Patent USRE22950E successfully refreshed from Google Patents.
Patent US5336274A successfully refreshed from Google Patents.
← Back to Patent Explorer
US5336274A Expired / Lapsed US ⏱️ 0.0 years remaining

Method for forming a cell separator for use in bipolar-stack energy storage devices

Assignee: University of California
•
Filing: 1993-07-08
•
Granted: 1994-08-09
•
Expires: 2013-07-08
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An improved multi-cell electrochemical energy storage device, such as a battery, fuel cell, or double layer capacitor using a cell separator which allows cells to be stacked and interconnected with low electrical resistance and high reliability while maximizing packaging efficiency. By adding repeating cells, higher voltages can be obtained. The cell separator is formed by applying an organic adhesive on opposing surfaces of adjacent carbon electrodes or surfaces of aerogel electrodes of a pair of adjacent cells prior to or after pyrolysis thereof to form carbon aerogel electrodes. The cell separator is electronically conductive, but ionically isolating, preventing an electrolytic conduction path between adjacent cells in the stack.

Inventors

  • 👤 Steven T. Mayer
  • 👤 John H. Feikert
  • 👤 James L. Kaschmitter
  • 👤 Richard W. Pekala

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 16:41
CPC Classifications
H; H01; H01M; H01M6/00; H01M6/42; H01M6/46; H01M6/48; H01G; H01G11/00; H01G11/10; H01G11/12; H01G11/22; H01G11/26; H01G11/28; H01G11/78; H01G11/82; H01M8/00; H01M8/02; H01M8/0202; H01M8/0204; H01M8/0213; H01G11/66; H01G11/72; H01G11/74; H01G11/76; Y; Y02; Y02E; Y02E60/00; Y02E60/13; Y02E60/30; Y02E60/50; Y10; Y10T; Y10T29/00; Y10T29/49; Y10T29/49002; Y10T29/49108; Y10T29/49114

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 62 words
A method for forming a cell separator between at least a pair of cells each having at least one carbon electrode, comprising the step of: depositing an adhesive material, having ionic isolation characteristics, on adjacent surface of at least one carbon electrode of each cell, and pressing the carbon electrodes together, thereby electrically interconnecting the adjacent electrodes while providing ionic isolation therebetween.
Claim 2
Independent Claim 62 words
A method for forming a cell separator between at least a pair of cells each having at least one carbon electrode, comprising the step of: depositing an adhesive material, having ionic isolation characteristics, on adjacent surface of at least one carbon electrode of each cell, and pressing the carbon electrodes together, thereby electrically interconnecting the adjacent electrodes while providing ionic isolation therebetween.
Claim 3
Dependent Claim 23 words
The method of claim 1, additionally including the step of carbonizing the adhesive material in an inert atmosphere at temperatures between 500°-3000° C.
Claim 4
Dependent Claim 30 words
The method of claim 1, wherein the step of depositing the adhesive material on the electrodes is carried by spraying, dipping, spreading by brush, or applying by squeegee or roller.
Claim 5
Dependent Claim 25 words
The method of claim 1, wherein the adhesive material is applied so as to have a thickness in the range of 2.5μ to 10 mils.
Claim 6
Dependent Claim 31 words
The method of claim 1, wherein said electrodes are formed from carbon foams, and wherein the adhesive material is deposited prior to or after pyrolyzing the electrodes to produce carbon foams.
Claim 7
Dependent Claim 61 words
The method of claim 1, additionally including the steps of forming the carbon electrodes from a carbon foam, comprising: forming a material composed of an aerogel, aerogel composite, xerogel, or hybrid aerogel-xerogel, and pyrolyzing the thus formed material for producing a carbon foam; and wherein the step of depositing the adhesive material is carried out prior to the step of pyrolyzing.
Claim 8
Dependent Claim 23 words
The method of claim 1, wherein the adhesive material is selected from the group of modified alkyd, furfural, furfuryl alcohol, and phenolic resins.
Claim 9
Dependent Claim 17 words
The method of claim 7, wherein the adhesive material is selected from GLYPTAL 1202 and FURCARB UP520.
Claim 10
Dependent Claim 21 words
The method of claim 1, additionally including the step of providing the adhesive material from material which is carbonizable and organic.

References Cited (Backward Citations)

JPS56117216A Cited
US4675258A Cited
US4806290A Cited
US4873218A Cited
US4997804A Cited
US5086085A Cited
US5260855A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1997-08-08 1998-02-07 1998-08-09 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2001-08-08 2002-02-07 2002-08-09 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2005-08-08 2006-02-07 2006-08-09 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag