Patent US5219499A successfully refreshed from Google Patents.
US5219499A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Method for manufacturing screw rotors
Assignee: Svenska Rotor Maskiner AB
•
Filing: 1989-04-04
•
Granted: 1993-06-15
•
Expires: 2009-04-04
Abstract
Abstract A method of manufacturing rotors having helical lands and intermediate grooves wherein a multi-layer rotor body (2) is moulded or otherwise formed on a shaft (1) to only a small degree of accuracy, whereafter an outer layer (3) of polymer-based material is moulded on the rotor body to a high degree of accuracy. For the purpose of eliminating shrinkage-induced distortion of the lands of the rotor body (2) subsequent to applying the outer layer, the rotor body is produced in a multiple of layers (21, 22), by casting or like moulding processes, with each of the body layers having a thickness which is greater than that of the high accuracy outer layer (3).
Inventors
- 👤 Karlis Timuska
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-09 04:31
CPC Classifications
B; B29; B29D; B29D99/00; B29D99/0025; B29C; B29C37/00; B29C37/005; B29C39/00; B29C39/02; B29C39/021; B29C39/025; F; F01; F01C; F01C1/00; F01C1/08; F01C1/082; F01C1/084; F01C1/12; F01C1/14; F01C1/16; F05; F05C; F05C2225/00; F05C2225/04; F05C2253/00; F05C2253/04
Claims Analysis
Total Claims: 13
Claim 1
Independent Claim
224 words
A method for manufacturing rotors for screw rotor machines, which rotors have helical lands extending along the length of the rotors, with intermediate grooves between said lands, comprising the steps of: forming a multi-layer rotor body (2) around a carrier shaft (1); said step of forming said multi-layer rotor body (2) comprising forming a plurality of body layers (21, 22) each of a solidifying material selected such that differences in coefficients of thermal expansion of each of the solidifying materials are minimized, which body layers all are formed with helical lands and intermediate grooves, at least one of said body layers being a material composite; and thereafter forming a thin-walled integral outer layer (3) of polymer-based material, formed with great measurement accuracy, on the formed multi-layer rotor body (2), for eliminating shrinkage-induced angular distortion that causes changes in the pitch of the lands of the plurality of body layers (21, 22) in the vicinity of the ends thereof caused by solidification of the material of said plurality of body layers (21, 22), said thin-walled integral outer layer (3) having a wall-thickness compensating for deviation of the pitch of the lands, after solidification of the plurality of body layers of the multi-layer rotor body (2), from an intended final form of the rotor, shrinkage of each layer being terminated prior to forming a subsequent layer.
Claim 2
Independent Claim
224 words
A method for manufacturing rotors for screw rotor machines, which rotors have helical lands extending along the length of the rotors, with intermediate grooves between said lands, comprising the steps of: forming a multi-layer rotor body (2) around a carrier shaft (1); said step of forming said multi-layer rotor body (2) comprising forming a plurality of body layers (21, 22) each of a solidifying material selected such that differences in coefficients of thermal expansion of each of the solidifying materials are minimized, which body layers all are formed with helical lands and intermediate grooves, at least one of said body layers being a material composite; and thereafter forming a thin-walled integral outer layer (3) of polymer-based material, formed with great measurement accuracy, on the formed multi-layer rotor body (2), for eliminating shrinkage-induced angular distortion that causes changes in the pitch of the lands of the plurality of body layers (21, 22) in the vicinity of the ends thereof caused by solidification of the material of said plurality of body layers (21, 22), said thin-walled integral outer layer (3) having a wall-thickness compensating for deviation of the pitch of the lands, after solidification of the plurality of body layers of the multi-layer rotor body (2), from an intended final form of the rotor, shrinkage of each layer being terminated prior to forming a subsequent layer.
Claim 3
Dependent Claim
22 words
The method of claim 1, wherein at least one of the body layers of the multi-layer rotor body is formed by sintering.
Claim 4
Dependent Claim
22 words
The method of claim 1, wherein at least one of the body layers of the multi-layer rotor body is formed by casting.
Claim 5
Dependent Claim
22 words
The method of claim 1, wherein at least one of the body layers of the multi-layer rotor body is formed by molding.
Claim 6
Independent Claim
54 words
The method of any one of claims 1, 2, 3 or 4, wherein at least one of the body layers of the multi-layer rotor body is formed from a porous material, the body layer of porous material having a density which increases in the directions towards two faces of the porous material body layer.
Claim 7
Dependent Claim
21 words
The method of claim 5, wherein the thickness of the body layers of the multi-layer rotor body decreases outwardly from within.
Claim 8
Dependent Claim
24 words
The method of claim 6, wherein the outer layer has a smaller thickness than any of the other layers of the multi-layer rotor body.
Claim 9
Independent Claim
28 words
The method of any one of claims 1, 2, 3 or 4 wherein the thickness of the body layers of the multi-layer rotor body decreases outwardly from within.
Claim 10
Dependent Claim
24 words
The method of claim 8, wherein the outer layer has a smaller thickness than any of the other layers of the multi-layer rotor body.
Claim 11
Independent Claim
31 words
The method of any one of claims 1, 2, 3 or 4, wherein the outer layer has a smaller thickness than any of the other layers of the multi-layer rotor body.
Claim 12
Dependent Claim
42 words
The method of claim 1, comprising forming two of said body layers of polymer-based material; the innermost body layer being thicker than the outermost body layer; said outer layer being applied after shrinkage of at least said outermost body layer is completed.
Claim 13
Dependent Claim
25 words
The method of claim 11, wherein said outer layer is made of polytetrafluoroethylene, and varies in thickness from about 1/100 mm to about 1-2 mm.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1996-06-14 | 1996-12-14 | 1997-06-15 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 2000-06-14 | 2000-12-14 | 2001-06-15 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2004-06-14 | 2004-12-14 | 2005-06-15 | $7700.00 | Window Closed / Lapsed |