A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 2001-09-07 | 2002-03-09 | 2002-09-08 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 2005-09-07 | 2006-03-09 | 2006-09-08 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2009-09-07 | 2010-03-09 | 2010-09-08 | $7700.00 | Window Closed / Lapsed |