Claim 1
Independent Claim
271 words
A composite for radiography comprising a) a silver halide photographic light-sensitive material comprising a transparent support and at least one light-sensitive silver halide emulsion layer provided on each side of the support, b) fluorescent screen A having a 80 kVp X-ray energy absorption of 40% or more and c) fluorescent screen B having a 80 kVp X-ray energy absorption of not less than 25% more than fluorescent screen A, the material being sandwiched between the screens A and B in such a manner that emulsion layer A is in close contact with screen A and emulsion layer B is in close contact with screen B, and screen A being positioned on the X-ray radiation source side, wherein the slope of the straight portion in the characteristic curve of emulsion layer A is less than that of emulsion layer B and emulsion layers A and B of the silver halide photographic light-sensitive material have sensitivity on an exposed side that, when the material is exposed to a monochromatic light having the same wavelength as a main emission peak wavelength of the screens and having a half band width of 15±5 nm and developed at 35° C. for 25 seconds with the following developer, an exposure necessary to give a density of the minimum density+0.5 is 0.027 to 0.040 lux·second, ______________________________________
Developer
Potassium hydroxide 21 g
Potassium sulfite 63 g
Boric acid 10 g
Hydroquinone 26 g
Triethylene glycol 16 g
5-methylbenzotriazole
0.06 g
1-phenyl-5-mercaptotetrazole
0.01 g
Glacial acetic acid 12 g
1-phenyl-3-pyrazolidone
1.2 g
Glutaraldehyde 5 g
Potassium bromide 4 g
______________________________________ Water added to 1 liter, and pH adjusted to 10.0.
Claim 2
Dependent Claim
271 words
A composite for radiography comprising a) a silver halide photographic light-sensitive material comprising a transparent support and at least one light-sensitive silver halide emulsion layer provided on each side of the support, b) fluorescent screen A having a 80 kVp X-ray energy absorption of 40% or more and c) fluorescent screen B having a 80 kVp X-ray energy absorption of not less than 25% more than fluorescent screen A, the material being sandwiched between the screens A and B in such a manner that emulsion layer A is in close contact with screen A and emulsion layer B is in close contact with screen B, and screen A being positioned on the X-ray radiation source side, wherein the slope of the straight portion in the characteristic curve of emulsion layer A is less than that of emulsion layer B and emulsion layers A and B of the silver halide photographic light-sensitive material have sensitivity on an exposed side that, when the material is exposed to a monochromatic light having the same wavelength as a main emission peak wavelength of the screens and having a half band width of 15±5 nm and developed at 35° C. for 25 seconds with the following developer, an exposure necessary to give a density of the minimum density+0.5 is 0.027 to 0.040 lux·second, ______________________________________
Developer
Potassium hydroxide 21 g
Potassium sulfite 63 g
Boric acid 10 g
Hydroquinone 26 g
Triethylene glycol 16 g
5-methylbenzotriazole
0.06 g
1-phenyl-5-mercaptotetrazole
0.01 g
Glacial acetic acid 12 g
1-phenyl-3-pyrazolidone
1.2 g
Glutaraldehyde 5 g
Potassium bromide 4 g
______________________________________ Water added to 1 liter, and pH adjusted to 10.0.
Claim 3
Dependent Claim
21 words
The composite of claim 1, wherein sensitivity of the emulsion layer A is higher than that of the emulsion layer B.
Claim 4
Dependent Claim
46 words
The composite of claim 1, wherein a layer reducing a light which emits from one fluorescent screen and arrives at the other emulsion layer of the support opposite the fluorescent screen through the support is provided between the support and the silver halide photographic light-sensitive layer.
Claim 5
Dependent Claim
20 words
The composite of claim 3, wherein said light reducing layer contains a dye, said layer being decolored by said developer.
Claim 6
Dependent Claim
25 words
The composite of claim 4, wherein said light reducing layer contains said dye in an amount of 5 to 300 mg per m 2 .
Claim 7
Dependent Claim
22 words
The composite of claim 1, wherein the filling rate of a fluorescent substance in the fluorescent screens is not less than 65%.
Claim 8
Dependent Claim
21 words
The composite of claim 3, wherein sensitivity of the emulsion layer A is higher than that of the emulsion layer B.
Claim 9
Dependent Claim
22 words
The composite of claim 7, wherein the filling rate of a fluorescent substance in the fluorescent screens is not less than 65%.
Claim 10
Dependent Claim
25 words
The composite of claim 7 wherein the absorption of fluorescent screen B is not less than 30% more than the absorption of fluorescent screen A.
Claim 11
Dependent Claim
25 words
The composite of claim 1 wherein the absorption of fluorescent screen B is not less than 30% more than the absorption of fluorescent screen A.