← Back to Patent Explorer
US5284717A Expired / Lapsed US ⏱️ 0.0 years remaining

Method for producing raw materials for a reformer by cracking and desulfurizing petroleum fuels

Assignee: Showa Shell Sekiyu KK
•
Filing: 1993-02-25
•
Granted: 1994-02-08
•
Expires: 2013-02-25
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract The present invention provides a method for producing raw materials for a reformer by cracking and desulfurizing petroleum fuels, characterized by cracking and desulfurizing petroleum fuels in a desulfurizer in the fuel cell electricity generation process at a temperature of 300 degrees-600 degrees C., preferably 350 degrees-500 degrees C., a pressure of 1-10 kg/cm2, an H2/oil of 500-2000, preferably 800-1000, and an SV of 0.5-4 hr-1 using a zeolite catalyst such as Y-type zeolite or a metallosilicate catalyst such as one having an Si/Me atomic ratio of 40-3200 where Me is Al, Ni, Co, Mo, W, Fe, Cr or Ga.

Inventors

  • 👤 Osamu Yamase
  • 👤 Tadayuki Miura
  • 👤 Hajime Kubota

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 19:59
CPC Classifications
C; C01; C01B; C01B3/00; C01B3/02; C01B3/32; C01B3/34; C01B3/48; H; H01; H01M; H01M8/00; H01M8/06; H01M8/0606; H01M8/0612; H01M8/0662; C01B2203/00; C01B2203/02; C01B2203/0205; C01B2203/0227; C01B2203/0233; C01B2203/0283; C01B2203/0288; C01B2203/04; C01B2203/0405; C01B2203/06; C01B2203/066; C01B2203/08; C01B2203/0805; C01B2203/0811; C01B2203/0816; C01B2203/0822; C01B2203/0827; C01B2203/0866; C01B2203/10; C01B2203/1041; C01B2203/1047; C01B2203/1052; C01B2203/1064; C01B2203/1076; C01B2203/1082; C01B2203/12; C01B2203/1205; C01B2203/1211; C01B2203/1235; C01B2203/1241; C01B2203/1247; C01B2203/1258; C01B2203/1264; C01B2203/127; Y; Y02; Y02E; Y02E60/00; Y02E60/30; Y02E60/50; Y02P; Y02P20/00; Y02P20/10

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 111 words
A method for producing raw materials for a steam reformer in a fuel cell electricity generation process which comprises: providing in combination, a desulfurzier, an adsorber; a steam reformer, a converter or gas separation membrane, and a fuel cell, and desulfurizing and cracking petroleum fuel in the desulfurizer using a metallosilicate catalyst having a Si/Al atomic ratio of 40-3200 at a temperature of 300°-600° C., a pressure of 1-10 kg/cm 2 , H 2 /oil ratio of 500-2000, and an SV of 0.5-4 hr -1 . wherein in said steam reformer, said desulfurzied and cracked fuel reacts with steam and is converted to product-gas comprising hydrogen, carbon monoxide, and carbon dioxide.
Claim 2
Independent Claim 111 words
A method for producing raw materials for a steam reformer in a fuel cell electricity generation process which comprises: providing in combination, a desulfurzier, an adsorber; a steam reformer, a converter or gas separation membrane, and a fuel cell, and desulfurizing and cracking petroleum fuel in the desulfurizer using a metallosilicate catalyst having a Si/Al atomic ratio of 40-3200 at a temperature of 300°-600° C., a pressure of 1-10 kg/cm 2 , H 2 /oil ratio of 500-2000, and an SV of 0.5-4 hr -1 . wherein in said steam reformer, said desulfurzied and cracked fuel reacts with steam and is converted to product-gas comprising hydrogen, carbon monoxide, and carbon dioxide.
Claim 3
Dependent Claim 43 words
A method according to claim 1, wherein the catalyst in said desulfurizing step is a metallosilicate catalyst has in atomic ratio Si/Me of 40-3200 wherein Me is metal selected from a group consisting of Al, Ni, Co, Mo, W, Fe, Cr and Ga.
Claim 4
Dependent Claim 17 words
A method according to claim 1, wherein the petroleum fuel is kerosene, naphtha or liquified petroleum gas.
Claim 5
Dependent Claim 36 words
A method according to claim 1, wherein the composition range of the desulfurized and cracked fuel fed into the reformed is C 3 to C 20 hydrocarbon and has a specific gravity of 0.5 to 0.85.
Claim 6
Dependent Claim 24 words
A method according to claim 1, wherein said cracking and desulfurizing is conducted at 350°-500° C. and an H 2 /oil ratio of 800-1000.
Claim 7
Independent Claim 194 words
A method for producing raw materials from a steam reformer in a fuel cell electricity generation process which comprises: providing, in combination, a desulfurizer, an adsorber, a steam reformer, a converter or gas separation membrane, and a fuel cell, desulfurizing and cracking fuel comprising kerosene, naphtha or liquified petroleum gas in said desulfurizer in the presence of a metallosilicate catalyst having an atomic ratio Si/Me of 40-3200, wherein Me is a metal selected from the group consisting of Al, Ni, Co, Mo, W, Fe, Cr and Ga, at a temperature of 300°-600° C., a a pressure of 1-10 kg/cm 2 , a H 2 /oil ratio of 500-2000, and an SV of 0.5-4 hr -1 whereby the desulfurized product contains ≦ 1 ppm sulfur, introducing said desulfurized product into said reformer wherein said product comprises C 3 to C 20 hydrocarbon and has a specific gravity of 0.5 to 0.85, steam reforming said product in said steam reformer wherein said product reacts with steam and is converted to product-gas comprising hydrogen, carbon monoxide, and carbon dioxide, and reducing the carbon monoxide content of the product-gas from said steam reformer to ≦ 1 vol. %.
Claim 8
Independent Claim 194 words
A method for producing raw materials from a steam reformer in a fuel cell electricity generation process which comprises: providing, in combination, a desulfurizer, an adsorber, a steam reformer, a converter or gas separation membrane, and a fuel cell, desulfurizing and cracking fuel comprising kerosene, naphtha or liquified petroleum gas in said desulfurizer in the presence of a metallosilicate catalyst having an atomic ratio Si/Me of 40-3200, wherein Me is a metal selected from the group consisting of Al, Ni, Co, Mo, W, Fe, Cr and Ga, at a temperature of 300°-600° C., a a pressure of 1-10 kg/cm 2 , a H 2 /oil ratio of 500-2000, and an SV of 0.5-4 hr -1 whereby the desulfurized product contains ≦ 1 ppm sulfur, introducing said desulfurized product into said reformer wherein said product comprises C 3 to C 20 hydrocarbon and has a specific gravity of 0.5 to 0.85, steam reforming said product in said steam reformer wherein said product reacts with steam and is converted to product-gas comprising hydrogen, carbon monoxide, and carbon dioxide, and reducing the carbon monoxide content of the product-gas from said steam reformer to ≦ 1 vol. %.

References Cited (Backward Citations)

FR1503018A Cited
US3485746A Cited
FR1555766A Cited
US3644200A Cited
US4151119A Cited
US4437978A Cited
US4336130A Cited
US4439310A Cited
US4429053A Cited
US4522894A Cited
US4816353A Cited
US4946750A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1997-02-07 1997-08-09 1998-02-08 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2001-02-07 2001-08-09 2002-02-08 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2005-02-07 2005-08-09 2006-02-08 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags