← Back to Patent Explorer
US5589305A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of fabricating a reticle

Assignee: Toshiba Corp
•
Filing: 1995-05-30
•
Granted: 1996-12-31
•
Expires: 2015-05-30
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract In a reticle, a semi-transparent film pattern in place of a light blocking film pattern is used as a mask pattern having a size within a certain range, whereby an exposure system can be improved in resolution limit and faithful pattern transfer can be realized with a constant light quantity. A reticle may be of a stacked layer structure which comprises a shift film for providing a different optical path to exposure light, a mask substrate formed on the top or bottom of the shift film, and a transmissivity ratio adjustment layer having a predetermined transmissivity ratio to the exposure light. The material of a phase shifter may be adjusted in amplitude transmissivity ratio so that a shifter width for effectively improving a contrast can be made large and an accuracy necessary for a shifter width can be loosened. The mask pattern may include a semi-transparent film pattern which is made of silicon, a silicon compound, a mixture containing silicon, germanium, a germanium compound or a mixture containing germanium to provide a different optical path from that of the transparent part with respect to lithographic light. A silicon compound, a mixture containing silicon, germanium, a germanium compound or a mixture containing germanium is controlled in its composition ratio to form a semi-transparent film pattern on a transparent substrate.

Inventors

  • 👤 Yoko Tomofuji
  • 👤 Makoto Nakase
  • 👤 Takashi Sato
  • 👤 Hiroaki Hazama
  • 👤 Haruki Komano
  • 👤 Shinichi Ito

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-07 22:44
CPC Classifications
G; G03; G03F; G03F1/00; G03F1/26; G03F1/32; G03F1/29; G03F1/36

Claims Analysis

Total Claims: 17
Claim 1
Independent Claim 201 words
A method of fabricating a reticle comprising the step of forming on a light-transmissible substrate a mask pattern of a semi-transparent film which causes length of an optical path for a light beam passing therethrough to be different from length of an optical path for a light beam passing through the light-transmissible substrate by a predetermined amount, wherein the step of forming a mask pattern comprises the steps of: determining ranges of refractive index n and extinction coefficient k of the semi-transparent film within which transmissivity ratio T and a phase difference φ between the semi-transparent film and air that has the same thickness of the semi-transparent film fall within ranges necessary to obtain desired resolution and depth of focus; obtaining relationship in the form of a curved line between the refractive index n and the extinction coefficient k by changing conditions for formation of the mask pattern; selecting values of the refractive index and the extinction coefficient from the range thus determined, and determining the conditions for formation of the mask pattern such that the refractive index and the extinction coefficient become the selected values; and forming a mask pattern based on the conditions for formation of the mask pattern.
Claim 2
Independent Claim 201 words
A method of fabricating a reticle comprising the step of forming on a light-transmissible substrate a mask pattern of a semi-transparent film which causes length of an optical path for a light beam passing therethrough to be different from length of an optical path for a light beam passing through the light-transmissible substrate by a predetermined amount, wherein the step of forming a mask pattern comprises the steps of: determining ranges of refractive index n and extinction coefficient k of the semi-transparent film within which transmissivity ratio T and a phase difference φ between the semi-transparent film and air that has the same thickness of the semi-transparent film fall within ranges necessary to obtain desired resolution and depth of focus; obtaining relationship in the form of a curved line between the refractive index n and the extinction coefficient k by changing conditions for formation of the mask pattern; selecting values of the refractive index and the extinction coefficient from the range thus determined, and determining the conditions for formation of the mask pattern such that the refractive index and the extinction coefficient become the selected values; and forming a mask pattern based on the conditions for formation of the mask pattern.
Claim 3
Dependent Claim 82 words
A method of fabricating a reticle as set forth in claim 1, wherein the step of forming a mask pattern further comprises the step of: forming a silicon nitride or silicon oxide film having desired values of amplitude transmissivity ratio and phase difference by mixing a predetermined quantity of nitrogen or oxygen gas in a sputtering atmosphere with use of silicon as a target and controlling a nitrogen or oxygen composition ratio based on the conditions for formation of the mask pattern.
Claim 4
Dependent Claim 84 words
A method of fabricating a reticle as set forth in claim 1, wherein the step of forming a mask pattern comprises the step of: depositing a silicon di-oxide film while adjusting the quantity of oxygen in a raw material gas by using a CVD technique based on the conditions for formation of the mask pattern so as to control an oxygen composition ratio in the silicon di-oxide film thereby to form a mask pattern having desired values of amplitude transmissivity ratio and phase difference.
Claim 5
Dependent Claim 78 words
A method of fabricating a reticle as set forth in claim 1, wherein the step of forming a mask pattern comprises the step of: depositing a silicon nitride film while adjusting the quantity of ammonium in a raw material gas by a CVD technique based on the conditions for formation of the mask pattern so as to control a nitrogen composition ratio thereby to form a mask pattern having desired values of amplitude transmissivity ratio and phase difference.
Claim 6
Dependent Claim 64 words
A method of fabricating a reticle as set forth in claim 1, wherein the step of forming a mask pattern comprises the step of: implanting ions into a surface of the semi-transparent film pattern formed based on the conditions for formation of the mask pattern; and/or a modification step of changing a crystalline state through heat treatment to finely adjust an amplitude transmissivity ratio.
Claim 7
Independent Claim 197 words
A method of fabricating a reticle comprising the step of forming on a light-transmissible substrate a mask pattern of a semi-transparent film which causes length of an optical path for a light beam passing therethrough to be different from length of an optical path for a light beam passing through the light-transmissible substrate by a predetermined amount, wherein the step of forming a mask pattern comprises the steps of: determining ranges of refractive index n and extinction coefficient k of the semi-transparent film within which transmissivity ratio T and a phase difference φ between the semi-transparent film and air that has the same thickness of the semi-transparent film fall within ranges necessary to obtain desired resolution and depth of focus; obtaining relationship in the form of a curved line between the refractive index n and the extinction coefficient k by changing composition ratio of a material constituting the mask pattern; selecting values of the refractive index and the extinction coefficient from the range thus determined, and determining the composition ratio of the constituting material such that the refractive index and the extinction coefficient become the selected values; and forming a mask pattern based on the composition ratio.
Claim 8
Independent Claim 197 words
A method of fabricating a reticle comprising the step of forming on a light-transmissible substrate a mask pattern of a semi-transparent film which causes length of an optical path for a light beam passing therethrough to be different from length of an optical path for a light beam passing through the light-transmissible substrate by a predetermined amount, wherein the step of forming a mask pattern comprises the steps of: determining ranges of refractive index n and extinction coefficient k of the semi-transparent film within which transmissivity ratio T and a phase difference φ between the semi-transparent film and air that has the same thickness of the semi-transparent film fall within ranges necessary to obtain desired resolution and depth of focus; obtaining relationship in the form of a curved line between the refractive index n and the extinction coefficient k by changing composition ratio of a material constituting the mask pattern; selecting values of the refractive index and the extinction coefficient from the range thus determined, and determining the composition ratio of the constituting material such that the refractive index and the extinction coefficient become the selected values; and forming a mask pattern based on the composition ratio.
Claim 9
Independent Claim 204 words
A method of fabricating a reticle comprising the step of forming on a light-transmissible substrate a mask pattern of a semi-transparent film which causes length of an optical path for a light beam passing therethrough to be different from length of an optical path for a light beam passing through the light-transmissible substrate by a predetermined amount, wherein the step of forming a mask pattern comprises the steps of: determining ranges of refractive index n and extinction coefficient k of the semi-transparent film within which transmissivity ratio T and a phase difference φ between the semi-transparent film and air that has the same thickness of the semi-transparent film fall within ranges necessary to obtain desired resolution and depth of focus; obtaining relationship in the form of a curved line between the refractive index n and the extinction coefficient k by changing composition of a material constituting the mask pattern; selecting values of the refractive index n and the extinction coefficient k from the range thus determined, and determining the composition of the constituting material such that the refractive index n and the extinction coefficient k become the selected values; and forming a mask pattern so that the mask pattern has the composition thus determined.
Claim 10
Independent Claim 204 words
A method of fabricating a reticle comprising the step of forming on a light-transmissible substrate a mask pattern of a semi-transparent film which causes length of an optical path for a light beam passing therethrough to be different from length of an optical path for a light beam passing through the light-transmissible substrate by a predetermined amount, wherein the step of forming a mask pattern comprises the steps of: determining ranges of refractive index n and extinction coefficient k of the semi-transparent film within which transmissivity ratio T and a phase difference φ between the semi-transparent film and air that has the same thickness of the semi-transparent film fall within ranges necessary to obtain desired resolution and depth of focus; obtaining relationship in the form of a curved line between the refractive index n and the extinction coefficient k by changing composition of a material constituting the mask pattern; selecting values of the refractive index n and the extinction coefficient k from the range thus determined, and determining the composition of the constituting material such that the refractive index n and the extinction coefficient k become the selected values; and forming a mask pattern so that the mask pattern has the composition thus determined.
Claim 11
Independent Claim 170 words
A method of fabricating a reticle comprising the step of forming on a light-transmissible substrate a mask pattern of a semi-transparent film which causes length of an optical path for a light beam passing therethrough to be different from length of an optical path for a light beam passing through the light-transmissible substrate by a predetermined amount, wherein the step of forming a mask pattern comprises the steps of: determining ranges of refractive index n and extinction coefficient k of the semi-transparent film within which transmissivity ratio T and a phase difference φ between the semi-transparent film and air that has the same thickness of the semi-transparent film fall within ranges necessary to obtain desired resolution and depth of focus; determining values of the refractive index n and the extinction coefficient k from the ranges, and selecting a material constituting a mask pattern such that the material has the refractive index n and the extinction coefficient k thus selected; and forming a mask pattern made of the material thus selected.
Claim 12
Independent Claim 170 words
A method of fabricating a reticle comprising the step of forming on a light-transmissible substrate a mask pattern of a semi-transparent film which causes length of an optical path for a light beam passing therethrough to be different from length of an optical path for a light beam passing through the light-transmissible substrate by a predetermined amount, wherein the step of forming a mask pattern comprises the steps of: determining ranges of refractive index n and extinction coefficient k of the semi-transparent film within which transmissivity ratio T and a phase difference φ between the semi-transparent film and air that has the same thickness of the semi-transparent film fall within ranges necessary to obtain desired resolution and depth of focus; determining values of the refractive index n and the extinction coefficient k from the ranges, and selecting a material constituting a mask pattern such that the material has the refractive index n and the extinction coefficient k thus selected; and forming a mask pattern made of the material thus selected.
Claim 13
Dependent Claim 22 words
A method of fabricating a reticle as set forth in claim 8, wherein the material constituting the mask pattern is amorphous silicon.
Claim 14
Independent Claim 291 words
A method of fabricating a reticle comprising the step of forming on a light-transmissible substrate a mask pattern of a semi-transparent film which causes length of an optical path for a light beam passing therethrough to be different from length of an optical path for a light beam passing through the light-transmissible substrate by a predetermined amount, wherein the step of forming the mask pattern comprises the step of: determining refractive index, extinction coefficient and film thickness of a semi-transparent film comprising the steps of: setting the initial value for two of the refractive index, extinction coefficient and film thickness of the semi-transparent film with respect to wavelength of an exposing light beam, an initial value of remaining one of the refractive index, extinction coefficient and film thickness being an arbitrary value; calculating transmissivity ratio and phase difference while considering multiple reflection from the refractive index, extinction coefficient and film thickness of the semi-transparent film and refrcative index, extinction coefficient and film thickness of a substrate and air; comparing the transmissivity ratio and the phase difference thus calculated with the transmissivity ratio T and phase difference required to obtain desired resolution and depth of focus and determining whether errors are smaller than respective predetermined values; and resetting the initial values for two of the refractive index, extinction coefficient and film thickness of the semi-transparent film, wherein, when the errors for the transmissivity ratio T and phase difference are larger than the respective predetermined values, a loop of steps comprising the resetting step, the calculating step and the comparing step are repeatedly performed until it is found that the errors for the transmissivity ratio T and phase difference become smaller than the respective predetermined values as a result of the comparing step.
Claim 15
Independent Claim 291 words
A method of fabricating a reticle comprising the step of forming on a light-transmissible substrate a mask pattern of a semi-transparent film which causes length of an optical path for a light beam passing therethrough to be different from length of an optical path for a light beam passing through the light-transmissible substrate by a predetermined amount, wherein the step of forming the mask pattern comprises the step of: determining refractive index, extinction coefficient and film thickness of a semi-transparent film comprising the steps of: setting the initial value for two of the refractive index, extinction coefficient and film thickness of the semi-transparent film with respect to wavelength of an exposing light beam, an initial value of remaining one of the refractive index, extinction coefficient and film thickness being an arbitrary value; calculating transmissivity ratio and phase difference while considering multiple reflection from the refractive index, extinction coefficient and film thickness of the semi-transparent film and refrcative index, extinction coefficient and film thickness of a substrate and air; comparing the transmissivity ratio and the phase difference thus calculated with the transmissivity ratio T and phase difference required to obtain desired resolution and depth of focus and determining whether errors are smaller than respective predetermined values; and resetting the initial values for two of the refractive index, extinction coefficient and film thickness of the semi-transparent film, wherein, when the errors for the transmissivity ratio T and phase difference are larger than the respective predetermined values, a loop of steps comprising the resetting step, the calculating step and the comparing step are repeatedly performed until it is found that the errors for the transmissivity ratio T and phase difference become smaller than the respective predetermined values as a result of the comparing step.
Claim 16
Dependent Claim 53 words
A method of fabricating a reticle as set forth in claim 1, wherein the step of forming a mask pattern further comprises the step of: forming the semi-transparent film having desired values of amplitude transmissivity ratio and phase difference by a sputtering method based on the conditions for formation of the mask pattern.
Claim 17
Dependent Claim 78 words
A method of fabricating a reticle as set forth in claim 1, wherein the step of forming a mask pattern comprises the step of: depositing the semi-transparent film pattern while adjusting the quantity of oxygen in a raw material gas by using a CVD technique based on the conditions for formation of the mask pattern so as to control a composition ratio, thereby to form a mask pattern having desired values of amplitude transmissivity ratio and phase difference.

References Cited (Backward Citations)

US4068018A Cited
US4686162A Cited
US5045417A Cited
US5126220A Cited
JPH04136854A Cited
JPH05127361A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1999-12-31 2000-07-01 2000-12-31 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2003-12-31 2004-07-01 2004-12-31 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2007-12-31 2008-07-01 2008-12-31 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag