Abstract

Abstract The present invention broadly is addressed to the marking, labeling, or tagging of hot metal or hot coils at elevated temperature with human readable and/or machine readable (e.g., bar code) characters. To this end, the present invention broadly is directed to a label which can be secured to hot metal stock (e.g.., coil stock) which is at a temperature of up to about 1200° F. The label is formed from a sheet of metal having a face and a back. The sheet face is coated with a layer of paint that is resistant to temperature of the hot metal stock and receptive to being thermally transfer printed. The metal sheet label is of a thickness so that the paint layer can be thermally transfer printed using conventional markers designed for paper or films. Alternatively, this paint layer can be marked upon using conventional dot matrix (wire) printers with carbon ribbon. The layer of paint also bears one or more human or machine readable identification bar code characters which were applied by a thermal transfer or wire matrix printer. The sheet face also has unpainted zones of bare metal for spot welding of the label to the hot stock while hot. While hot or upon cooling of the hot metal stock and label, the human identification characters can be readily read by humans, and the machine readable identification characters can be readily machine read even after exterior storage of the labeled stock for extended periods of time. The paint composition which finds efficacy for use in manufacturing the label of the present invention preferably comprises a phenyl silicone resin, an aluminum stearate extender in an amount effective to provides gloss for the paint of less than about 35, and opacifying amount of titanium dioxide pigment, and a solvent in an amount for application of the paint composition.

Inventors

  • 👤 John A. Robertson
  • 👤 Ken R. Vaughn

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 19:39
CPC Classifications
G; G09; G09F; G09F3/00; G09F3/02; G09F3/0297; G09F2003/023; G09F2003/0232; Y; Y10; Y10T; Y10T428/00; Y10T428/12; Y10T428/12347; Y10T428/24; Y10T428/24802; Y10T428/24851; Y10T428/24868; Y10T428/24876; Y10T428/24917; Y10T428/24942; Y10T428/2495

Claims Analysis

Total Claims: 28
Claim 1
Independent Claim 140 words
Method for labeling hot metal stock which has a surface and is at a temperature of up to about 1,200° F., which comprises the steps of: (a) coating a portion of the sheet face of a metal label having a face and a back with a layer of a paint that is resistant to the temperature of the hot metal stock and receptive to being thermally transfer printed, the metal label being of a thickness so that the paint layer can be thermally transfer printed and having unpainted zones of bare metal; (b) thermally transfer printing on said paint one or more of human or machine readable identification characters; (c) placing the back surface of the printed label of step (b) on a surface of the hot metal stock; and (d) welding said unpainted zones to said hot metal stock.
Claim 2
Dependent Claim 140 words
Method for labeling hot metal stock which has a surface and is at a temperature of up to about 1,200° F., which comprises the steps of: (a) coating a portion of the sheet face of a metal label having a face and a back with a layer of a paint that is resistant to the temperature of the hot metal stock and receptive to being thermally transfer printed, the metal label being of a thickness so that the paint layer can be thermally transfer printed and having unpainted zones of bare metal; (b) thermally transfer printing on said paint one or more of human or machine readable identification characters; (c) placing the back surface of the printed label of step (b) on a surface of the hot metal stock; and (d) welding said unpainted zones to said hot metal stock.
Claim 3
Dependent Claim 19 words
Method of claim 1, wherein said label is provided at a thickness of between about 0.001 and 0.004 inches.
Claim 4
Dependent Claim 14 words
Method of claim 1, wherein said paint is provided to be white in color.
Claim 5
Dependent Claim 15 words
Method of claim 1, wherein said label is spot welded to said hot metal stock.
Claim 6
Dependent Claim 20 words
Method of claim 1, wherein said label is provided in a rectangular shape with opposing side edges being unpainted zones.
Claim 7
Dependent Claim 11 words
Method of claim 1, wherein said label is manufactured from steel.
Claim 8
Dependent Claim 62 words
Method of claim 1, wherein said paint coated on said sheet face comprises: (a) a phenyl silicone resin; (b) an aluminum stearate extender in an amount effective to provide a gloss for the paint of less than about 35; (c) an opacifying amount of titanium dioxide (TiO 2 ) pigment; and (d) solvent in an amount for application of the paint composition.
Claim 9
Dependent Claim 10 words
Method of claim 7, wherein said paint is spray applied.
Claim 10
Dependent Claim 10 words
Method of claim 7, wherein said paint is roller applied.
Claim 11
Dependent Claim 27 words
The method of claim 7, wherein the painted labels are supplied to thermal transfer printing from a roll, wherein the thermally transferred printed labels then are severed.
Claim 12
Dependent Claim 15 words
The method of claim 1, wherein said hot metal stock is hot metal coil stock.
Claim 13
Dependent Claim 25 words
The method of claim 7, wherein the painted labels are supplied to thermal transfer printing from a roll, wherein the thermally-printed labels then are severed.
Claim 14
Dependent Claim 9 words
Metal stock labelled by the method of claim 1.
Claim 15
Dependent Claim 142 words
Method for labeling hot metal stock which has a surface and is at a temperature of up to about 1,200° F., which comprises the steps of: (a) coating a portion of the sheet face of a metal label having a face and a back with a layer of a paint that is resistant to the temperature of the hot metal stock and receptive to being wire matrix ribbon printed, the metal label being of a thickness so that the paint layer can be thermally transfer printed and having unpainted zones of bare metal; (b) wire matrix ribbon printing on said paint one or more of human or machine readable identification characters; (c) placing the back surface of the printed label of step (b) on a surface of the hot metal stock; and (d) welding said unpainted zones to said hot metal stock.
Claim 16
Dependent Claim 142 words
Method for labeling hot metal stock which has a surface and is at a temperature of up to about 1,200° F., which comprises the steps of: (a) coating a portion of the sheet face of a metal label having a face and a back with a layer of a paint that is resistant to the temperature of the hot metal stock and receptive to being wire matrix ribbon printed, the metal label being of a thickness so that the paint layer can be thermally transfer printed and having unpainted zones of bare metal; (b) wire matrix ribbon printing on said paint one or more of human or machine readable identification characters; (c) placing the back surface of the printed label of step (b) on a surface of the hot metal stock; and (d) welding said unpainted zones to said hot metal stock.
Claim 17
Dependent Claim 20 words
The method of claim 14, wherein said label is provided at a thickness of between about 0.001 and 0.010 inches.
Claim 18
Dependent Claim 15 words
The method of claim 14, wherein said paint is provided to be white in color.
Claim 19
Dependent Claim 16 words
The method of claim 14, wherein said label is spot welded to said hot metal stock.
Claim 20
Dependent Claim 21 words
The method of claim 14, wherein said label is provided in a rectangular shape with opposing side edges being unpainted zones.
Claim 21
Dependent Claim 12 words
The method of claim 14, wherein said label is manufactured from steel.
Claim 22
Dependent Claim 63 words
The method of claim 14, wherein said paint coated on said sheet face comprises: (a) a phenyl silicone resin; (b) an aluminum stearate extender in an amount effective to provide a gloss for the paint of less than about 35; (c) an opacifying amount of titanium dioxide (TiO 2 ) pigment; and (d) solvent in an amount for application of the paint composition.
Claim 23
Dependent Claim 11 words
The method of claim 20, wherein said paint is spray applied.
Claim 24
Dependent Claim 11 words
The method of claim 20, wherein said paint is roller applied.
Claim 25
Dependent Claim 26 words
The method of claim 20, wherein the painted labels are supplied to wire matrix ribbon printing from a roll, wherein the printed labels then are severed.
Claim 26
Dependent Claim 26 words
The method of claim 14, wherein the painted labels are supplied to wire matrix ribbon printing from a roll, wherein the printed labels then are severed.
Claim 27
Dependent Claim 15 words
The method of claim 14, wherein said hot metal stock is hot metal coil stock.
Claim 28
Dependent Claim 9 words
Metal stock labelled by the method of claim 14.

References Cited (Backward Citations)

US4242789A Cited
US4353951A Cited
US4743890A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1999-01-15 1999-07-17 2000-01-16 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2003-01-15 2003-07-17 2004-01-16 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2007-01-15 2007-07-17 2008-01-16 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag