Patent US4890147A successfully refreshed from Google Patents.
Patent US5541948A successfully refreshed from Google Patents.
← Back to Patent Explorer
US5541948A Expired / Lapsed US ⏱️ 0.0 years remaining

Transition-metal doped sulfide, selenide, and telluride laser crystal and lasers

Assignee: University of California
•
Filing: 1994-11-28
•
Granted: 1996-07-30
•
Expires: 2014-11-28
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A new class of solid state laser crystals and lasers are formed of transition metal doped sulfide, selenide, and telluride host crystals which have four fold coordinated substitutional sites. The host crystals include II-VI compounds. The host crystal is doped with a transition metal laser ion, e.g., chromium, cobalt or iron. In particular, Cr 2+ -doped ZnS and ZnSe generate laser action near 2.3 μm. Oxide, chloride, fluoride, bromide and iodide crystals with similar structures can also be used. Important aspects of these laser materials are the tetrahedral site symmetry of the host crystal, low excited state absorption losses and high luminescence efficiency, and the d 4 and d 6 electronic configurations of the transition metal ions. The same materials are also useful as saturable absorbers for passive Q-switching applications. The laser materials can be used as gain media in amplifiers and oscillators; these gain media can be incorporated into waveguides and semiconductor lasers.

Inventors

  • 👤 William F. Krupke
  • 👤 Ralph H. Page
  • 👤 Laura D. DeLoach
  • 👤 Stephen A. Payne

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 14:23
CPC Classifications
H; H01; H01S; H01S3/00; H01S3/14; H01S3/16; H01S3/10; H01S3/106; H01S3/108; H01S3/109; H01S3/1095; H01S3/11; H01S3/1106; H01S3/1112; H01S3/1685; H01S3/1601; H01S3/162; H01S3/1621; H01S3/1623; H01S3/1628

Claims Analysis

Total Claims: 24
Claim 1
Independent Claim 103 words
A laser gain medium comprising: a host material selected from the group consisting of sulfides, selenides, and tellurides, and a transition metal ion dopant in the host material, wherein: said transition metal ion dopant is selected from the group consisting of Ti, V, Cr, Mn, Fe, Co, Ni, and Cu; said host material has a crystal structure having four fold coordinated substitutional sites; said transition metal ion dopant is substituted at said four-fold coordinated sites: and excitation means associated with the host material and transition metal ion dopant for pumping optical energy directly to the energy levels of the transition metal ion dopant.
Claim 2
Dependent Claim 103 words
A laser gain medium comprising: a host material selected from the group consisting of sulfides, selenides, and tellurides, and a transition metal ion dopant in the host material, wherein: said transition metal ion dopant is selected from the group consisting of Ti, V, Cr, Mn, Fe, Co, Ni, and Cu; said host material has a crystal structure having four fold coordinated substitutional sites; said transition metal ion dopant is substituted at said four-fold coordinated sites: and excitation means associated with the host material and transition metal ion dopant for pumping optical energy directly to the energy levels of the transition metal ion dopant.
Claim 3
Dependent Claim 51 words
The laser gain medium of claim 1, wherein said host material is a II-VI compound having the formula MX, where M is a divalent cation selected from the group consisting of Mg, Zn, and Cd, and X is a divalent anion selected from the group consisting of S, Se and Te.
Claim 4
Dependent Claim 15 words
The laser gain medium of claim 2, wherein said gain medium is a polycrystalline material.
Claim 5
Dependent Claim 25 words
The laser gain medium of claim 2, wherein said host material is selected from the group consisting of ZnS, ZnSe, ZnTe, CdS, CdSe and CdTe.
Claim 6
Dependent Claim 16 words
The laser gain medium of claim 4 wherein the transition metal ion is Cr 2+ .
Claim 7
Dependent Claim 16 words
The laser gain medium of claim 4 wherein the transition metal ion is Fe 2+ .
Claim 8
Dependent Claim 58 words
The laser gain medium of claim 1, wherein said host material has the formula MY 2 X 4 , where M is selected from the group consisting of Zn, Cd, Ca, Sr and Ba, Y is selected from the group consisting of Ga and In, and X is selected from the group consisting of S, Se and Te.
Claim 9
Dependent Claim 103 words
A laser gain medium comprising: a host material selected from the group consisting of oxides, sulfides, selenides, tellurides, fluorides, chlorides, bromides, and iodides, and a transition metal ion dopant in the host material, wherein: said transition metal ion is characterized by the 3d 4 , 4d 4 , 5d 4 , 3d 6 , 4d 6 , or 5d 6 electronic structure and by ground and excited states described by 5 T 2 and 5 E tetrahedral symmetries; said host material has a crystal structure having four fold coordinated substitutional sites; said transition metal ion dopant is substituted at said four-fold coordinated sites.
Claim 10
Dependent Claim 103 words
A laser gain medium comprising: a host material selected from the group consisting of oxides, sulfides, selenides, tellurides, fluorides, chlorides, bromides, and iodides, and a transition metal ion dopant in the host material, wherein: said transition metal ion is characterized by the 3d 4 , 4d 4 , 5d 4 , 3d 6 , 4d 6 , or 5d 6 electronic structure and by ground and excited states described by 5 T 2 and 5 E tetrahedral symmetries; said host material has a crystal structure having four fold coordinated substitutional sites; said transition metal ion dopant is substituted at said four-fold coordinated sites.
Claim 11
Dependent Claim 45 words
The laser gain medium of claim 8 wherein: said host material is selected from the group consisting of sulfide, selenide and telluride host materials; said transition metal ion dopant is selected from the group consisting of Ti, V, Cr, Mn, Fe, Co, Ni, and Cu.
Claim 12
Dependent Claim 16 words
The laser gain medium of claim 8 wherein the transition metal ion is Cr 2+ .
Claim 13
Dependent Claim 88 words
An optical element comprising: an intracavity saturable absorber for use in a laser and formed of a transition metal ion doped host material, wherein: said transition metal ion is selected from the group consisting of Ti, V, Cr, Mn, Fe, Co, Ni and Cu; and said host material is a II-VI compound having the formula MX, where M is a divalent cation selected from the group consisting of Mg, Zn and Cd, and X is a divalent anion selected from the group consisting of S, Se and Te.
Claim 14
Dependent Claim 88 words
An optical element comprising: an intracavity saturable absorber for use in a laser and formed of a transition metal ion doped host material, wherein: said transition metal ion is selected from the group consisting of Ti, V, Cr, Mn, Fe, Co, Ni and Cu; and said host material is a II-VI compound having the formula MX, where M is a divalent cation selected from the group consisting of Mg, Zn and Cd, and X is a divalent anion selected from the group consisting of S, Se and Te.
Claim 15
Dependent Claim 14 words
The saturable absorber of claim 11, wherein said saturable absorber is a polycrystalline material.
Claim 16
Dependent Claim 41 words
The saturable absorber of claim 11 wherein the transition metal ion is selected from the group consisting of Cr 2+ and Fe 2+ and the host material is selected from the group consisting of ZnS, ZnSe, ZnTe, CdS, CdSe and CdTe.
Claim 17
Dependent Claim 148 words
A solid state laser, comprising: a laser gain medium comprising: a host material selected from the group consisting of oxides, sulfides, selenides, tellurides, fluorides, chlorides, bromides, and iodides, and a transition metal ion dopant in the host material, wherein: said transition metal ion is characterized by the 3d 4 ,4d 4 , 5d 4 , 3d 6 , 4d 6 , or 5d 6 electronic structure and by ground and excited states described by 5 T 2 and 5 E tetrahedral symmetries; said host material has a crystal structure having four fold coordinated substitutional sites; said transition metal ion dopant is substituted at said four-fold coordinated sites; excitation means associated with the gain medium for pumping the gain medium; cavity forming means surrounding the gain medium to form a resonant laser cavity; energy extraction means associated with the cavity forming means to remove laser energy from the cavity.
Claim 18
Dependent Claim 148 words
A solid state laser, comprising: a laser gain medium comprising: a host material selected from the group consisting of oxides, sulfides, selenides, tellurides, fluorides, chlorides, bromides, and iodides, and a transition metal ion dopant in the host material, wherein: said transition metal ion is characterized by the 3d 4 ,4d 4 , 5d 4 , 3d 6 , 4d 6 , or 5d 6 electronic structure and by ground and excited states described by 5 T 2 and 5 E tetrahedral symmetries; said host material has a crystal structure having four fold coordinated substitutional sites; said transition metal ion dopant is substituted at said four-fold coordinated sites; excitation means associated with the gain medium for pumping the gain medium; cavity forming means surrounding the gain medium to form a resonant laser cavity; energy extraction means associated with the cavity forming means to remove laser energy from the cavity.
Claim 19
Dependent Claim 43 words
The solid state laser of claim 14, wherein: the host material is selected from the group consisting of sulfide, selenide and, telluride host materials; the transition metal ion dopant is selected from consisting of Ti, V, Cr, Mn, Fe, Co, Ni, and Cu.
Claim 20
Dependent Claim 51 words
The solid state laser of claim 15, wherein said host material is a II-VI compound having the formula MX, where M is a divalent cation selected from the group consisting of Mg, Zn, and Cd, and X is a divalent anion selected from the group consisting of S, Se and Te.
Claim 21
Dependent Claim 15 words
The solid state laser of claim 16, wherein said gain medium is a polycrystalline material.
Claim 22
Dependent Claim 21 words
The solid state laser of claim 16, wherein said host material is selected from ZnS, ZnSe, ZnTe, CdS, CdSe and CdTe.
Claim 23
Dependent Claim 25 words
The solid state laser of claim 18 wherein the transition metal ion is selected from the group consisting of Cr 2+ and Fe 2+ .
Claim 24
Dependent Claim 58 words
The solid state laser of claim 15, wherein said host material has the formula MY 2 X 4 , where M is selected from the group consisting of Zn, Cd, Ca, Sr and Ba, Y is selected from the group consisting of Ga and In, and X is selected from the group consisting of S, Se and Te.

References Cited (Backward Citations)

US4081763A Cited
US4000247A Cited
US4377864A Cited
US4627064A Cited
US4648094A Cited
US4935934A Cited
US4987575A Cited
US5140604A Cited
US5173911A Cited
US5166948A Cited
US5319653A Cited
US5287373A Cited
US5422907A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1999-07-30 2000-01-29 2000-07-30 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2003-07-30 2004-01-29 2004-07-30 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2007-07-30 2008-01-29 2008-07-30 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag