Patent US5441670A successfully refreshed from Google Patents.
← Back to Patent Explorer
US5441670A Expired / Lapsed US ⏱️ 0.0 years remaining

Process for producing an electrically conductive mixed oxide of titanium and tantalum or niobium

Assignee: De Nora Permelec Ltd
•
Filing: 1993-09-15
•
Granted: 1995-08-15
•
Expires: 2013-09-15
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A process for producing an electrically conductive mixed oxide comprises sintering a power mixture comprising from 30 to 98% by weight of titanium oxide, in terms of the amount of titanium based on the total amount of all the metallic elements, from 1 to 10% by weight of at least one of titanium metal and titanium hydride, in terms of the amount of titanium based on the total amount of all the metallic elements, and from 1 to 60% by weight of at least one of tantalum oxide and niobium oxide, in terms of the amount of tantalum, niobium, or tantalum and niobium based on the total amount of all of the metallic elements. The process provides a sintered solid comprising titanium, at least one of tantalum and niobium, and a stoichiometrically deficient amount of oxygen. The content of titanium in the sintered solid is from 40 to 99% by weight and the content of tantalum, niobium, or tantalum and niobium in the sintered solid is from 1 to 60% by weight, respectively, based on the total amount of all of the metallic elements in the mixed oxide.

Inventors

  • 👤 Takayuki Shimamune
  • 👤 Yasuo Nakajima

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 02:59
CPC Classifications
H; H01; H01B; H01B1/00; H01B1/06; H01B1/08

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 191 words
A process for producing an electrically conductive mixed oxide which comprises sintering a powder mixture comprising from 30 and 98% by weight of titanium oxide, in terms of the amount of titanium based on the total amount of all the metallic elements, from 1 to 10% by weight of at least one of titanium metal and titanium hydride, in terms of the amount of titanium based on the total amount of all of the metallic elements, and from 1 to 60% by weight of at least one of tantalum oxide and niobium oxide, in terms of the amount of tantalum, niobium, or combination of tantalum and niobium based on the total amount of all the metallic elements, to thereby obtain a sintered solid comprising titanium, at least one of tantalum and niobium, and a stoichiometrically deficient amount of oxygen, the content of titanium in the sintered solid being from 40 to 99% by weight and the content of tantalum, niobium, or tantalum and niobium in the sintered solid being from 1 to 60% by weight, respectively, based on the total amount of all of the metallic elements in the mixed oxide.
Claim 2
Dependent Claim 191 words
A process for producing an electrically conductive mixed oxide which comprises sintering a powder mixture comprising from 30 and 98% by weight of titanium oxide, in terms of the amount of titanium based on the total amount of all the metallic elements, from 1 to 10% by weight of at least one of titanium metal and titanium hydride, in terms of the amount of titanium based on the total amount of all of the metallic elements, and from 1 to 60% by weight of at least one of tantalum oxide and niobium oxide, in terms of the amount of tantalum, niobium, or combination of tantalum and niobium based on the total amount of all the metallic elements, to thereby obtain a sintered solid comprising titanium, at least one of tantalum and niobium, and a stoichiometrically deficient amount of oxygen, the content of titanium in the sintered solid being from 40 to 99% by weight and the content of tantalum, niobium, or tantalum and niobium in the sintered solid being from 1 to 60% by weight, respectively, based on the total amount of all of the metallic elements in the mixed oxide.
Claim 3
Dependent Claim 19 words
The process of claim 1, wherein the powder mixture comprises from 5 to 9% by weight of titanium metal.
Claim 4
Dependent Claim 15 words
The process of claim 1, wherein the sintering temperature is from 700° to 1,500° C.
Claim 5
Dependent Claim 15 words
The process of claim 1, wherein the sintering temperature is from 1,000° to 1,300° C.

References Cited (Backward Citations)

US3033907A Cited
EP0052468A1 Cited
US5028568A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1998-08-14 1999-02-13 1999-08-15 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2002-08-14 2003-02-13 2003-08-15 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2006-08-14 2007-02-13 2007-08-15 $7700.00 Window Closed / Lapsed