← Back to Patent Explorer
US5320899A Expired / Lapsed US ⏱️ 0.0 years remaining

Thermoplastic block copolymer films

Assignee: Kraton Polymers US LLC
•
Filing: 1993-10-12
•
Granted: 1994-06-14
•
Expires: 2013-10-12
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract The tensile properties of elastic polymer films which contain thermoplastic block copolymer compositions and ethylene/vinyl acetate copolymers are improved by replacing some of the ethylene/vinyl acetate with a polyolefin having low crystallinity. The increase in tensile strength occurs without significant loss of elasticity and is most significant when the polyolefin is an ultra-low density polyolefin.

Inventors

  • 👤 Lie K. Djiauw

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 06:10
CPC Classifications
C; C08; C08J; C08J5/00; C08J5/18; C08L; C08L33/00; C08L33/02; C08J2353/00; C08J2353/02

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 86 words
A blown polymer film, comprising a thickness between about 0.5 and 10 mils; about 40% to about 80% of a thermoplastic block copolymer composition containing predominantly a block copolymer of a monoalkenylarene and an unsaturated conjugated diene; about 5% to about 20% of an ethylene/vinyl acetate copolymer having a vinyl acetate content between 12% and 33%; 10 to 45 parts polystyrene per hundred parts of the block copolymer in the block copolymer composition; and 5% to 20% of a polyolefin having a crystallinity less than 60%.
Claim 2
Dependent Claim 86 words
A blown polymer film, comprising a thickness between about 0.5 and 10 mils; about 40% to about 80% of a thermoplastic block copolymer composition containing predominantly a block copolymer of a monoalkenylarene and an unsaturated conjugated diene; about 5% to about 20% of an ethylene/vinyl acetate copolymer having a vinyl acetate content between 12% and 33%; 10 to 45 parts polystyrene per hundred parts of the block copolymer in the block copolymer composition; and 5% to 20% of a polyolefin having a crystallinity less than 60%.
Claim 3
Dependent Claim 23 words
The polymer film of claim 1, wherein the thermoplastic block copolymer composition is a blend of a polystyrene-polybutadiene-polystyrene block copolymer and an oil.
Claim 4
Dependent Claim 16 words
The polymer film of claim 2, wherein the polyolefin has a crystallinity from 50% to 58%.
Claim 5
Dependent Claim 18 words
The polymer film of claim 3, wherein the vinyl acetate content of the ethylene/vinyl acetate polymer is 28%.
Claim 6
Dependent Claim 22 words
The polymer film of claim 1, wherein the film has a tensile strength of at least 2000 psi in the machine direction.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1997-06-13 1997-12-13 1998-06-14 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2001-06-13 2001-12-13 2002-06-14 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2005-06-13 2005-12-13 2006-06-14 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag