Patent US5290603A successfully refreshed from Google Patents.
← Back to Patent Explorer
US5290603A Expired / Lapsed US ⏱️ 0.0 years remaining

Method for spraying polymeric compositions with reduced solvent emission and enhanced atomization

Assignee: Union Carbide Chemicals and Plastics Technology LLC
•
Filing: 1992-12-18
•
Granted: 1994-03-01
•
Expires: 2012-12-18
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Methods are presented by which polymeric compositions, such as coating compositions, can be sprayed with compressed fluids, such as carbon dioxide, nitrous oxide, or ethane, at higher solids levels and with finer atomization to give improved spray application quality with reduced emission of solvent.

Inventors

  • 👤 Kenneth A. Nielsen
  • 👤 David C. Busby
  • 👤 Marc D. Donohue
  • 👤 Charles W. Glancy

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-31 12:43
CPC Classifications
B; B05; B05D; B05D1/00; B05D1/02; B05D1/025; C; C09; C09D; C09D7/00; C09D7/20; B05D2401/00; B05D2401/90

Claims Analysis

Total Claims: 22
Claim 1
Independent Claim 215 words
A process for spraying a polymeric composition to form a spray of finely atomized liquid droplets, which comprises: (1) forming a liquid mixture at temperature T 0 in a closed system, said mixture comprising: (a) a nonvolatile materials fraction containing at least one polymeric compound and which is capable of being sprayed; and (b) a solvent fraction which is at least partially miscible wit the nonvolatile materials fraction and contains at least one compressed fluid in an amount which when added to (a) is sufficient: (i) to render the viscosity of said mixture to a point suitable for being sprayed; and (ii) to enable said liquid mixture to form a liquid compressed fluid phase at temperature T 0 ; wherein the compressed fluid is a gas at standard conditions of 0° C. and one atmosphere pressure (STP); and (2) spraying said liquid mixture by passing the mixture at temperature T 0 and spray pressure P 1 into an orifice through which said mixture flows to form a liquid spray, wherein spray pressure P 1 is above the minimum pressure p 2 at which said liquid mixture forms a liquid compressed fluid phase at temperature T 0 , thereby passing the liquid mixture through the liquid-liquid region of the polymeric composition and compressed fluid during depressurization.
Claim 2
Dependent Claim 215 words
A process for spraying a polymeric composition to form a spray of finely atomized liquid droplets, which comprises: (1) forming a liquid mixture at temperature T 0 in a closed system, said mixture comprising: (a) a nonvolatile materials fraction containing at least one polymeric compound and which is capable of being sprayed; and (b) a solvent fraction which is at least partially miscible wit the nonvolatile materials fraction and contains at least one compressed fluid in an amount which when added to (a) is sufficient: (i) to render the viscosity of said mixture to a point suitable for being sprayed; and (ii) to enable said liquid mixture to form a liquid compressed fluid phase at temperature T 0 ; wherein the compressed fluid is a gas at standard conditions of 0° C. and one atmosphere pressure (STP); and (2) spraying said liquid mixture by passing the mixture at temperature T 0 and spray pressure P 1 into an orifice through which said mixture flows to form a liquid spray, wherein spray pressure P 1 is above the minimum pressure p 2 at which said liquid mixture forms a liquid compressed fluid phase at temperature T 0 , thereby passing the liquid mixture through the liquid-liquid region of the polymeric composition and compressed fluid during depressurization.
Claim 3
Dependent Claim 36 words
The process of claim 1, wherein said spray pressure P 1 is above or just below the maximum pressure P 3 at which said mixture forms a liquid compressed fluid phase at temperature T 0 .
Claim 4
Dependent Claim 22 words
The process of claim 2, wherein said spray pressure P is less than about 600 psi above said pressure P 3 .
Claim 5
Dependent Claim 22 words
The process of claim 1, wherein the viscosity of the liquid mixture of (a) and (b) is less than about 200 centipoise.
Claim 6
Dependent Claim 19 words
The process of claim 1, wherein the solvent fraction contains at least one active solvent for the polymeric compound.
Claim 7
Dependent Claim 23 words
The process of claim 1, wherein the compressed fluid is a supercritical fluid at temperature T 0 and spray pressure P 1 .
Claim 8
Dependent Claim 19 words
The process of claim 1, wherein the compressed fluid is carbon dioxide, nitrous oxide, ethane, or a mixture thereof.
Claim 9
Dependent Claim 225 words
A process for the spray application of polymeric coating compositions to a substrate, which comprises: (1) forming a liquid mixture at temperature T 0 in a closed system, said mixture comprising: (a) a nonvolatile materials fraction containing at least one polymeric compound capable of forming a coating on a substrate; and (b) a solvent fraction which is at least partially miscible with the nonvolatile materials fraction and contains at least one compressed fluid in an amount which when added to (a) is sufficient: (i) to render the viscosity of said mixture to a point suitable for being sprayed; and (ii) to enable said liquid mixture to form a liquid compressed fluid phase at temperature T 0 ; wherein the compressed fluid is a gas at standard conditions of 0° C. and one atmosphere pressure (STP); and (2) spraying said liquid mixture onto a substrate to form a coating thereon by passing the mixture at temperature T 0 and spray pressure P 1 into an orifice through which said mixture flows to form a liquid spray, wherein spray pressure P 1 is above the minimum pressure P 2 at which said liquid mixture forms a liquid compressed fluid phase at temperature T 0 , thereby passing the liquid mixture through the liquid-liquid region of the liquid mixture of the polymeric composition and compressed fluid during depressurization.
Claim 10
Dependent Claim 225 words
A process for the spray application of polymeric coating compositions to a substrate, which comprises: (1) forming a liquid mixture at temperature T 0 in a closed system, said mixture comprising: (a) a nonvolatile materials fraction containing at least one polymeric compound capable of forming a coating on a substrate; and (b) a solvent fraction which is at least partially miscible with the nonvolatile materials fraction and contains at least one compressed fluid in an amount which when added to (a) is sufficient: (i) to render the viscosity of said mixture to a point suitable for being sprayed; and (ii) to enable said liquid mixture to form a liquid compressed fluid phase at temperature T 0 ; wherein the compressed fluid is a gas at standard conditions of 0° C. and one atmosphere pressure (STP); and (2) spraying said liquid mixture onto a substrate to form a coating thereon by passing the mixture at temperature T 0 and spray pressure P 1 into an orifice through which said mixture flows to form a liquid spray, wherein spray pressure P 1 is above the minimum pressure P 2 at which said liquid mixture forms a liquid compressed fluid phase at temperature T 0 , thereby passing the liquid mixture through the liquid-liquid region of the liquid mixture of the polymeric composition and compressed fluid during depressurization.
Claim 11
Dependent Claim 36 words
The process of claim 8, wherein said spray pressure P 1 is above or just below the maximum pressure P 3 at which said mixture forms a liquid compressed fluid phase at temperature T 0 .
Claim 12
Dependent Claim 23 words
The process of claim 9, wherein said spray pressure P 1 is less than about 600 psi above said pressure P 3 .
Claim 13
Dependent Claim 22 words
The process of claim 8, wherein the viscosity of the liquid mixture of (a) and (b) is less than about 200 centipoise.
Claim 14
Dependent Claim 19 words
The process of claim 8, wherein the solvent fraction contains at least one active solvent for the polymeric compound.
Claim 15
Dependent Claim 23 words
The process of claim 8, wherein the compressed fluid is a supercritical fluid at temperature T 0 and spray pressure P 1 .
Claim 16
Dependent Claim 19 words
The process of claim 8, wherein the compressed fluid is carbon dioxide, nitrous oxide, ethane, or a mixture thereof.
Claim 17
Dependent Claim 30 words
The process of claim 8, wherein the at least one polymeric compound is selected from the group consisting of thermoplastic polymers, thermosetting polymers, crosslinkable film forming systems, and mixtures thereof.
Claim 18
Dependent Claim 49 words
The process of claim 15, wherein the at least one polymeric compound is selected from the group consisting of enamels, varnished, lacquers, acrylic polymers, vinyl polymers, styrenic polymers, polyesters, alkyds, polyurethanes, two-package polyurethanes, epoxy systems, phenolic systems, cellulosic polymers, amino polymers, silicone polymers, polymers containing fluorine, and mixtures thereof.
Claim 19
Dependent Claim 13 words
The process of claim 8, wherein the spray is a feathered, decompressive spray.
Claim 20
Dependent Claim 19 words
The process of claim 8, wherein the liquid mixture or spray is electrically charged by a high electrical voltage.
Claim 21
Dependent Claim 34 words
The process of claim 1, wherein the polymeric coating composition has a solvent portion composition of: ______________________________________ Weight Percent of Total Solvent Portion RER ______________________________________ 30-100% <50 0-70% 50-100 0-40% 101-250 <10% >250 ______________________________________
Claim 22
Dependent Claim 34 words
The process of claim 19, wherein the polymeric coating composition has a solvent portion composition of: ______________________________________ Weight Percent of Total Solvent Portion RER ______________________________________ 40-100% <50 0-60% 50-100 0-30% 101-250 <5% >250 ______________________________________

References Cited (Backward Citations)

US4582731A Cited
US4734451A Cited
US4734227A Cited
US4923720A Cited
US5057342A Cited
US5009367A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1997-02-28 1997-08-30 1998-03-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2001-02-28 2001-08-30 2002-03-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2005-02-28 2005-08-30 2006-03-01 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag