Abstract

Abstract Chemical vapor deposition apparatus is provided for the quick and efficient deposition of Parylene AF4 onto silicon wafers in the production of semiconductor chips. A method of depositing parylene AF4 onto the surface of a semiconductor wafer includes cooling the semiconductor chip wafer to a temperature below 0° C., creating an inert atmosphere around the apparatus, creating sub-atmospheric pressure conditions around the wafer while maintaining the inert external atmosphere, and depositing a predetermined thickness of the parylene AF4 polymer onto the wafer. The method further includes the steps of heating the wafer back to room temperature prior to removing the wafer from the sub-atmospheric conditions, and may still further include the steps of further heating the wafer to a predetermined annealing temperature, and the cooling the wafer back to room temperature prior to removing the wafer from the sub-atmospheric conditions.

Inventors

  • 👤 William F. Beach
  • 👤 Roger A. Olson
  • 👤 John Wary

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 19:56
CPC Classifications
C; C23; C23C; C23C16/00; C23C16/44; C23C16/46; C23C16/463; B; B05; B05D; B05D1/00; B05D1/60; C08; C08G; C08G61/00; C08G61/02; C08G61/025; C23C16/4412; C23C16/448; C23C16/4485; C23C16/52; C08G2261/00; C08G2261/30; C08G2261/34; C08G2261/342; C08G2261/3424

Claims Analysis

Total Claims: 15
Claim 1
Independent Claim 59 words
A method for the deposition of a parylene polymer onto a substrate comprising the steps of: cooling the substrate to a temperature below 0° C.; creating sub-atmospheric pressure conditions around said substrate; depositing a predetermined thickness of said parylene polymer onto said substrate; and heating said substrate to room temperature prior to removing said substrate from said sub-atmospheric conditions.
Claim 2
Independent Claim 59 words
A method for the deposition of a parylene polymer onto a substrate comprising the steps of: cooling the substrate to a temperature below 0° C.; creating sub-atmospheric pressure conditions around said substrate; depositing a predetermined thickness of said parylene polymer onto said substrate; and heating said substrate to room temperature prior to removing said substrate from said sub-atmospheric conditions.
Claim 3
Dependent Claim 42 words
The method of claim 1 wherein said step of cooling said substrate comprises the step of disposing said substrate on the surface of a thermally conductive platen and cooling said platen to a predetermined temperature whereby said substrate is cooled by conduction.
Claim 4
Dependent Claim 24 words
The method of claim 2 wherein said step of cooling said substrate further comprises clamping said substrate in intimate thermal contact with said platen.
Claim 5
Dependent Claim 16 words
The method of claim 3, wherein said further step of clamping comprises electrostatically clamping said substrate.
Claim 6
Dependent Claim 39 words
The method of claim 1 wherein said step of depositing said parylene comprises the steps of vaporizing a parylene dimer at a predetermined temperature, pyrolyzing said vaporized dimer into its monomer form, and polymerizing said monomer onto said substrate.
Claim 7
Dependent Claim 23 words
The method of claim 1 further comprising the step of heating said substrate to a predetermined annealing temperature after depositing said parylene polymer.
Claim 8
Dependent Claim 30 words
The method of claim 6 further comprising the step of cooling said substrate back to room temperature from said annealing temperature prior to removing said substrate from said sub-atmospheric conditions.
Claim 9
Independent Claim 77 words
A method for the deposition of a parylene polymer onto a substrate comprising the steps of: disposing said substrate in a deposition chamber; cooling a substrate to a temperature below 0° C.; creating a substantially inert atmosphere externally of deposition chamber; creating sub-atmospheric pressure conditions within said deposition chamber while maintaining said inert external atmosphere; and depositing a predetermined thickness of a parylene polymer onto said substrate to form a polymer film while maintaining said inert atmosphere.
Claim 10
Independent Claim 77 words
A method for the deposition of a parylene polymer onto a substrate comprising the steps of: disposing said substrate in a deposition chamber; cooling a substrate to a temperature below 0° C.; creating a substantially inert atmosphere externally of deposition chamber; creating sub-atmospheric pressure conditions within said deposition chamber while maintaining said inert external atmosphere; and depositing a predetermined thickness of a parylene polymer onto said substrate to form a polymer film while maintaining said inert atmosphere.
Claim 11
Dependent Claim 25 words
The method of claim 8 further comprising the step of heating said substrate to room temperature prior to removing said substrate from said sub-atmospheric conditions.
Claim 12
Dependent Claim 24 words
The method of claim 9 further comprising the step of further heating said substrate to a predetermined annealing temperature to anneal said polymer film.
Claim 13
Dependent Claim 28 words
The method of claim 10 further comprising the step of cooling said substrate back to room temperature from said annealing temperature prior to removal from said sub-atmospheric conditions.
Claim 14
Independent Claim 65 words
A method for the deposition of a parylene polymer onto a substrate comprising the steps of: disposing said substrate in a deposition chamber; creating a substantially inert atmosphere externally of the deposition chamber; creating sub-atmospheric pressure conditions within said deposition chamber while maintaining said inert external atmosphere; and depositing a predetermined thickness of a parylene polymer onto said substrate while maintaining said inert external atmosphere.
Claim 15
Independent Claim 65 words
A method for the deposition of a parylene polymer onto a substrate comprising the steps of: disposing said substrate in a deposition chamber; creating a substantially inert atmosphere externally of the deposition chamber; creating sub-atmospheric pressure conditions within said deposition chamber while maintaining said inert external atmosphere; and depositing a predetermined thickness of a parylene polymer onto said substrate while maintaining said inert external atmosphere.

References Cited (Backward Citations)

US3246627A Cited
US4495889A Cited
US4683143A Cited
US4945856A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1999-07-23 2000-01-22 2000-07-23 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2003-07-23 2004-01-22 2004-07-23 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2007-07-23 2008-01-22 2008-07-23 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag