Process for producing an organic electroluminescence device

Assignee: Idemitsu Kosan Co Ltd
•
Filing: 1995-01-20
•
Granted: 1996-04-09
•
Expires: 2015-01-20
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A process for producing an organic electroluminescent device, comprising (a) preparing a laminated structure including at least a light-emitting layer formed of a luminescent organic solid which is disposed between mutually opposing positive and negative electrodes, the luminescent organic solid being implantable with electrons from the negative electrode and holes from the positive electrode when direct current is charged between the positive electrode and the negative electrode and thereby having an excited state therein to recombine the electrons and the holes injected into the luminescent organic solid for light emission, and (b) depositing a film of an electrically insulating polymer compound as a protection layer on an outer surface of the laminated structure, wherein the electrically insulating polymer is heated to a temperature of not more than 600 DEG C. and the protection layer is deposited at a rate of not more than 50 nm/second, wherein the layers beginning from a layer directly disposed on a lower electrode of said positive and negative electrodes and continuing to the protection layer are disposed without breaking a vacuum environment in a vacuum chamber and where the pressure in the vacuum chamber is not more than 1x10-2 Pa prior to each of the layers being disposed.

Inventors

  • 👤 Hiroaki Nakamura
  • 👤 Masahide Matsuura
  • 👤 Tadashi Kusumoto

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 18:12
CPC Classifications
H; H05; H05B; H05B33/00; H05B33/10; H05B33/02; H05B33/04; H10; H10K; H10K50/00; H10K50/80; H10K50/84; H10K50/842; H10K50/8426; H10K50/844; H10K50/846; H10K59/00; H10K59/80; H10K59/87; H10K59/871; H10K59/872; H10K59/8722; H10K59/873; H10K59/874; Y; Y10; Y10S; Y10S428/00; Y10S428/917; Y10T; Y10T428/00; Y10T428/24; Y10T428/24802; Y10T428/24917; Y10T428/31504; Y10T428/3154; Y10T428/31544

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 280 words
A process for producing an organic electroluminescent device, comprising (a) preparing a laminated structure including at least a light-emitting layer formed of a luminescent organic solid which is disposed between mutually opposing positive and negative electrodes, the luminescent organic solid being implantable with electrons from the negative electrode and holes from the positive electrode when direct current is charged between the positive electrode and the negative electrode and thereby having an excited state therein to recombine the electrons and the holes injected into the luminescent organic solid for light emission, and (b) depositing a film of an electrically insulating polymer compound as a protection layer on an outer surface of the laminated structure, the electrically insulating polymer compound being selected from the group consisting of (i) a fluorine-free polymer compound selected from the group consisting of polyethylene, polypropylene, polystyrene, polymethyl methacrylate, polyurea and polyimide, (ii) a compound having a molecular weight not less than 400 selected from the group consisting of polytetrafluoroethylene, polychlorotrifluoroethylene, polydicholorodifluoroethylene and a copolymer of chlorotrifluoroethylene and dichlorodifluoroethylene and (iii) a fluorine-containing copolymer having a main chain including a cyclic structure, wherein a deposition source of the electrically insulating polymer is heated to a temperature of not more than 600° C. and the protection layer is deposited at a rate of not more than 50 nm/second, wherein said layers beginning from a layer directly disposed on a lower electrode of said positive and negative electrodes and continuing to said protection layer are disposed without breaking a vacuum environment in a vacuum chamber and where the pressure in the vacuum chamber is maintained at not more than 1×10 -2 Pa prior to each of said layers being disposed.
Claim 2
Dependent Claim 280 words
A process for producing an organic electroluminescent device, comprising (a) preparing a laminated structure including at least a light-emitting layer formed of a luminescent organic solid which is disposed between mutually opposing positive and negative electrodes, the luminescent organic solid being implantable with electrons from the negative electrode and holes from the positive electrode when direct current is charged between the positive electrode and the negative electrode and thereby having an excited state therein to recombine the electrons and the holes injected into the luminescent organic solid for light emission, and (b) depositing a film of an electrically insulating polymer compound as a protection layer on an outer surface of the laminated structure, the electrically insulating polymer compound being selected from the group consisting of (i) a fluorine-free polymer compound selected from the group consisting of polyethylene, polypropylene, polystyrene, polymethyl methacrylate, polyurea and polyimide, (ii) a compound having a molecular weight not less than 400 selected from the group consisting of polytetrafluoroethylene, polychlorotrifluoroethylene, polydicholorodifluoroethylene and a copolymer of chlorotrifluoroethylene and dichlorodifluoroethylene and (iii) a fluorine-containing copolymer having a main chain including a cyclic structure, wherein a deposition source of the electrically insulating polymer is heated to a temperature of not more than 600° C. and the protection layer is deposited at a rate of not more than 50 nm/second, wherein said layers beginning from a layer directly disposed on a lower electrode of said positive and negative electrodes and continuing to said protection layer are disposed without breaking a vacuum environment in a vacuum chamber and where the pressure in the vacuum chamber is maintained at not more than 1×10 -2 Pa prior to each of said layers being disposed.
Claim 3
Dependent Claim 16 words
The process according to claim 1, wherein the pressure is not more than 6×10 -3 Pa.
Claim 4
Dependent Claim 17 words
The process according to claim 2, wherein the rate of deposition is not more than 3 nm/second.
Claim 5
Dependent Claim 17 words
The process according to claim 1, wherein the rate of deposition is not more than 3 nm/second.
Claim 6
Dependent Claim 19 words
The process according to claim 1, wherein the protection layer has a thickness of 1 nm to 10 nm.

References Cited (Backward Citations)

US4720432A Cited
US5188901A Cited
US5094185A Cited
US5124204A Cited
US4853594A Cited
US5107175A Cited
US5093210A Cited
US5047687A Cited
US5246782A Cited
US5061769A Cited
US5178955A Cited
US5139879A Cited
US5403614A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1999-04-09 1999-10-09 2000-04-09 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2003-04-09 2003-10-09 2004-04-09 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2007-04-09 2007-10-09 2008-04-09 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag