Abstract
Abstract A method of preparing an electrochemical cell wherein the electrode material adheres to the current collector to create good electrical contact is provided. A critical aspect in the process of preparing the polymer mixture for both the anode and cathode slurries is that the polymer (or copolymer) not be subject to high shear so as to be degraded. Polymer degradation contributes to the creation of the polymer concentration gradient in the electrode film.
Inventors
- 👤 Porter H. Mitchell
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-09 10:17
CPC Classifications
H; H01; H01M; H01M4/00; H01M4/02; H01M4/04; H01M4/0402; H01M4/0404; H01M10/00; H01M10/05; H01M10/052; H01M10/056; H01M10/0564; H01M10/0565; H01M4/0416; H01M4/043; H01M4/0435; H01M4/13; H01M4/62; H01M4/621; H01M4/622; H01M4/623; H01M2300/00; H01M2300/0017; H01M2300/0025; Y; Y02; Y02E; Y02E60/00; Y02E60/10; Y02P; Y02P70/00; Y02P70/50; Y10; Y10T; Y10T29/00; Y10T29/49; Y10T29/49002; Y10T29/49108; Y10T29/49115
Claims Analysis
Total Claims: 22
Claim 1
Independent Claim
169 words
A method of preparing an electrochemical cell comprising the steps of: (a) preparing an anode mixture comprising a first polymer, an intercalation carbon material, and a first inert liquid solvent wherein the first polymer is homogeneously distributed within said anode mixture; (b) evaporating the first inert liquid solvent from the anode mixture to form an anode film; (c) preparing a cathode mixture comprising a second polymer, a cathode active material, and a second inert liquid solvent wherein the second polymer is homogeneously distributed with said cathode mixture; (d) evaporating the second liquid solvent from the cathode mixture to form a cathode film; (e) forming anode by laminating said anode film onto at least one side of an anode current collector; (f) forming a cathode by laminating said cathode film onto at least one side of a cathode current collector; (g) interposing a polymeric layer between said anode and cathode; (h) placing an electrolyte solution comprising an electrolyte solvent and an inorganic salt into said anode, cathode, and polymeric layer.
Claim 2
Independent Claim
169 words
A method of preparing an electrochemical cell comprising the steps of: (a) preparing an anode mixture comprising a first polymer, an intercalation carbon material, and a first inert liquid solvent wherein the first polymer is homogeneously distributed within said anode mixture; (b) evaporating the first inert liquid solvent from the anode mixture to form an anode film; (c) preparing a cathode mixture comprising a second polymer, a cathode active material, and a second inert liquid solvent wherein the second polymer is homogeneously distributed with said cathode mixture; (d) evaporating the second liquid solvent from the cathode mixture to form a cathode film; (e) forming anode by laminating said anode film onto at least one side of an anode current collector; (f) forming a cathode by laminating said cathode film onto at least one side of a cathode current collector; (g) interposing a polymeric layer between said anode and cathode; (h) placing an electrolyte solution comprising an electrolyte solvent and an inorganic salt into said anode, cathode, and polymeric layer.
Claim 3
Dependent Claim
33 words
The method of claim 1 wherein the anode mixture, cathode mixture, and polymeric layer each further comprises a plasticizer and said method further comprises the step of removing said plasticizer before step (e).
Claim 4
Dependent Claim
124 words
The method of claim 1 wherein the step of preparing the anode mixture comprises the steps of: (i) mixing the first polymer and a portion of said first inert liquid solvent under low shear conditions; (ii) mixing the intercalation carbon material and a portion of said first inert liquid solvent; and (iii) mixing the mixtures of steps (i) and (ii) under low shear conditions; and wherein the step of preparing the cathode mixture comprises the steps of: (iv) mixing the first polymer and a portion of said second inert liquid solvent under low shear conditions; (v) mixing the cathode active material and a portion of said first inert liquid solvent; and (vi) mixing the mixtures of steps (iv) and (v) under low shear conditions.
Claim 5
Dependent Claim
157 words
The method of claim 1 wherein the anode mixture, cathode mixture, and polymeric layer each further comprises a plasticizer and said method further comprises the step of removing said plasticizer prior to step (h), wherein the step of preparing the anode mixture comprises the steps of: (i) mixing the first polymer and a portion of said first inert liquid solvent under low shear conditions; (ii) mixing the intercalation carbon material, plasticizer, and a portion of said first inert liquid solvent; and (iii) mixing the mixtures produced in steps (i) and (ii) under low shear conditions; and wherein the step of preparing the cathode mixture comprises the steps of: (iv) mixing the first polymer and a portion of said second inert liquid solvent under low shear conditions; (v) mixing the cathode active material, plasticizer, and a portion of said first inert liquid solvent; and (vi) mixing the mixtures produced in steps (iv) and (v) under low shear conditions.
Claim 6
Dependent Claim
13 words
The method of claim 1 wherein said first and second polymers comprise polyvinylidenedifluoride.
Claim 7
Dependent Claim
13 words
The method of claim 1 wherein said first and second solvents comprise acetone.
Claim 8
Dependent Claim
11 words
The method of claim 2 wherein said plasticizer comprises dibutyl phthalate.
Claim 9
Dependent Claim
23 words
The method of claim 1 wherein each of said anode mixture and cathode mixture further comprise an electrically conductive material and a surfactant.
Claim 10
Dependent Claim
28 words
The method of claim 1 wherein the polymeric layer comprises polymeric matrix and third inert liquid solvent, said third inert liquid solvent being removed prior to step (h).
Claim 11
Independent Claim
151 words
A method of preparing an electrochemical cell comprising the steps of: (a) preparing an anode mixture comprising a first polymer, an intercalation carbon material, and a first inert liquid solvent wherein the first polymer is homogeneously distributed within said anode mixture; (b) coating the anode mixture onto at least one side of an anode current conductor layer to form an anode; (c) preparing a cathode mixture comprising a second polymer, a cathode active material, and a second inert liquid solvent wherein the second polymer is homogeneously distributed with said cathode mixture; (d) coating the cathode mixture onto at least one side of a cathode current collector layer to form a cathode; (c) interposing a polymeric layer between said anode and cathode; (d) removing said first and second inert liquid solvents; and (e) placing an electrolyte solution comprising an electrolyte solvent and an inorganic salt into said anode, cathode, and polymeric layer.
Claim 12
Independent Claim
151 words
A method of preparing an electrochemical cell comprising the steps of: (a) preparing an anode mixture comprising a first polymer, an intercalation carbon material, and a first inert liquid solvent wherein the first polymer is homogeneously distributed within said anode mixture; (b) coating the anode mixture onto at least one side of an anode current conductor layer to form an anode; (c) preparing a cathode mixture comprising a second polymer, a cathode active material, and a second inert liquid solvent wherein the second polymer is homogeneously distributed with said cathode mixture; (d) coating the cathode mixture onto at least one side of a cathode current collector layer to form a cathode; (c) interposing a polymeric layer between said anode and cathode; (d) removing said first and second inert liquid solvents; and (e) placing an electrolyte solution comprising an electrolyte solvent and an inorganic salt into said anode, cathode, and polymeric layer.
Claim 13
Dependent Claim
33 words
The method of claim 10 wherein the anode mixture, cathode mixture, and polymeric layer each further comprises a plasticizer and said method further comprises the step of removing said plasticizer before step (e).
Claim 14
Dependent Claim
124 words
The method of claim 10 wherein the step of preparing the anode mixture comprises the steps of: (i) mixing the first polymer and a portion of said first inert liquid solvent under low shear conditions; (ii) mixing the intercalation carbon material and a portion of said first inert liquid solvent; and (iii) mixing the mixtures of steps (i) and (ii) under low shear conditions; and wherein the step of preparing the cathode mixture comprises the steps of: (iv) mixing the first polymer and a portion of said second inert liquid solvent under low shear conditions; (v) mixing the cathode active material and a portion of said first inert liquid solvent; and (vi) mixing the mixtures of steps (iv) and (v) under low shear conditions.
Claim 15
Dependent Claim
157 words
The method of claim 10 wherein the anode mixture, cathode mixture, and electrolyte composition each further comprises a plasticizer and said method further comprises the step of removing said plasticizer prior to step (e), wherein the step of preparing the anode mixture comprises the steps of: (i) mixing the first polymer and a portion of said first inert liquid solvent under low shear conditions; (ii) mixing the intercalation carbon material, plasticizer, and a portion of said first inert liquid solvent; and (iii) mixing the mixtures produced in steps (i) and (ii) under low shear conditions; and wherein the step of preparing the cathode mixture comprises the steps of: (iv) mixing the first polymer and a portion of said second inert liquid solvent under low shear conditions; (v) mixing the cathode active material, plasticizer, and a portion of said first inert liquid solvent; and (vi) mixing the mixtures produced in steps (iv) and (v) under low shear conditions.
Claim 16
Dependent Claim
13 words
The method of claim 10 wherein said first and second polymers comprise polyvinylidenedifluoride.
Claim 17
Dependent Claim
13 words
The method of claim 10 wherein said first and second solvents comprise acetone.
Claim 18
Dependent Claim
11 words
The method of claim 11 wherein said plasticizer comprises dibutyl phthalate.
Claim 19
Dependent Claim
23 words
The method of claim 10 wherein each of said anode mixture and cathode mixture further comprise an electrically conductive material and a surfactant.
Claim 20
Dependent Claim
28 words
The method of claim 10 wherein the polymeric layer comprises polymeric matrix and third inert liquid solvent, said third inert liquid solvent being removed prior to step (e).
Claim 21
Dependent Claim
18 words
The method of claim 1 wherein said first and second polymers comprise a copolymer of polyvinylidenedifluoride and hexafluoropropylene.
Claim 22
Dependent Claim
18 words
The method of claim 10 wherein said first and second polymers comprise a copolymer of polyvinylidenedifluoride and hexafluoropropylene.
References Cited (Backward Citations)
US5219680A
Cited
US5514492A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1999-12-17 | 2000-06-17 | 2000-12-17 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 2003-12-17 | 2004-06-17 | 2004-12-17 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2007-12-17 | 2008-06-17 | 2008-12-17 | $7700.00 | Window Closed / Lapsed |