Abstract

Abstract A method is described for providing a protective finish to a vinyl substrate by applying to the vinyl substrate a vinyl protectant composition. In one embodiment the composition is an abrasive free mixture of a film forming polysiloxane; a diluent; and a wax in the form of micronized particles having an average diameter of 3-12 microns. In another embodiment, the composition is a hydrocarbon solvent free mixture of a film forming polysiloxane; water; and an amorphous silica in the form of fumed silica particles having an average diameter of 7-30 nanometers.

Inventors

  • 👤 Suzanne M. Greenleaf
  • 👤 Martin E. Cifuentes

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 11:43
CPC Classifications
B; B05; B05D; B05D7/00; B05D7/02; C; C08; C08J; C08J7/00; C08J7/04; C08J7/0427; C08J7/043; C09; C09D; C09D183/00; C09D183/04; C08J2483/00

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 125 words
A method of providing a protective finish to a vinyl substrate comprising applying to the vinyl substrate a vinyl protectant composition which is an abrasive free mixture of 5-60 percent by weight of a film forming polysiloxane which is selected from the group consisting of a polydimethylsiloxane having a viscosity of 100 to 1000 centistokes and having a silanol functional phenyl based silicone resin having present in the resin CH 3 SiO 1 .5, (CH 3 ) 2 SiO, (CH 3 )(C 6 H 5 )SiO, and (C 6 H 5 ) 2 SiO siloxane units; 20-50 percent by weight of a diluent; and 1-20 percent by weight of a wax in the form of micronized particles having an average particle size of 3-12 microns.
Claim 2
Independent Claim 125 words
A method of providing a protective finish to a vinyl substrate comprising applying to the vinyl substrate a vinyl protectant composition which is an abrasive free mixture of 5-60 percent by weight of a film forming polysiloxane which is selected from the group consisting of a polydimethylsiloxane having a viscosity of 100 to 1000 centistokes and having a silanol functional phenyl based silicone resin having present in the resin CH 3 SiO 1 .5, (CH 3 ) 2 SiO, (CH 3 )(C 6 H 5 )SiO, and (C 6 H 5 ) 2 SiO siloxane units; 20-50 percent by weight of a diluent; and 1-20 percent by weight of a wax in the form of micronized particles having an average particle size of 3-12 microns.
Claim 3
Dependent Claim 24 words
A method according to claim 1 in which the diluent is selected from the group consisting of water, toluene, mineral spirits, ethanol and isopropanol.
Claim 4
Independent Claim 128 words
A method of providing a protective finish to a vinyl substrate comprising applying to the vinyl substrate a vinyl protectant composition which is a hydrocarbon solvent free mixture of 5-60 percent by weight of a film forming polysiloxane which is selected from the group consisting of a polydimethylsiloxane fluid having a viscosity of 100 to 1000 centistokes and having a silanol functional phenyl based silicone resin having present in the resin CH 3 SiO 1 .5, (CH 3 ) 2 SiO, (CH 3 )(C 6 H 5 )SiO, and (C 6 H 5 ) 2 SiO siloxane units; 20-50 percent by weight of water; and 0.25-5 percent by weight of an amorphous silica in the form of fumed silica particles having an average particle size of 7-30 nanometers.
Claim 5
Independent Claim 128 words
A method of providing a protective finish to a vinyl substrate comprising applying to the vinyl substrate a vinyl protectant composition which is a hydrocarbon solvent free mixture of 5-60 percent by weight of a film forming polysiloxane which is selected from the group consisting of a polydimethylsiloxane fluid having a viscosity of 100 to 1000 centistokes and having a silanol functional phenyl based silicone resin having present in the resin CH 3 SiO 1 .5, (CH 3 ) 2 SiO, (CH 3 )(C 6 H 5 )SiO, and (C 6 H 5 ) 2 SiO siloxane units; 20-50 percent by weight of water; and 0.25-5 percent by weight of an amorphous silica in the form of fumed silica particles having an average particle size of 7-30 nanometers.
Claim 6
Dependent Claim 25 words
A method according to claim 3 in which the film forming polysiloxane is present in the mixture in an amount of 10-35 percent by weight.
Claim 7
Independent Claim 68 words
A method of providing a protective finish to a vinyl substrate comprising applying to the vinyl substrate a vinyl protectant composition which is a hydrocarbon solvent free mixture of 5-60 percent by weight of a film forming polysiloxane; 20-50 percent by weight of water; and 0.25-2.5 percent by weight of an amorphous silica in the form of fumed silica particles having an average particle size of 7-30 nanometers.
Claim 8
Independent Claim 68 words
A method of providing a protective finish to a vinyl substrate comprising applying to the vinyl substrate a vinyl protectant composition which is a hydrocarbon solvent free mixture of 5-60 percent by weight of a film forming polysiloxane; 20-50 percent by weight of water; and 0.25-2.5 percent by weight of an amorphous silica in the form of fumed silica particles having an average particle size of 7-30 nanometers.

References Cited (Backward Citations)

US4261758A Cited
US4304897A Cited
US4404035A Cited
US4642265A Cited
US4477517A Cited
US4454288A Cited
US4732694A Cited
US4548854A Cited
US4828885A Cited
US4846887A Cited
US5104735A Cited
US5036131A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1996-06-07 1996-12-07 1997-06-08 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2000-06-07 2000-12-07 2001-06-08 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2004-06-07 2004-12-07 2005-06-08 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag