Abstract

Abstract Protective overcoat compositions and photographic elements containing same comprise: (a) a hydroxylated latex polymer; (b) a hydrolyzed metal lower alkoxide; and, (c) a fluoroalkyl polyether surface active agent. The overcoat is transparent and flexible and provides protection against scratches and abrasion.

Inventors

  • 👤 Raymond T. Jones

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 21:46
CPC Classifications
C; C09; C09D; C09D5/00; C09D5/02; C09D5/024; G; G03; G03C; G03C11/00; G03C11/08

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 41 words
An aqueous coating composition useful in forming cross-linked protective layers on photographic elements, such coating composition comprising: (a) a hydroxylated polymer formed from a water-insoluble, hydroxyl-containing monomer; (b) a hydrolyzed metal lower alkoxide; and (c) a fluoroalkyl polyether surface active agent.
Claim 2
Dependent Claim 41 words
An aqueous coating composition useful in forming cross-linked protective layers on photographic elements, such coating composition comprising: (a) a hydroxylated polymer formed from a water-insoluble, hydroxyl-containing monomer; (b) a hydrolyzed metal lower alkoxide; and (c) a fluoroalkyl polyether surface active agent.
Claim 3
Dependent Claim 20 words
The aqueous coating composition of claim 1, wherein said polymer contains at least 40 mole percent of hydroxyl containing monomer.
Claim 4
Dependent Claim 16 words
The aqueous coating composition of claim 1, wherein said hydrolyzed metal lower alkoxide is polysilicic acid.
Claim 5
Dependent Claim 32 words
The aqueous coating composition of claim 1, wherein said hydrolyzed metal lower alkoxide comprises by weight proportion from about 2 parts to about 4 parts to one part of said hydroxylated polymer.
Claim 6
Dependent Claim 27 words
The aqueous coating composition of claim 1, wherein said hydrolyzed metal lower alkoxide comprises by weight proportion about 3 parts to one part of said hydroxylated polymer.
Claim 7
Dependent Claim 30 words
The aqueous coating composition of claim 1, wherein said fluoroalkyl polyether surface active agent comprises a mixture of compounds having the general formula ##STR2## wherein R is hydrogen or methyl.
Claim 8
Dependent Claim 33 words
The aqueous coating composition of claim 1, wherein said fluroalkyl polyether surface agent is present in an amount of from about 0.01 to about 0.1 percent by weight of said aqueous coating composition.
Claim 9
Dependent Claim 33 words
The aqueous coating composition of claim 1, wherein said fluroalkyl polyether surface agent is present in an amount of from about 0.04 to about 0.06 percent by weight of said aqueous coating composition.
Claim 10
Dependent Claim 11 words
The aqueous coating composition of claim 6, wherein R is hydrogen.

References Cited (Backward Citations)

US3429846A Cited
US4028300A Cited
US3971872A Cited
US4049868A Cited
US5037871A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1996-01-12 1996-07-13 1997-01-12 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2000-01-12 2000-07-13 2001-01-12 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2004-01-12 2004-07-13 2005-01-12 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag