Abstract

Abstract Bituminous compositions are provided by mixing 100 parts of an inorganic skeleton or an aggregate with up to 7 parts of bitumen with a first modifier chosen from the group comprising styrene-butadiene polymers, styrene-isoprene polymers, recycled tires or any mixtures thereof, and a second modifier selected from the group comprising polyolefins, polyethylene terephthalate or any mixtures thereof. The present composition allows the utilization of large amounts of recycled plastics.

Inventors

  • 👤 Pierre Bredael

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-07 05:28
CPC Classifications
E; E01; E01C; E01C11/00; E01C11/22; E01C11/224; E01C11/225; E01C11/226; C; C08; C08L; C08L95/00; E01C7/00; E01C7/08; E01C7/18; E01C7/26; E01C7/265; Y; Y10; Y10S; Y10S106/00; Y10S106/07

Claims Analysis

Total Claims: 11
Claim 1
Independent Claim 158 words
A composition comprising: (A) 100 parts of an aggregate comprising (i) from 79 to 88 parts by weight of macadam having a particle size of between 6 and 17 mm, (ii) from 9 to 15 parts by weight of sand having a particle size of between 0.08 and 2 mm, and (iii) from 3 to 8 parts by weight of inert filling material having a particle size smaller than 0.08 mm; (B) from 3.5 to 7 parts by weight based on the aggregate of bitumen which has a penetration value from 65 to 150 tenths of millimeter at 25° C.; (C) from 2 to 7% by weight of the bitumen of a first modifier chosen from the group consisting of styrene-butadiene polymers, styrene-isoprene polymers, recycled tires and mixtures thereof; and (D) from 0.5 to 5 parts by weight based on the aggregate of a second modifier chosen from the group consisting of polyolefins, polyethylene terephthalate and mixtures thereof.
Claim 2
Dependent Claim 158 words
A composition comprising: (A) 100 parts of an aggregate comprising (i) from 79 to 88 parts by weight of macadam having a particle size of between 6 and 17 mm, (ii) from 9 to 15 parts by weight of sand having a particle size of between 0.08 and 2 mm, and (iii) from 3 to 8 parts by weight of inert filling material having a particle size smaller than 0.08 mm; (B) from 3.5 to 7 parts by weight based on the aggregate of bitumen which has a penetration value from 65 to 150 tenths of millimeter at 25° C.; (C) from 2 to 7% by weight of the bitumen of a first modifier chosen from the group consisting of styrene-butadiene polymers, styrene-isoprene polymers, recycled tires and mixtures thereof; and (D) from 0.5 to 5 parts by weight based on the aggregate of a second modifier chosen from the group consisting of polyolefins, polyethylene terephthalate and mixtures thereof.
Claim 3
Dependent Claim 62 words
The compositions according to claim 1, in which the aggregate comprises: (i) from 81 to 85 parts of macadam having a particle size of between 7 and 14 mm, (ii) from 11 to 13 parts having a particle size of between 0.08 and 2 mm, and (iii) from 4 to 6 parts of filling material of particle size smaller than 0.08 mm.
Claim 4
Dependent Claim 20 words
The compositions according to claim 1, wherein the bitumen has a penetration value from 80 to 100 tenths of millimeter.
Claim 5
Dependent Claim 26 words
The compositions according to claim 1, in which the first modifier is introduced in a quantity corresponding to 4 to 7 weight percent of the bitumen.
Claim 6
Dependent Claim 28 words
The compositions according to claim 1, in which the second modifier is introduced in a quantity corresponding to 0.5 to 3 parts by weight based on the aggregate.
Claim 7
Dependent Claim 177 words
A process for the preparation of an asphalt composition, comprising introducing into a mixer, at temperatures of between 130° and 185° C., (A) 100 parts of an aggregate comprising (i) from 79 to 88 parts by weight of macadam having a particle size of between 6 and 17 mm, (ii) from 9 to 15 parts by weight of sand having a particle size of between 0.08 and 2 mm, and (iii) from 3 to 8 parts by weight of inert filling material having a particle size smaller than 0.08 mm; (B) from 3.5 to 7 parts by weight based on the aggregate of bitumen which has a penetration value from 65 to 150 tenths of millimeter at 25° C.; (C) from 2 to 7% by weight of the bitumen of a first modifier chosen from the group consisting of styrene-butadiene polymers, styrene-isoprene polymers, recycled tires and mixtures thereof; and (D) from 0.5 to 5 parts by weight based on the aggregate of a second modifier chosen from the group consisting of polyolefins, polyethylene terephthalate and mixtures thereof.
Claim 8
Dependent Claim 177 words
A process for the preparation of an asphalt composition, comprising introducing into a mixer, at temperatures of between 130° and 185° C., (A) 100 parts of an aggregate comprising (i) from 79 to 88 parts by weight of macadam having a particle size of between 6 and 17 mm, (ii) from 9 to 15 parts by weight of sand having a particle size of between 0.08 and 2 mm, and (iii) from 3 to 8 parts by weight of inert filling material having a particle size smaller than 0.08 mm; (B) from 3.5 to 7 parts by weight based on the aggregate of bitumen which has a penetration value from 65 to 150 tenths of millimeter at 25° C.; (C) from 2 to 7% by weight of the bitumen of a first modifier chosen from the group consisting of styrene-butadiene polymers, styrene-isoprene polymers, recycled tires and mixtures thereof; and (D) from 0.5 to 5 parts by weight based on the aggregate of a second modifier chosen from the group consisting of polyolefins, polyethylene terephthalate and mixtures thereof.
Claim 9
Dependent Claim 22 words
The process according to claim 6, in which the components are introduced into the mixer at a temperature of approximately 140° C.
Claim 10
Dependent Claim 131 words
A process for the preparation of an asphalt composition, comprising introducing into a mixer, at temperatures of between 130° and 185° C., (A) 100 parts of an aggregate comprising (i) from 79 to 88 parts by weight of macadam having a particle size of between 6 and 17 mm, (ii) from 9 to 15 parts by weight of sand having a particle size of between 0.08 and 2 mm, and (iii) from 3 to 8 parts by weight of inert filling material having a particle size smaller than 0.08 mm; (B) a homogeneous modified bitumen-copolymer binder premixed at 150° C. to 180° C., and (C) from 0.5 to 5 parts by weight based on the aggregate of a modifier chosen from the group consisting of polyolefins, polyethylene terephthalate and mixtures thereof.
Claim 11
Dependent Claim 131 words
A process for the preparation of an asphalt composition, comprising introducing into a mixer, at temperatures of between 130° and 185° C., (A) 100 parts of an aggregate comprising (i) from 79 to 88 parts by weight of macadam having a particle size of between 6 and 17 mm, (ii) from 9 to 15 parts by weight of sand having a particle size of between 0.08 and 2 mm, and (iii) from 3 to 8 parts by weight of inert filling material having a particle size smaller than 0.08 mm; (B) a homogeneous modified bitumen-copolymer binder premixed at 150° C. to 180° C., and (C) from 0.5 to 5 parts by weight based on the aggregate of a modifier chosen from the group consisting of polyolefins, polyethylene terephthalate and mixtures thereof.

References Cited (Backward Citations)

US1565258A Cited
US3206319A Cited
US3986889A Cited
US3824109A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1999-09-24 2000-03-25 2000-09-24 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2003-09-24 2004-03-25 2004-09-24 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2007-09-24 2008-03-25 2008-09-24 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag