Process for making a mask ROM with self-aligned coding technology

Assignee: United Microelectronics Corp
•
Filing: 1994-08-09
•
Granted: 1995-12-05
•
Expires: 2014-08-09
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A self-aligned coding process for mask ROM is disclosed. First, a substrate having a plurality of bit-lines formed therein, a gate oxide layer formed on the bit-lines, and a plurality of word-lines formed on the gate oxide, which together construct an array of memory cells, is provided. Next, a barrier layer is formed on the word-lines. A silicon dioxide layer is formed on the gate oxide between the word-lines by using liquid phase deposition, wherein the thickness of the silicon dioxide layer is larger than that of the word-lines. Then, the barrier layer is removed. A mask layer is formed on the substrate exposing parts of the memory cells that will be programmed. Finally, impurities are implanted into the substrate not covered by the mask layer and the silicon dioxide layer to make the memory cells that will be programmed operating in a first state, and leave other non-programmed memory cells operating in a second state.

Inventors

  • 👤 Gary Hong
  • 👤 Chen-Chiu Hsue

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-28 23:06
CPC Classifications
H; H10; H10B; H10B20/00; H10B20/27; H10B20/30; H10B20/38; H10B20/383

Claims Analysis

Total Claims: 16
Claim 1
Independent Claim 158 words
A self-aligned coding process for mask ROM, comprising the steps of: providing a substrate having a plurality of bit-lines formed therein, a gate oxide layer formed on said bit-lines, and a plurality of word-lines formed on said gate oxide layer, which together define an array of memory cells; forming a barrier layer on said word-lines; forming a silicon dioxide layer on said gate oxide layer between said word-lines by using liquid phase deposition, wherein the thickness of said silicon dioxide layer is larger than that of said word-lines; removing said barrier layer so as to define trenches in said silicon dioxide layer; forming a mask layer on said substrate exposing parts of said memory cells that will be programmed; and implanting impurities into said substrate not covered by said mask layer and said silicon dioxide layer whereby said memory cells that are programmed operate in a first state and other non-programmed memory cells operate in a second state.
Claim 2
Dependent Claim 158 words
A self-aligned coding process for mask ROM, comprising the steps of: providing a substrate having a plurality of bit-lines formed therein, a gate oxide layer formed on said bit-lines, and a plurality of word-lines formed on said gate oxide layer, which together define an array of memory cells; forming a barrier layer on said word-lines; forming a silicon dioxide layer on said gate oxide layer between said word-lines by using liquid phase deposition, wherein the thickness of said silicon dioxide layer is larger than that of said word-lines; removing said barrier layer so as to define trenches in said silicon dioxide layer; forming a mask layer on said substrate exposing parts of said memory cells that will be programmed; and implanting impurities into said substrate not covered by said mask layer and said silicon dioxide layer whereby said memory cells that are programmed operate in a first state and other non-programmed memory cells operate in a second state.
Claim 3
Dependent Claim 15 words
The process as recited in claim 1, wherein said barrier layer is a photoresist layer.
Claim 4
Dependent Claim 22 words
The process as recited in claim 1, further comprising a step of forming sidewall spacers on the side walls of said trenches.
Claim 5
Dependent Claim 14 words
The process as recited in claim 3, wherein said sidewall spacers comprise silicon oxide.
Claim 6
Dependent Claim 14 words
The process as recited in claim 3, wherein said sidewall spacers comprise silicon nitride.
Claim 7
Dependent Claim 23 words
The process as recited in claim 1, wherein said first state is an OFF state, and said second state is an ON state.
Claim 8
Dependent Claim 178 words
A self-aligned coding process for mask ROM, comprising the steps of: providing a substrate having a plurality of bit-lines formed therein, a gate oxide layer formed on said bit-lines, and a plurality of word-lines formed on said gate oxide layer, which together define an array of memory cells; forming a barrier layer on said word-lines; forming a silicon dioxide layer on said gate oxide layer between said word-lines by using liquid phase deposition, wherein the thickness of said silicon dioxide layer is greater than that of said word-lines; removing said barrier layer so as to define trenches in said silicon dioxide layer; forming an insulating layer on the surface of said silicon dioxide layer and said word-lines; forming a mask layer on said insulating layer exposing parts of said memory cells that will be programmed; and implanting impurities through said insulating layer into said substrate not covered by said mask layer and said silicon dioxide layer whereby said memory cells that are programmed operate in a first state and other non-programmed memory cells operate in a second state.
Claim 9
Dependent Claim 178 words
A self-aligned coding process for mask ROM, comprising the steps of: providing a substrate having a plurality of bit-lines formed therein, a gate oxide layer formed on said bit-lines, and a plurality of word-lines formed on said gate oxide layer, which together define an array of memory cells; forming a barrier layer on said word-lines; forming a silicon dioxide layer on said gate oxide layer between said word-lines by using liquid phase deposition, wherein the thickness of said silicon dioxide layer is greater than that of said word-lines; removing said barrier layer so as to define trenches in said silicon dioxide layer; forming an insulating layer on the surface of said silicon dioxide layer and said word-lines; forming a mask layer on said insulating layer exposing parts of said memory cells that will be programmed; and implanting impurities through said insulating layer into said substrate not covered by said mask layer and said silicon dioxide layer whereby said memory cells that are programmed operate in a first state and other non-programmed memory cells operate in a second state.
Claim 10
Dependent Claim 15 words
The process as recited in claim 7, wherein said barrier layer is a photoresist layer.
Claim 11
Dependent Claim 21 words
The process as recited in claim 7, further comprising a step of forming sidewall spacers on side walls of said trenches.
Claim 12
Dependent Claim 14 words
The process as recited in claim 9, wherein said sidewall spacers comprise silicon oxide.
Claim 13
Dependent Claim 14 words
The process as recited in claim 9, wherein said sidewall spacers comprise silicon nitride.
Claim 14
Dependent Claim 23 words
The process as recited in claim 7, wherein said first state is an OFF state, and said second state is an ON state.
Claim 15
Dependent Claim 14 words
The process as recited in claim 7, wherein said insulating layer comprises borophosphosilicate glass.
Claim 16
Dependent Claim 14 words
The process as recited in claim 7, wherein said insulating layer comprises phosphosilicate glass.

References Cited (Backward Citations)

US5306657A Cited
US5318921A Cited
US5418175A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1998-12-04 1999-06-05 1999-12-05 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2002-12-04 2003-06-05 2003-12-05 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2006-12-04 2007-06-05 2007-12-05 $7700.00 Window Closed / Lapsed