Abstract
Abstract A magneto-optical disc includes a recording layer (4) and a protective film (7) of radiation-cured resin on a substrate (2). Information is written in the recording layer with the aid of a magnetic head in sliding contact with the disc. In a first form, when the protective film is subject to a micro-vibration scratch test by setting the disc in a thin film scratch tester equipped with a diamond indentor having a radius of curvature R of up to 50 μm, the relationship: 0.8≦L/R 2 ≦2.7 is met wherein L is the critical load (N.m) under which the thin film is scratched. In a second form, the protective film has a dynamic modulus of 5.0×10 9 to 4.0×10 10 dyn/cm 2 at 100° C. The disc is highly durable.
Inventors
- 👤 Tsuyoshi Komaki
- 👤 Hiroyuki Endo
- 👤 Hideki Hirata
- 👤 Isamu Kuribayashi
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-09 16:14
CPC Classifications
G; G11; G11B; G11B11/00; G11B11/10; G11B11/105; G11B11/10582; G11B11/10586; G11B11/10584
Claims Analysis
Total Claims: 13
Claim 1
Independent Claim
103 words
In a magneto-optical disc comprising on a substrate a recording layer and a protective film of radiation-cured resin, wherein information is written in the recording layer with the aid of a magnetic head in sliding contact with the protective film, the improvement wherein in a micro-vibration scratch test made on the protective film by setting the disc in a thin film scratch tester equipped with a diamond indentor having a radius of curvature R (μm) of up to 50 μm, the protective film satisfies the relationship: 0.8≦L/R 2 ≦2.7 wherein L is the critical load (N.m) under which the thin film is scratched.
Claim 2
Dependent Claim
103 words
In a magneto-optical disc comprising on a substrate a recording layer and a protective film of radiation-cured resin, wherein information is written in the recording layer with the aid of a magnetic head in sliding contact with the protective film, the improvement wherein in a micro-vibration scratch test made on the protective film by setting the disc in a thin film scratch tester equipped with a diamond indentor having a radius of curvature R (μm) of up to 50 μm, the protective film satisfies the relationship: 0.8≦L/R 2 ≦2.7 wherein L is the critical load (N.m) under which the thin film is scratched.
Claim 3
Dependent Claim
64 words
In a magneto-optical disc comprising on a substrate a recording layer and a protective film of radiation-cured resin, wherein information is written in the recording layer with the aid of a magnetic head in sliding contact with the protective film, the improvement wherein said protective film of radiation-cured resin has a dynamic modulus of 5.0×10 9 to 4.0×10 10 dyn/cm 2 at 100° C.
Claim 4
Dependent Claim
64 words
In a magneto-optical disc comprising on a substrate a recording layer and a protective film of radiation-cured resin, wherein information is written in the recording layer with the aid of a magnetic head in sliding contact with the protective film, the improvement wherein said protective film of radiation-cured resin has a dynamic modulus of 5.0×10 9 to 4.0×10 10 dyn/cm 2 at 100° C.
Claim 5
Dependent Claim
28 words
The magneto-optical disc of claim 2 wherein said protective film of radiation-cured resin has a dynamic modulus of 2.5×10 9 to 3.0×10 10 dyn/cm 2 at 150° C.
Claim 6
Dependent Claim
21 words
The magneto-optical disc of claim 2 wherein said protective film of radiation-cured resin has a maximum tanδ of up to 0.2.
Claim 7
Dependent Claim
33 words
The magneto-optical disc of claim 1 wherein said protective film of radiation-cured resin is obtained by radiation curing a polymerizable composition comprising 40 to 90% by weight of a trifunctional or polyfunctional monomer.
Claim 8
Dependent Claim
15 words
The magneto-optical disc of claim 1 further comprising a lubricating layer on said protective film.
Claim 9
Dependent Claim
21 words
The magneto-optical disc of claim 1 wherein said magnetic head includes a slider having a dynamic hardness of 5 to 40.
Claim 10
Dependent Claim
21 words
The magneto-optical disk of claim 3, wherein said protective film of radiation-cured resin has a maximum tanδ of up to 0.2.
Claim 11
Dependent Claim
33 words
The magneto-optical disk of claim 2, wherein said protective film of radiation-cured resin is obtained by radiation curing a polymerizable composition comprising 40 to 90% by weight of a trifunctional or polyfunctional monomer.
Claim 12
Dependent Claim
15 words
The magneto-optical disk of claim 2, further comprising a lubricating layer on said protective film.
Claim 13
Dependent Claim
21 words
The magneto-optical disk of claim 2, wherein said magnetic head includes a slider having a dynamic hardness of 5 to 40.
References Cited (Backward Citations)
US4694358A
Cited
US5237548A
Cited
JPH0210540A
Cited
US5492773A
Cited
US5020048A
Cited
US5266409A
Cited
US5353278A
Cited
JPH04195746A
Cited
JPH04195747A
Cited
JPH04195748A
Cited
JPH04195749A
Cited
JPH04195943A
Cited
JPH04195944A
Cited
US5202220A
Cited
US5342669A
Cited
JPH05210877A
Cited
JPH0528559A
Cited
JPH0536131A
Cited
US5416754A
Cited
JPH05210883A
Cited
JPH05303784A
Cited
JPH05242542A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1999-10-22 | 2000-04-22 | 2000-10-22 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 2003-10-22 | 2004-04-22 | 2004-10-22 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2007-10-22 | 2008-04-22 | 2008-10-22 | $7700.00 | Window Closed / Lapsed |