Abstract A ferroelectric liquid crystal is injected into a liquid crystal cell including a pair of substrates each having at least an electrode thereon and disposed with a sealing agent therebetween so as to provide a prescribed gap therein. The liquid crystal is injected while (a) changing a pressure or a pressure and a temperature of an environment of the liquid crystal cell with time so that (i) in an initial stage of injection, the liquid crystal is injected at a suppressed speed, and (ii) in an intermediate stage of injection, the liquid crystal is injected at a controlled speed so that a front end of the liquid crystal injected within the cell progresses at a substantially constant speed, (b) in a final stage of injection, cooling the liquid crystal under a pressure so as to avoid occurrence of a local liquid crystal injection failure due to a difference in thermal expansion coefficient between the liquid crystal and the substrates, and (c) during the pressure-changing step with time, introducing an inert gas into the environment so as to increase the environmental pressure to a pressure exceeding a normal pressure (760 Torr).
A method of injecting a ferroelectric liquid crystal into a liquid crystal cell comprising a pair of substrates each having at least an electrode thereon and disposed with a sealing agent therebetween so as to provide a prescribed gap therebetween, the method comprising: (a) changing a pressure or a pressure and a temperature of an environment of the liquid crystal cell with time so that, in an initial stage of injection, the liquid crystal is injected at a suppressed speed, and in an intermediate stage of injection, the liquid crystal is injected at a controlled speed so that a front end of the liquid crystal injected within the cell progresses at a substantially constant speed, (b) in a final stage of injection, cooling the liquid crystal under a pressure so as to avoid occurrence of a local liquid crystal injection failure due to a difference in thermal expansion coefficient between the liquid crystal and the substrates, and (c) during the pressure-changing step with time, introducing an inert gas into the environment so as to increase the environmental pressure to a pressure exceeding 760 Torr.
Claim 2
Independent Claim
184 words
A method of injecting a ferroelectric liquid crystal into a liquid crystal cell comprising a pair of substrates each having at least an electrode thereon and disposed with a sealing agent therebetween so as to provide a prescribed gap therebetween, the method comprising: (a) changing a pressure or a pressure and a temperature of an environment of the liquid crystal cell with time so that, in an initial stage of injection, the liquid crystal is injected at a suppressed speed, and in an intermediate stage of injection, the liquid crystal is injected at a controlled speed so that a front end of the liquid crystal injected within the cell progresses at a substantially constant speed, (b) in a final stage of injection, cooling the liquid crystal under a pressure so as to avoid occurrence of a local liquid crystal injection failure due to a difference in thermal expansion coefficient between the liquid crystal and the substrates, and (c) during the pressure-changing step with time, introducing an inert gas into the environment so as to increase the environmental pressure to a pressure exceeding 760 Torr.
Claim 3
Dependent Claim
19 words
A method according to claim 1, wherein the pressure in the initial stage of injection is held substantially constant.
Claim 4
Dependent Claim
18 words
A method according to claim 1, wherein the pressure in the intermediate stage of injection is generally increased.
Claim 5
Dependent Claim
22 words
A method according to claim 3, wherein the pressure is held constant for a prescribed period during the intermediate stage of injection.
Claim 6
Dependent Claim
19 words
A method according to claim 1, wherein the pressure is held substantially constant in the final stage of injection.