← Back to Patent Explorer
US5492777A Expired / Lapsed US ⏱️ 0.0 years remaining

Electrochemical energy conversion and storage system

Assignee: Siemens AG
•
Filing: 1995-01-25
•
Granted: 1996-02-20
•
Expires: 2015-01-25
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An apparatus and method for storing electrical energy as chemical energy and recovering electrical energy from stored chemical energy. A solid oxide electrolyte electrochemical cell is operated in two modes. The first, energy storage, mode comprises steps of: (A) supplying electrical energy and steam to a solid oxide electrolyte electrochemical cell operating between 600° C. and 1200° C. as an electrolysis cell, to produce H 2 and O 2 ; (B) passing the H 2 gas so produced into an energy storage reactor containing iron oxide, to produce iron metal and steam; (C) recirculating the steam produced in the energy storage reactor to the cathode of the electrolysis cell; and (D) repeating steps (A) to (C) until the iron oxide is converted to iron metal, for chemical storage of electrical energy. The second, energy recovery, mode comprises steps of: (E) supplying steam to the energy storage reactor containing iron metal, to produce iron oxides and H 2 gas; (F) passing this H 2 gas to the fuel anode of an electrochemical cell operating as a fuel cell, and supplying O 2 gas to the air cathode of the electrochemical cell, to produce electrical energy and steam at the fuel anode; (G) recirculating the steam so produced to the energy storage reactor bed; (H) repeating steps (E) to (G) until the iron metal is converted to iron oxide and H 2 gas; and (I) recovering the electrical energy produced.

Inventors

  • 👤 Arnold O. Isenberg
  • 👤 Roswell J. Ruka

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-31 04:13
CPC Classifications
C; C01; C01B; C01B3/00; C01B3/02; C01B3/06; C01B3/061; C25; C25B; C25B1/00; C25B1/01; C25B1/02; C25B9/00; C25B9/01; C25B9/015; C25B9/17; H; H01; H01M; H01M8/00; H01M8/06; H01M8/0606; H01M8/0656; H01M8/18; H01M8/184; H01M8/186; H01M8/24; H01M8/241; H01M8/2425; H01M8/243; H01M8/10; H01M8/12; H01M2008/1293; H01M2300/00; H01M2300/0017; H01M2300/0065; H01M2300/0068; H01M2300/0071; H01M2300/0074; Y; Y02; Y02E; Y02E60/00; Y02E60/30; Y02E60/36; Y02E60/50; Y02P; Y02P20/00; Y02P20/10; Y02P20/129

Claims Analysis

Total Claims: 24
Claim 1
Independent Claim 378 words
A method of storing electrical energy as chemical energy and recovering electrical energy from the stored chemical energy by operating an electrochemical cell in two modes, an energy storage mode and an energy recovery mode, comprising: I. In the energy storage mode, (a) supplying external electrical energy to electrical leads and H 2 O (steam) gas to a cathode of at least one electrochemical cell operating as an electrolysis cell using a solid oxide electrolyte between an anode and the cathode, said electrolysis cell operating at a temperature of between about 600° C. to 1200° C., to produce H 2 gas along the cathode and O 2 gas along the anode; (b) passing the H 2 gas produced along the cathode of the electrolysis cell into a energy storage reactor containing iron oxide operating at a temperature of between about 600° C. to 800° C., to produce iron metal in the energy storage reactor and H 2 O (steam); (c) recirculating the H 2 O (steam) produced in the energy storage reactor to the cathode of the electrolysis cell to be electrolyzed; and (d) repeating steps (a) to (c) until substantially complete conversion of iron oxide to iron metal, for chemical energy storage of electrical energy; II. In the energy recovery mode, (e) supplying H 2 O (steam) gas to said energy storage reactor containing iron metal operating at a temperature of between about 600° C. to 800° C., to produce iron oxide in the energy storage reactor and H 2 gas; (f) passing the H 2 gas to a fuel anode of said at least one electrochemical cell operating as a fuel cell and supplying O 2 gas or air to an air cathode of said at least one electrochemical cell operating at a temperature of between about 600° C. to 1200° C., to conduct electrical energy along the external leads and produce H 2 O (steam) along the fuel anode; (g) recirculating the H 2 O (steam) produced at the fuel anode of the fuel cell to said energy storage bed; (h) repeating steps (e) to (g) until substantially complete conversion of iron metal to iron oxide and H 2 gas for electrical energy recovery form chemical energy storage; and, (i) recovering said electrical energy produced.
Claim 2
Independent Claim 378 words
A method of storing electrical energy as chemical energy and recovering electrical energy from the stored chemical energy by operating an electrochemical cell in two modes, an energy storage mode and an energy recovery mode, comprising: I. In the energy storage mode, (a) supplying external electrical energy to electrical leads and H 2 O (steam) gas to a cathode of at least one electrochemical cell operating as an electrolysis cell using a solid oxide electrolyte between an anode and the cathode, said electrolysis cell operating at a temperature of between about 600° C. to 1200° C., to produce H 2 gas along the cathode and O 2 gas along the anode; (b) passing the H 2 gas produced along the cathode of the electrolysis cell into a energy storage reactor containing iron oxide operating at a temperature of between about 600° C. to 800° C., to produce iron metal in the energy storage reactor and H 2 O (steam); (c) recirculating the H 2 O (steam) produced in the energy storage reactor to the cathode of the electrolysis cell to be electrolyzed; and (d) repeating steps (a) to (c) until substantially complete conversion of iron oxide to iron metal, for chemical energy storage of electrical energy; II. In the energy recovery mode, (e) supplying H 2 O (steam) gas to said energy storage reactor containing iron metal operating at a temperature of between about 600° C. to 800° C., to produce iron oxide in the energy storage reactor and H 2 gas; (f) passing the H 2 gas to a fuel anode of said at least one electrochemical cell operating as a fuel cell and supplying O 2 gas or air to an air cathode of said at least one electrochemical cell operating at a temperature of between about 600° C. to 1200° C., to conduct electrical energy along the external leads and produce H 2 O (steam) along the fuel anode; (g) recirculating the H 2 O (steam) produced at the fuel anode of the fuel cell to said energy storage bed; (h) repeating steps (e) to (g) until substantially complete conversion of iron metal to iron oxide and H 2 gas for electrical energy recovery form chemical energy storage; and, (i) recovering said electrical energy produced.
Claim 3
Dependent Claim 24 words
The method of claim 1, wherein the thermal energy is supplied from external sources and the electrical energy is supplied from a power plant.
Claim 4
Dependent Claim 45 words
The method of claim 1, wherein said electrolysis cell anode and said fuel cathode are comprised of lanthanum manganite, said solid oxide electrolyte is comprised of yttria or scandia stabilized zirconia, and the electrolysis cell cathode and fuel cell anode are comprised of nickel-zirconia cermet.
Claim 5
Dependent Claim 20 words
The method of claim 1, wherein the O 2 gas produced in step (a) is recovered as a useful by-product.
Claim 6
Dependent Claim 119 words
An electrochemical energy storage device, comprising: at least one solid oxide electrolyte, electrolysis cell including an anode, a cathode and a solid oxide electrolyte between said anode and cathode of the cell, and electrical leads connected to an external circuit from said anode to said cathode, and operating at a temperature to effectively electrolyze incoming H 2 O (steam) to H 2 gas and O 2 gas; at least one energy storage reactor including iron oxide/iron metal materials in the iron oxide state connected to said at least one electrolysis cell operating at a temperature to effectively react with the produced H 2 gas during electrolysis to reduce iron oxide to charged iron metal and produce water vapor (steam).
Claim 7
Dependent Claim 119 words
An electrochemical energy storage device, comprising: at least one solid oxide electrolyte, electrolysis cell including an anode, a cathode and a solid oxide electrolyte between said anode and cathode of the cell, and electrical leads connected to an external circuit from said anode to said cathode, and operating at a temperature to effectively electrolyze incoming H 2 O (steam) to H 2 gas and O 2 gas; at least one energy storage reactor including iron oxide/iron metal materials in the iron oxide state connected to said at least one electrolysis cell operating at a temperature to effectively react with the produced H 2 gas during electrolysis to reduce iron oxide to charged iron metal and produce water vapor (steam).
Claim 8
Dependent Claim 35 words
The device of claim 5, further comprising: a recirculation channel from said energy storage reactor to said electrolysis cell to recirculate the water vapor (steam) produced during energy storage to said electrolysis cell for electrolysis.
Claim 9
Dependent Claim 41 words
The device of claim 5, wherein said electrolysis cell is tubular and said anode defines the inner walls of the tube, said cathode defines the outer walls of the tube, and said solid oxide electrolyte is between the anode and cathode.
Claim 10
Dependent Claim 37 words
The device of claim 5, wherein said anode of the electrolysis cell is comprised of lanthanum manganite, the solid oxide electrolyte is comprised of yttria or scandia stabilized zirconia, and the cathode is comprised of nickel-zirconia cermet.
Claim 11
Dependent Claim 20 words
The device of claim 5, wherein said electrolysis cell is operated at temperatures between about 600° C. and 1200° C.
Claim 12
Dependent Claim 21 words
The device of claim 5, wherein said energy storage reactor is operated at temperatures between about 600° C. and 800° C.
Claim 13
Dependent Claim 13 words
The device of claim 5, wherein said iron oxide/iron metal materials are pellets.
Claim 14
Dependent Claim 123 words
An electrochemical energy recovery device, comprising: at least one energy storage reactor including iron oxide/iron metal materials in the iron metal state operating at a temperature to effectively react with incoming H 2 O (steam) to effectively oxidize iron metal to iron oxide and produce H 2 gas; at least one solid oxide electrolyte, fuel cell connected to said energy storage reactor, said fuel cell including an anode, a cathode and a solid oxide electrolyte between said anode and cathode of the cell, and electrical leads connected to an external circuit from said anode to said cathode, and operating at a temperature to effectively convert the H 2 gas produced from said energy storage reactor to electrical energy and H 2 O (steam).
Claim 15
Dependent Claim 123 words
An electrochemical energy recovery device, comprising: at least one energy storage reactor including iron oxide/iron metal materials in the iron metal state operating at a temperature to effectively react with incoming H 2 O (steam) to effectively oxidize iron metal to iron oxide and produce H 2 gas; at least one solid oxide electrolyte, fuel cell connected to said energy storage reactor, said fuel cell including an anode, a cathode and a solid oxide electrolyte between said anode and cathode of the cell, and electrical leads connected to an external circuit from said anode to said cathode, and operating at a temperature to effectively convert the H 2 gas produced from said energy storage reactor to electrical energy and H 2 O (steam).
Claim 16
Dependent Claim 35 words
The device of claim 12, further comprising: a recirculation channel from said fuel cell to said energy storage reactor to recirculate the water vapor (steam) produced during fuel cell operation to said energy storage reactor.
Claim 17
Dependent Claim 41 words
The device of claim 12, wherein said fuel cell is tubular and said cathode defines the inner walls of the tube, said anode defines the outer walls of the tube, and said solid oxide electrolyte is between the anode and cathode.
Claim 18
Dependent Claim 37 words
The device of claim 12, wherein said cathode of the fuel cell is comprised of lanthanum manganite, the solid oxide electrolyte is comprised of yttria or scandia stabilized zirconia, and the anode is comprised of nickel-zirconia cermet.
Claim 19
Dependent Claim 20 words
The device of claim 12, wherein said fuel cell is operated at temperatures between about 600° C. and 1200° C.
Claim 20
Dependent Claim 21 words
The device of claim 12, wherein said energy storage reactor is operated at temperatures between about 600° C. and 800° C.
Claim 21
Dependent Claim 13 words
The device of claim 12, wherein said iron oxide/iron metal materials are pellets.
Claim 22
Dependent Claim 40 words
An energy conversion and storage system, comprising the energy storage device of claim 6 and the energy recovery device of claim 13, wherein the energy storage and energy recovery devices are one and the same and operated in reverse modes.
Claim 23
Dependent Claim 313 words
An electrochemical energy conversion and storage device operational in two modes, an energy recovery mode and an energy storage mode, comprising: an electrochemical cell chamber, the cell chamber containing at least one electrochemical cell bundle, the cell bundle containing a plurality of parallel, axially elongated, interconnected electrochemical cells, each cell including a porous exterior electrode, a porous interior electrode, and a gas-tight solid oxide electrolyte between the two electrodes; a combustion chamber connected to the cell chamber; at least one combustion exhaust channel connected from the combustion chamber to the atmosphere; at least one energy storage chamber connected to the cell chamber, the energy storage chamber containing either iron oxide in the energy storage mode of operation or iron metal in the energy recovery mode of operation; at least one recirculation gas channel connected from outside of the porous exterior electrode in the cell chamber to the energy storage chamber; a steam inlet connected to the outside of the porous exterior electrode in the cell chamber; an oxidant inlet connected to the inside of the porous interior electrode in the cell chamber; and, electrical leads connected from the cell bundles in the cell chamber to an external circuit, in which the device can be operated in an energy storage mode by supplying direct current electrical energy from the external circuit through the leads to the electrochemical cells and steam through the steam inlet to the porous exterior electrode and providing the energy storage chamber in the iron oxide state, and in which the device can be operated in an energy recovery mode by providing the energy storage chamber in the iron state and supplying steam through the steam inlet to the energy storage chamber and an oxidant through the oxygen inlet to the porous interior electrode and recovering direct current electrical energy from the electrochemical cells through the leads to the external circuit.
Claim 24
Dependent Claim 313 words
An electrochemical energy conversion and storage device operational in two modes, an energy recovery mode and an energy storage mode, comprising: an electrochemical cell chamber, the cell chamber containing at least one electrochemical cell bundle, the cell bundle containing a plurality of parallel, axially elongated, interconnected electrochemical cells, each cell including a porous exterior electrode, a porous interior electrode, and a gas-tight solid oxide electrolyte between the two electrodes; a combustion chamber connected to the cell chamber; at least one combustion exhaust channel connected from the combustion chamber to the atmosphere; at least one energy storage chamber connected to the cell chamber, the energy storage chamber containing either iron oxide in the energy storage mode of operation or iron metal in the energy recovery mode of operation; at least one recirculation gas channel connected from outside of the porous exterior electrode in the cell chamber to the energy storage chamber; a steam inlet connected to the outside of the porous exterior electrode in the cell chamber; an oxidant inlet connected to the inside of the porous interior electrode in the cell chamber; and, electrical leads connected from the cell bundles in the cell chamber to an external circuit, in which the device can be operated in an energy storage mode by supplying direct current electrical energy from the external circuit through the leads to the electrochemical cells and steam through the steam inlet to the porous exterior electrode and providing the energy storage chamber in the iron oxide state, and in which the device can be operated in an energy recovery mode by providing the energy storage chamber in the iron state and supplying steam through the steam inlet to the energy storage chamber and an oxidant through the oxygen inlet to the porous interior electrode and recovering direct current electrical energy from the electrochemical cells through the leads to the external circuit.

References Cited (Backward Citations)

USRE28792E Cited
US3939257A Cited
US3981745A Cited
US4395468A Cited
US4490444A Cited
US4412895A Cited
US4474862A Cited
US4745038A Cited
US4751152A Cited
US4839247A Cited
US4983471A Cited
US5143800A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1999-02-19 1999-08-21 2000-02-20 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2003-02-19 2003-08-21 2004-02-20 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2007-02-19 2007-08-21 2008-02-20 $7700.00 Window Closed / Lapsed