← Back to Patent Explorer
US4242789A Expired / Lapsed US ⏱️ 0.0 years remaining

Method for making an improved magnetic encoding device

Assignee: United States Department of Energy
•
Filing: 1979-03-16
•
Granted: 1981-01-06
•
Expires: 1999-03-16
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A magnetic encoding device and method for making the same are provided for use as magnetic storage mediums in identification control applications which give output signals from a reader that are of shorter duration and substantially greater magnitude than those of the prior art. Magnetic encoding elements are produced by uniformly bending wire or strip stock of a magnetic material longitudinally about a common radius to exceed the elastic limit of the material and subsequently mounting the material so that it is restrained in an unbent position on a substrate of nonmagnetic material. The elements are spot weld attached to a substrate to form a binary coded array of elements according to a desired binary code. The coded substrate may be enclosed in a plastic laminate structure. Such devices may be used for security badges, key cards, and the like and may have many other applications.

Inventors

  • 👤 Richard J. Fox

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 22:51
CPC Classifications
G; G06; G06K; G06K19/00; G06K19/02; G06K19/06; G06K19/08; G06K19/10; G06K19/12; Y; Y10; Y10T; Y10T29/00; Y10T29/49; Y10T29/49826; Y10T29/49863; Y10T29/49906

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 138 words
A method of making an improved magnetic encoding device having at least one element of magnetic material for use as a magnetic storage medium, comprising the steps of: bending said element uniformly along the length thereof by passing said element about a roller having a radius sufficient to bend said element along a common radius of curvature sufficient to exceed the yield point of said element; attaching the free end of said element passing about said roller to a non-magnetic substrate; advancing said roller over said substrate to extend said element in an unbent orientation a desired length thereover; and restraining the prebent element in an unbent orientation on said substrate by attaching said element to said substrate at said desired length position so that a uniform stress is produced in said element along said desired length thereof.
Claim 2
Independent Claim 138 words
A method of making an improved magnetic encoding device having at least one element of magnetic material for use as a magnetic storage medium, comprising the steps of: bending said element uniformly along the length thereof by passing said element about a roller having a radius sufficient to bend said element along a common radius of curvature sufficient to exceed the yield point of said element; attaching the free end of said element passing about said roller to a non-magnetic substrate; advancing said roller over said substrate to extend said element in an unbent orientation a desired length thereover; and restraining the prebent element in an unbent orientation on said substrate by attaching said element to said substrate at said desired length position so that a uniform stress is produced in said element along said desired length thereof.
Claim 3
Dependent Claim 20 words
The method as set forth in claim 1 wherein said elements comprise lengths of wire formed of a magnetic material.
Claim 4
Dependent Claim 28 words
The method as set forth in claim 1 wherein said elements comprise lengths of strips formed of a magnetic material having a length greater than the width thereof.
Claim 5
Dependent Claim 51 words
The method as set forth in claim 1 wherein said at least one element includes a plurality of elements and further comprising the steps of repeating the steps of claim 1 at selected parallel bit positions along said substrate to produce a desired binary coded array of elements on said substrate.
Claim 6
Dependent Claim 105 words
The method as set forth in claim 4 wherein said substrate is in the form of an elongated strip and said bit positions extend transversely of said substrate and wherein said elements for bit positions indicative of a first binary state extend from one edge of said strip to a point substantially greater than half the distance across said substrate, and said elements for bit positions indicative of a second binary state extend from the other edge of said substrate to a point substantially greater than half the distance across said substrate to form a partially interleaved binary coded array of elements on said substrate.
Claim 7
Dependent Claim 35 words
The method as set forth in claim 5 wherein said substrate is formed of an electrically conductive material and said elements are attached to said substrate by spot welding their respective ends to said substrate.
Claim 8
Dependent Claim 20 words
The method as set forth in claim 6 further including the step of enclosing said substrate in a laminated covering.
Claim 9
Dependent Claim 22 words
The method as set forth in claim 7 wherein said magnetic material is Vicalloy and said substrate is made of stainless steel.

References Cited (Backward Citations)

US3820090A Cited
US3892118A Cited
US3676644A Cited
US3818465A Cited
US3866193A Cited
US3774180A Cited
US3774179A Cited
US3783249A Cited
US3780313A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-01-06 1984-07-07 1985-01-06 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-01-06 1988-07-07 1989-01-06 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-01-06 1992-07-07 1993-01-06 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag