Abstract
Abstract Bituminous compositions are provided by mixing 100 parts of an inorganic skeleton or an aggregate with up to 7 parts of bitumen with a first modifier chosen from the group comprising styrene-butadiene polymers, styrene-isoprene polymers, recycled tires or any mixtures thereof, and a second modifier selected from the group comprising polyolefins, polyethylene terephthalate or any mixtures thereof. The present composition allows the utilization of large amounts of recycled plastics.
Inventors
- 👤 Pierre Bredael
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-07 05:45
CPC Classifications
E; E01; E01C; E01C11/00; E01C11/22; E01C11/224; E01C11/225; E01C11/226; C; C08; C08L; C08L95/00; E01C7/00; E01C7/08; E01C7/18; E01C7/26; E01C7/265; Y; Y10; Y10S; Y10S106/00; Y10S106/07
Claims Analysis
Total Claims: 11
Claim 1
Independent Claim
158 words
A composition comprising: (A) 100 parts of an aggregate comprising (i) from 79 to 88 parts by weight of macadam having a particle size of between 6 and 17 mm, (ii) from 9 to 15 parts by weight of sand having a particle size of between 0.08 and 2 mm, and (iii) from 3 to 8 parts by weight of inert filling material having a particle size smaller than 0.08 mm; (B) from 3.5 to 7 parts by weight based on the aggregate of bitumen which has a penetration value from 65 to 150 tenths of millimeter at 25° C.; (C) from 2 to 7% by weight of the bitumen of a first modifier chosen from the group consisting of styrene-butadiene polymers, styrene-isoprene polymers, recycled tires and mixtures thereof; and (D) from 0.5 to 5 parts by weight based on the aggregate of a second modifier chosen from the group consisting of polyolefins, polyethylene terephthalate and mixtures thereof.
Claim 2
Dependent Claim
158 words
A composition comprising: (A) 100 parts of an aggregate comprising (i) from 79 to 88 parts by weight of macadam having a particle size of between 6 and 17 mm, (ii) from 9 to 15 parts by weight of sand having a particle size of between 0.08 and 2 mm, and (iii) from 3 to 8 parts by weight of inert filling material having a particle size smaller than 0.08 mm; (B) from 3.5 to 7 parts by weight based on the aggregate of bitumen which has a penetration value from 65 to 150 tenths of millimeter at 25° C.; (C) from 2 to 7% by weight of the bitumen of a first modifier chosen from the group consisting of styrene-butadiene polymers, styrene-isoprene polymers, recycled tires and mixtures thereof; and (D) from 0.5 to 5 parts by weight based on the aggregate of a second modifier chosen from the group consisting of polyolefins, polyethylene terephthalate and mixtures thereof.
Claim 3
Dependent Claim
62 words
The compositions according to claim 1, in which the aggregate comprises: (i) from 81 to 85 parts of macadam having a particle size of between 7 and 14 mm, (ii) from 11 to 13 parts having a particle size of between 0.08 and 2 mm, and (iii) from 4 to 6 parts of filling material of particle size smaller than 0.08 mm.
Claim 4
Dependent Claim
20 words
The compositions according to claim 1, wherein the bitumen has a penetration value from 80 to 100 tenths of millimeter.
Claim 5
Dependent Claim
26 words
The compositions according to claim 1, in which the first modifier is introduced in a quantity corresponding to 4 to 7 weight percent of the bitumen.
Claim 6
Dependent Claim
28 words
The compositions according to claim 1, in which the second modifier is introduced in a quantity corresponding to 0.5 to 3 parts by weight based on the aggregate.
Claim 7
Dependent Claim
177 words
A process for the preparation of an asphalt composition, comprising introducing into a mixer, at temperatures of between 130° and 185° C., (A) 100 parts of an aggregate comprising (i) from 79 to 88 parts by weight of macadam having a particle size of between 6 and 17 mm, (ii) from 9 to 15 parts by weight of sand having a particle size of between 0.08 and 2 mm, and (iii) from 3 to 8 parts by weight of inert filling material having a particle size smaller than 0.08 mm; (B) from 3.5 to 7 parts by weight based on the aggregate of bitumen which has a penetration value from 65 to 150 tenths of millimeter at 25° C.; (C) from 2 to 7% by weight of the bitumen of a first modifier chosen from the group consisting of styrene-butadiene polymers, styrene-isoprene polymers, recycled tires and mixtures thereof; and (D) from 0.5 to 5 parts by weight based on the aggregate of a second modifier chosen from the group consisting of polyolefins, polyethylene terephthalate and mixtures thereof.
Claim 8
Dependent Claim
177 words
A process for the preparation of an asphalt composition, comprising introducing into a mixer, at temperatures of between 130° and 185° C., (A) 100 parts of an aggregate comprising (i) from 79 to 88 parts by weight of macadam having a particle size of between 6 and 17 mm, (ii) from 9 to 15 parts by weight of sand having a particle size of between 0.08 and 2 mm, and (iii) from 3 to 8 parts by weight of inert filling material having a particle size smaller than 0.08 mm; (B) from 3.5 to 7 parts by weight based on the aggregate of bitumen which has a penetration value from 65 to 150 tenths of millimeter at 25° C.; (C) from 2 to 7% by weight of the bitumen of a first modifier chosen from the group consisting of styrene-butadiene polymers, styrene-isoprene polymers, recycled tires and mixtures thereof; and (D) from 0.5 to 5 parts by weight based on the aggregate of a second modifier chosen from the group consisting of polyolefins, polyethylene terephthalate and mixtures thereof.
Claim 9
Dependent Claim
22 words
The process according to claim 6, in which the components are introduced into the mixer at a temperature of approximately 140° C.
Claim 10
Dependent Claim
131 words
A process for the preparation of an asphalt composition, comprising introducing into a mixer, at temperatures of between 130° and 185° C., (A) 100 parts of an aggregate comprising (i) from 79 to 88 parts by weight of macadam having a particle size of between 6 and 17 mm, (ii) from 9 to 15 parts by weight of sand having a particle size of between 0.08 and 2 mm, and (iii) from 3 to 8 parts by weight of inert filling material having a particle size smaller than 0.08 mm; (B) a homogeneous modified bitumen-copolymer binder premixed at 150° C. to 180° C., and (C) from 0.5 to 5 parts by weight based on the aggregate of a modifier chosen from the group consisting of polyolefins, polyethylene terephthalate and mixtures thereof.
Claim 11
Dependent Claim
131 words
A process for the preparation of an asphalt composition, comprising introducing into a mixer, at temperatures of between 130° and 185° C., (A) 100 parts of an aggregate comprising (i) from 79 to 88 parts by weight of macadam having a particle size of between 6 and 17 mm, (ii) from 9 to 15 parts by weight of sand having a particle size of between 0.08 and 2 mm, and (iii) from 3 to 8 parts by weight of inert filling material having a particle size smaller than 0.08 mm; (B) a homogeneous modified bitumen-copolymer binder premixed at 150° C. to 180° C., and (C) from 0.5 to 5 parts by weight based on the aggregate of a modifier chosen from the group consisting of polyolefins, polyethylene terephthalate and mixtures thereof.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1999-09-24 | 2000-03-25 | 2000-09-24 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 2003-09-24 | 2004-03-25 | 2004-09-24 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2007-09-24 | 2008-03-25 | 2008-09-24 | $7700.00 | Window Closed / Lapsed |