Abstract

Abstract A thin-film bypass capacitor is fabricated by forming a plurality of through holes through the thickness of a nonconductive base substrate and filling the through holes with a conductive material to form ground vias and power vias. A sequence of back side metalization layers are applied to the back side surface of the base substrate. A sequence of bottom contact layers are applied to the front side surface of the base substrate. A bottom contact power terminal is formed and a bottom contact metalization layer is applied to the surface of the bottom contact layers. A portion of the metalization layer is removed and an insulating layer is formed on the surface of the bottom contact metalization layer. A ground metalization feedthrough and a power metalization feedthrough are formed at the surface of the insulating layer. A sequence of top contact layers are applied to the surface of the insulating layer and a front side ground terminal and front side power terminal are formed. A back side ground terminal and a back side power terminal are formed at the back side of the base substrate.

Inventors

  • 👤 Michael G. Peters
  • 👤 William T. Chou
  • 👤 Wen-chou V. Wang
  • 👤 Michael G. Lee
  • 👤 Solomon I. Beilin

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 04:17
CPC Classifications
H; H01; H01G; H01G4/00; H01G4/002; H01G4/228; H01G4/232; H01G4/30; H01G4/306; H05; H05K; H05K1/00; H05K1/16; H05K1/162; H05K1/02; H05K1/11; H05K1/111; H05K1/112; H05K2201/00; H05K2201/03; H05K2201/0302; H05K2201/0317; H05K2201/09; H05K2201/09209; H05K2201/0929; H05K2201/09309; H05K2203/00; H05K2203/03; H05K2203/0315; H10; H10W; H10W90/00; H10W90/701; H10W90/721; H10W90/722; H10W90/724; Y; Y10; Y10T; Y10T29/00; Y10T29/43; Y10T29/435; Y10T29/49; Y10T29/49002; Y10T29/49117; Y10T29/49124; Y10T29/49155; Y10T29/49165

Claims Analysis

Total Claims: 29
Claim 1
Independent Claim 200 words
A method for forming a thin-film capacitor comprising the steps of: forming a plurality of conductive vias through a nonconductive substrate; forming a power electrical terminal on a back side of the substrate in contact with one of the vias; forming a ground electrical terminal on a back side of the substrate in contact with one of the vias; depositing a bottom contact layer on the front side of the substrate in electrical contact with at least two vias; electrically isolating a portion of the bottom contact layer adjacent to one of the vias for forming a front side power terminal in electrical contact with the back side power electrical terminal by way of one of the vias; forming a dielectric layer over a portion of the bottom contact layer which is not adjacent to the front side power terminal, leaving an opening through the dielectric layer adjacent to one of the vias for forming a front side ground terminal in electrical contact with the back side ground electrical terminal by way of one of the vias; and depositing a top contact layer over at least a portion of the dielectric layer and across the opening for forming a capacitor.
Claim 2
Independent Claim 200 words
A method for forming a thin-film capacitor comprising the steps of: forming a plurality of conductive vias through a nonconductive substrate; forming a power electrical terminal on a back side of the substrate in contact with one of the vias; forming a ground electrical terminal on a back side of the substrate in contact with one of the vias; depositing a bottom contact layer on the front side of the substrate in electrical contact with at least two vias; electrically isolating a portion of the bottom contact layer adjacent to one of the vias for forming a front side power terminal in electrical contact with the back side power electrical terminal by way of one of the vias; forming a dielectric layer over a portion of the bottom contact layer which is not adjacent to the front side power terminal, leaving an opening through the dielectric layer adjacent to one of the vias for forming a front side ground terminal in electrical contact with the back side ground electrical terminal by way of one of the vias; and depositing a top contact layer over at least a portion of the dielectric layer and across the opening for forming a capacitor.
Claim 3
Dependent Claim 54 words
The method as recited in claim 1 comprising forming the power terminal and ground terminal on the back side of the substrate by depositing a back side metalization layer onto the back side surface of the substrate and removing selected portions of the metalization layer that are not adjacent to one of the vias.
Claim 4
Dependent Claim 42 words
The method as recited in claim 2 comprising forming a front side power terminal by removing selected portions of the bottom contact layer that are not adjacent to one of the vias in electrical contact with the back side power electrical terminal.
Claim 5
Dependent Claim 42 words
The method as recited in claim 3 comprising forming a front side ground terminal comprising removing selected portions of the top contact layer that are not adjacent to one of the vias in electrical contact with the back side ground electrical terminal.
Claim 6
Dependent Claim 25 words
The method as recited in claim 4 comprising forming the dielectric layer by oxidizing a selected portion of the surface of the bottom contact layer.
Claim 7
Dependent Claim 29 words
The method as recited in claim 4 comprising forming the dielectric layer by depositing a dielectric material onto a selected portion of the surface of the bottom contact layer.
Claim 8
Independent Claim 178 words
A method for fabricating a thin-film capacitor comprising the steps of: forming a plurality of through holes through an electrically nonconductive substrate between a front side substrate surface and a back side substrate surface opposite the front side surface; filling the plurality of through holes with an electrically conductive material; depositing a back side metalization layer onto the back side surface of the nonconductive substrate; depositing a bottom contact layer onto the front side surface of the nonconductive substrate; electrically isolating a bottom contact power terminal in the bottom contact layer; forming an insulating layer on selected portions of the surface of the bottom contact layer, including selected portions of the bottom contact power terminal; depositing a top contact layer onto the surface of the insulating layer; forming a front side ground terminal and a front side power terminal in the top contact layer; and forming a back side ground terminal and a back side power terminal in the back side metalization layer in electrical contact with the front side ground terminal and front side power terminal, respectively.
Claim 9
Independent Claim 178 words
A method for fabricating a thin-film capacitor comprising the steps of: forming a plurality of through holes through an electrically nonconductive substrate between a front side substrate surface and a back side substrate surface opposite the front side surface; filling the plurality of through holes with an electrically conductive material; depositing a back side metalization layer onto the back side surface of the nonconductive substrate; depositing a bottom contact layer onto the front side surface of the nonconductive substrate; electrically isolating a bottom contact power terminal in the bottom contact layer; forming an insulating layer on selected portions of the surface of the bottom contact layer, including selected portions of the bottom contact power terminal; depositing a top contact layer onto the surface of the insulating layer; forming a front side ground terminal and a front side power terminal in the top contact layer; and forming a back side ground terminal and a back side power terminal in the back side metalization layer in electrical contact with the front side ground terminal and front side power terminal, respectively.
Claim 10
Dependent Claim 67 words
The method as recited in claim 7 wherein the step of depositing the back side metalization layer comprises the steps of: depositing a back side adhesion layer onto the back side surface of the nonconducting substrate; depositing a back side conductive layer onto the surface of the back side adhesion layer; and depositing a back side metal layer onto the surface of the back side conductive layer.
Claim 11
Dependent Claim 75 words
The method as recited in claim 8 wherein the step of depositing the bottom contact layer onto the front side surface of the nonconducting substrate comprises the steps of: depositing a bottom contact adhesion layer onto the front side surface of the nonconducting substrate; depositing a bottom contact conductive layer onto the surface of the bottom contact adhesion layer; and depositing a bottom contact metal layer onto the surface of the bottom contact conductive layer.
Claim 12
Dependent Claim 55 words
The method as recited in claim 7 comprising forming the bottom contact power terminal by selectively removing portions of the bottom contact layers that are not disposed adjacent to a power via for electrically isolating a portion of the bottom contact layer disposed adjacent to a power via for forming the bottom contact power terminal.
Claim 13
Dependent Claim 71 words
The method as recited in claim 10 wherein the step of depositing the top contact layer onto the surface of the insulating layer comprises the steps of: depositing a top contact adhesion layer onto the surface of the insulating layer; depositing a top contact conductive layer onto the surface of the top contact adhesion layer; and depositing a top contact metal layer onto the surface of the top contact conductive layer.
Claim 14
Dependent Claim 55 words
The method as recited in claim 11 comprising forming the front side ground terminal by selectively removing portions of the top contact layers that are not disposed adjacent to a ground via for electrically isolating a portion of the top contact layer disposed adjacent to a power via for forming the front side ground terminal.
Claim 15
Dependent Claim 43 words
The method as recited in claim 7 comprising forming the back side ground terminal and back side power terminal by selectively removing a portion of the back side metalization layers that are not positioned adjacent to the ground via and the power via.
Claim 16
Dependent Claim 25 words
The method as recited in claim 7 comprising forming the insulating layer by depositing a nonconductive material onto the surface of the bottom contact layer.
Claim 17
Dependent Claim 44 words
The method as recited in claim 14 wherein after the step of forming the insulating layer, a ground metalization feedthrough and a power metalization feed are formed by removing select portions of the insulating layer adjacent to the ground via and the power via.
Claim 18
Dependent Claim 42 words
The method as recited in claim 7 comprising forming the insulating layer by depositing a bottom contact metalization layer onto the surface of the bottom contact layer and then oxidizing the bottom contact metalization layer to create an electrically nonconductive oxide film.
Claim 19
Dependent Claim 62 words
The method as recited in claim 16 wherein prior to the step of oxidizing the bottom contact metalization layer, portions of the surface of the bottom contact metalization layer adjacent to the ground via and the power via are protected from becoming oxidized, the non-oxidized portions of the bottom contact metalization layer forming a ground metalization feedthrough and a power metalization feedthrough.
Claim 20
Independent Claim 283 words
A method for fabricating a thin-film bypass capacitor comprising the steps of: applying a sequence of back side metalization layers to a back side surface of an electrically nonconducting substrate, the substrate having a back side surface and a front side surface opposite to the back side surface, the substrate comprising a plurality of electrically conductive ground vias and power vias extending through the substrate; applying a sequence of bottom contact layers to the front side surface of the substrate; creating a bottom contact power terminal by removing select portions of the bottom contact layers to form bottom contact notches, the bottom contact notches electrically isolating a portion of the bottom contact layers adjacent to such a power via from the rest of the bottom contact layers for forming the bottom contact power terminal; applying a bottom contact metalization layer onto the surface of the bottom contact layers; forming an insulating layer at the surface of the bottom contact metalization layer; applying a sequence of top contact layers to the surface of the insulating layer; creating a front side ground terminal by removing select portions of the top contact layers to form ground terminal notches, the ground terminal notches electrically isolating a portion of the top contact layers adjacent to such a ground via from the rest of the top contact layers for forming the front side ground terminal; and creating a back side ground terminal and a back side power terminal by removing select portions of the back side metalization layers, the remaining portions of the back side metalization layers forming a back side ground terminal adjacent to the ground via, and a back side power terminal adjacent to the power via.
Claim 21
Independent Claim 283 words
A method for fabricating a thin-film bypass capacitor comprising the steps of: applying a sequence of back side metalization layers to a back side surface of an electrically nonconducting substrate, the substrate having a back side surface and a front side surface opposite to the back side surface, the substrate comprising a plurality of electrically conductive ground vias and power vias extending through the substrate; applying a sequence of bottom contact layers to the front side surface of the substrate; creating a bottom contact power terminal by removing select portions of the bottom contact layers to form bottom contact notches, the bottom contact notches electrically isolating a portion of the bottom contact layers adjacent to such a power via from the rest of the bottom contact layers for forming the bottom contact power terminal; applying a bottom contact metalization layer onto the surface of the bottom contact layers; forming an insulating layer at the surface of the bottom contact metalization layer; applying a sequence of top contact layers to the surface of the insulating layer; creating a front side ground terminal by removing select portions of the top contact layers to form ground terminal notches, the ground terminal notches electrically isolating a portion of the top contact layers adjacent to such a ground via from the rest of the top contact layers for forming the front side ground terminal; and creating a back side ground terminal and a back side power terminal by removing select portions of the back side metalization layers, the remaining portions of the back side metalization layers forming a back side ground terminal adjacent to the ground via, and a back side power terminal adjacent to the power via.
Claim 22
Dependent Claim 111 words
The method as recited in claim 18 wherein the step of applying a sequence of back side metalization layers comprises the steps of: applying a back side adhesion layer to the back side surface of the substrate, the back side adhesion layer being selected from the group of materials consisting of chromium and titanium; applying a back side conductive layer to the surface of the back side adhesion layer, the back side conductive layer being selected from the group of conductive materials consisting of metals and metal alloys; and applying a back side metal layer to the surface of the back side conductive layer, the back side metal layer being chromium.
Claim 23
Dependent Claim 110 words
The method as recited in claim 19 wherein the step of applying a sequence of bottom contact layers comprises the steps of: applying a bottom contact adhesion layer to the front side surface of the substrate, the bottom contact adhesion layer being selected from the group of materials consisting of chromium and titanium; applying a bottom contact conductive layer to the surface of the bottom contact adhesion layer, the bottom contact conductive layer being selected from the group of conductive materials consisting of metals and metal alloys; and applying a bottom contact metal layer to the surface of the bottom contact conductive layer, the bottom contact metal layer being chromium.
Claim 24
Dependent Claim 29 words
The method as recited in claim 20 comprising forming the bottom contact metalization layer by depositing a material selected from the group consisting of tantalum, titanium, niobium and hafnium.
Claim 25
Dependent Claim 26 words
The method as recited in claim 21 comprising removing a portion of the bottom contact metalization layer deposited onto the front side surface of the substrate.
Claim 26
Dependent Claim 27 words
The method as recited in claim 22 comprising protecting against oxidation selected portions of the bottom contact metalization layer adjacent to the ground via and power via.
Claim 27
Dependent Claim 29 words
The method as recited in claim 23 comprising forming the insulating layer by oxidizing the surface of the bottom contact metalization layer to form a electrically nonconductive oxide film.
Claim 28
Dependent Claim 39 words
The method as recited in claim 24 comprising removing the protected portions of the bottom contact metalization layer to form a ground metalization feedthrough, adjacent to the ground via, and a power metalization feedthrough, adjacent to the power via.
Claim 29
Dependent Claim 108 words
The method as recited in claim 25 wherein the step of applying a sequence of top contact layers comprises the steps of: applying a top contact adhesion layer to the surface of the insulating layer, the top contact adhesion layer being selected from the group consisting of tantalum, titanium, and molybdenum; applying a top contact conductive layer to the surface of the top contact adhesion layer, the top contact conductive layer being selected from the group of conductive materials consisting of metals and metal alloys; and applying a top contact metal layer to the surface of the top contact conductive layer, the top contact metal layer being chromium.

References Cited (Backward Citations)

US4285780A Cited
US4317700A Cited
US4830691A Cited
US4912020A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1997-06-27 1997-12-27 1998-06-28 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2001-06-27 2001-12-27 2002-06-28 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2005-06-27 2005-12-27 2006-06-28 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag