Claims Analysis
Total Claims: 10
Claim 1
Independent Claim
133 words
A method of manufacturing a second harmonic generation device, comprising the steps of: forming a pattern for forming a periodic domain inversion area on a substrate of a non-linear material; performing proton-exchange and heat-treatment for said substrate on which said pattern is formed to thereby form said periodic domain inversion area having a predetermined period and width; forming a straight optical waveguide and a segmental optical waveguide, for forming an optical waveguide, in the direction perpendicular to said periodic domain inversion area; and forming an insulating buffer layer on said substrate where said periodic domain inversion area and said straight and segmental optical waveguides are formed, and forming a metal electrode on said insulating buffer layer on the upper portion of said segmental optical waveguide, and polishing an end facet, and anti-reflection coating.
Claim 2
Independent Claim
133 words
A method of manufacturing a second harmonic generation device, comprising the steps of: forming a pattern for forming a periodic domain inversion area on a substrate of a non-linear material; performing proton-exchange and heat-treatment for said substrate on which said pattern is formed to thereby form said periodic domain inversion area having a predetermined period and width; forming a straight optical waveguide and a segmental optical waveguide, for forming an optical waveguide, in the direction perpendicular to said periodic domain inversion area; and forming an insulating buffer layer on said substrate where said periodic domain inversion area and said straight and segmental optical waveguides are formed, and forming a metal electrode on said insulating buffer layer on the upper portion of said segmental optical waveguide, and polishing an end facet, and anti-reflection coating.
Claim 3
Dependent Claim
44 words
The method as claimed in claim 1, wherein said proton-exchange is performed by dipping said substrate into a benzoic acid or pyrophosphoric acid of 200°-300° C., and said heat-treatment is then executed below a Curie temperature, to thereby form said periodic domain inversion area.
Claim 4
Dependent Claim
44 words
The method as claimed in claim 1, wherein said proton-exchange is executed by dipping said substrate into a benzoic acid or pyrophosphoric acid of 200°-300° C., and said heat-treatment is then executed at 300°-400° C., to thereby form said straight and segmental optical waveguides.
Claim 5
Dependent Claim
23 words
The method as claimed in claim 1, wherein said insulating buffer layer is comprised of Al 2 O 3 or SiO 2 .
Claim 6
Dependent Claim
20 words
The method as claimed in claim 1, wherein said non-linear medium is comprised of LiTaO 3 or LiNbO 3 .
Claim 7
Dependent Claim
24 words
The method as claimed in claim 1, wherein said pattern for forming said periodic domain inversion area is comprised of chromium (Cr) or Ta.
Claim 8
Dependent Claim
22 words
The method as claimed in claim 1, wherein said pattern for forming said optical waveguide is comprised of chromium (Cr) or Ta.
Claim 9
Dependent Claim
23 words
The method as claimed in claim 1, wherein said pattern for forming said segmented optical waveguide has a period of about 2 m.
Claim 10
Dependent Claim
23 words
The method as claimed in claim 1, wherein said pattern for forming said periodic domain inversion area has a period of 3-4 m.