Abstract

Abstract A method for forming ferroelectric wafers is provided. A prestress layer is placed on the desired mold. A ferroelectric wafer is placed on top of the prestress layer. The layers are heated and then cooled, causing the ferroelectric wafer to become prestressed. The prestress layer may include reinforcing material and the ferroelectric wafer may include electrodes or electrode layers may be placed on either side of the ferroelectric layer. Wafers produced using this method have greatly improved output motion.

Inventors

  • 👤 Richard F. Hellbaum
  • 👤 Robert G. Bryant
  • 👤 Robert L. Fox

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-28 22:01
CPC Classifications
B; B32; B32B; B32B37/00; B32B37/14; B32B37/144; H; H10; H10N; H10N30/00; H10N30/01; H10N30/07; H10N30/072; H10N30/073; H10N30/20; H10N30/204; H10N30/2047; H10N30/2048; Y; Y10; Y10T; Y10T29/00; Y10T29/42

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 58 words
A method for producing ferroelectric devices, comprising: selecting a mold for the device; placing a prestress layer on the mold; placing a ferroelectric layer on the prestress layer to create layer structure; heating the prestress and ferroelectric layers; and cooling the prestress and ferroelectric layers whereby the heating and cooling steps induce a prestress into the layered structure.
Claim 2
Independent Claim 58 words
A method for producing ferroelectric devices, comprising: selecting a mold for the device; placing a prestress layer on the mold; placing a ferroelectric layer on the prestress layer to create layer structure; heating the prestress and ferroelectric layers; and cooling the prestress and ferroelectric layers whereby the heating and cooling steps induce a prestress into the layered structure.
Claim 3
Dependent Claim 12 words
The method of claim 1 wherein the prestress layer includes reinforcing material.
Claim 4
Dependent Claim 12 words
The method of claim 1 wherein the ferroelectric layer includes surface electrodes.
Claim 5
Dependent Claim 32 words
The method of claim 1 further comprising: placing a first electrode layer between the prestress layer and the ferroelectric layer; and placing a second electrode layer on top of the ferroelectric layer.
Claim 6
Dependent Claim 12 words
The method of claim 1 wherein the prestress layer is an adhesive.
Claim 7
Dependent Claim 13 words
The method of claim 1 wherein the ferroelectric layer is a piezoelectric material.
Claim 8
Dependent Claim 13 words
The method of claim 1 wherein the ferroelectric layer is a piezostrictive material.
Claim 9
Dependent Claim 14 words
The method of claim 1 wherein the ferroelectric layer is formed from a composite.

References Cited (Backward Citations)

US3631383A Cited
US5042493A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 2000-05-26 2000-11-25 2001-05-27 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2004-05-26 2004-11-25 2005-05-27 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2008-05-26 2008-11-25 2009-05-27 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag