← Back to Patent Explorer
US5175043A Expired / Lapsed US ⏱️ 0.0 years remaining

Aromatic polymer molded article with modified surface condition and process for producing the same

Assignee: DJK Research Center KK
•
Filing: 1988-12-10
•
Granted: 1992-12-29
•
Expires: 2008-12-10
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract PCT No. PCT/JP88/01252 Sec. 371 Date Jan. 7, 1991 Sec. 102(e) Date Jan. 7, 1991 PCT Filed Dec. 10, 1988 PCT Pub. No. WO89/05330 PCT Pub. Date Jun. 15, 1989.The present invention lies in a process for modifying the surface of a molded article, which process comprises irradiating the surface of a molded article composed of an aromatic polymer or a polymer composition containing said aromatic polymer, with an ultraviolet laser beam having a wavelength of about 150 nm-380 nm at a fluence at least lower than the threshold to modify the surface as compared with the condition before the irradiation. The process makes it possible to modify the condition of the laser beam-irradiated surface portions of the molded article to, for example, a white color or black color, whereby the molded article can be endowed with functions and properties required in its use in various applications.

Inventors

  • 👤 Akira Yabe
  • 👤 Hiroyuki Niino
  • 👤 Shozaburo Nagano
  • 👤 Masahiro Hosoi
  • 👤 Takatoshi Kuratsuji
  • 👤 Kazuaki Hotta
  • 👤 Masashi Nakano

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-06 03:56
CPC Classifications
B; B29; B29C; B29C59/00; B29C59/16; G; G11; G11B; G11B7/00; G11B7/24; G11B7/241; G11B7/242; G11B7/244; G11B7/245; G11B7/26; G11B7/263; B29C35/00; B29C35/02; B29C35/08; B29C35/0805; B29C2035/0827; B29C2035/0838; B29C2791/00; B29C2791/004; B29C2791/009; B29K; B29K2063/00; B29K2067/00; B29K2069/00; B29K2071/00; B29K2077/00; B29K2077/10; B29K2079/00; B29K2079/08; B29K2081/00; B29K2081/04; B29K2081/06; B29K2995/00; B29K2995/0018; B29K2995/002; B29K2995/0021; Y; Y10; Y10T; Y10T428/00; Y10T428/24; Y10T428/24479; Y10T428/24942

Claims Analysis

Total Claims: 32
Claim 1
Independent Claim 83 words
A process for producing a molded article having a modified surface condition as a result of the irradiation with an ultraviolet laser beam, which process is characterized by irradiating the surface of a molded article composed of an aromatic polymer or a polymer composition containing said aromatic polymer (a) with an ultraviolet laser beam having a wavelength of about 150 nm-380 nm, (b) at a density of at least 10 4 w/cm 2 , and (c) at a fluence lower than the threshold.
Claim 2
Dependent Claim 83 words
A process for producing a molded article having a modified surface condition as a result of the irradiation with an ultraviolet laser beam, which process is characterized by irradiating the surface of a molded article composed of an aromatic polymer or a polymer composition containing said aromatic polymer (a) with an ultraviolet laser beam having a wavelength of about 150 nm-380 nm, (b) at a density of at least 10 4 w/cm 2 , and (c) at a fluence lower than the threshold.
Claim 3
Dependent Claim 102 words
A process for producing a molded article having an at least partially discolored surface as a result of the irradiation with an ultraviolet laser beam, which process is characterized by irradiating the surface of a molded article composed of an aromatic polymer or a polymer composition containing said aromatic polymer (a) with an ultraviolet laser beam having a wavelength of about 150 nm-380 nm, (b) at a density of at least 10 4 w/cm 2 , (c') at a fluence which is 300% or less of the threshold, (d) so that the surface portions irradeated with the ultraviolet laser beam are discolored.
Claim 4
Dependent Claim 102 words
A process for producing a molded article having an at least partially discolored surface as a result of the irradiation with an ultraviolet laser beam, which process is characterized by irradiating the surface of a molded article composed of an aromatic polymer or a polymer composition containing said aromatic polymer (a) with an ultraviolet laser beam having a wavelength of about 150 nm-380 nm, (b) at a density of at least 10 4 w/cm 2 , (c') at a fluence which is 300% or less of the threshold, (d) so that the surface portions irradeated with the ultraviolet laser beam are discolored.
Claim 5
Dependent Claim 31 words
The process for producing a molded article, set forth in claim 1 or 2, wherein the polymer composition contains an aromatic polymer in an amount of 20% by weight or more.
Claim 6
Dependent Claim 65 words
The process for producing a molded article, set forth in claim 1 or 2, wherein the aromatic polymer is at least one member selected from the group consisting of an aromatic polyester, an aromatic polyether ether ketone, an aromatic polysulfone, an aromatic polysulfide, an aromatic polyethersulfone, a polyarylate, an aromatic polyimide, and aromatic polyamide, an aromatic polyetherimide, an aromatic polycarbonate and an aromatic epoxy resin.
Claim 7
Dependent Claim 23 words
The process for producing a molded article, set forth in claim 1 or 2, wherein the aromatic polymer is a substantially linear polymer.
Claim 8
Dependent Claim 29 words
The process for producing a molded article, set forth in claim 1 or 2, wherein the aromatic polymer has at least one aromatic hydrocarbon ring in the recurring unit.
Claim 9
Dependent Claim 31 words
The process for producing a molded article, set forth in claim 6, wherein the aromatic hydrocarbon ring is a benzene ring, a naphthalene ring, an anthracene ring or a diphenyl ring.
Claim 10
Dependent Claim 28 words
The process for producing a molded article, set forth in claim 6, wherein the aromatic hydrocarbon ring is a naphthalene ring, an anthracene ring or a diphenyl ring.
Claim 11
Dependent Claim 25 words
The process for producing a molded article, set forth in claim 1 or 2, wherein the aromatic polymer is an aromatic poly(ethersulfone) or a polyarylate.
Claim 12
Dependent Claim 49 words
The process for producing a molded article, set forth in claim 1 or 2, wherein a molded article composed of a composition containing an aromatic polymer of crystalline or semi-cryltalline form is subjected beforehand to the formation of latent crystal nuclei and then irradiated with an ultraviolet laser beam.
Claim 13
Dependent Claim 23 words
The process for producing a molded article, set forth in claim 1 or 2, wherein the aromatic polymer is an amorphous aromatic polymer.
Claim 14
Dependent Claim 46 words
The process for producing a molded article, set forth in claim 11, wherein the amorphous aromatic polymer is selected from the group consisting of a polyethylene terephthalate, a polyphenylene sulfide, an aromatic polyether ether ketone, an aromatic polyetherimide, an aromatic polysulfone and an aromatic epoxy resin.
Claim 15
Dependent Claim 28 words
The process for producing a molded article, set forth in claim 1 or 2, wherein the aromatic polymer is a mixture of an aromatic polycarbonate and a polystyrene.
Claim 16
Dependent Claim 28 words
The process for producing a molded article, set forth in claim 1 or 2, wherein the molded article is a film, a sheet, a plate or a board.
Claim 17
Dependent Claim 36 words
The process for producing a molded article, set forth in claim 1 or 2, wherein a light-transmitting plate is interposed between the surface of the molded article and a light source of the ultraviolet laser beam.
Claim 18
Dependent Claim 26 words
The process for producing a molded article, set forth in claim 15, wherein the light-transmitting plate has substantially no absorbability for the ultraviolet laser beam applied.
Claim 19
Dependent Claim 48 words
The process for producing a molded article, set forth in claim 15, wherein the light-transmitting plate is composed of one member selected from the group consisting of quartz, calcium fluoride, amgnesium fluoride, lithium fluoride, glass, a polyolefin, a polystyrene, a polymethyl methacrylate, a poly(4-methylpentene-1) and a cellulose acetate.
Claim 20
Dependent Claim 38 words
The process for producing a molded article, set forth in claim 15, wherein the light-transmitting plate is placed in tight contact with the molded article or at a distance of 1 mm or less from the molded article.
Claim 21
Dependent Claim 19 words
The process for producing a molded article, set forth in claim 15, wherein the light-transmitting plate is a photomask.
Claim 22
Dependent Claim 11 words
A molded article obtained by the production process of claim 1.
Claim 23
Dependent Claim 11 words
A molded article obtained by the production process of claim 2.
Claim 24
Independent Claim 75 words
A method of recording information comprising providing a molded article composed of an aromatic polymer or a polymer composition containing said aromatic polyer as a recording materials; irradiating a surface of said molded article (a) with an ultraviolet laser beam having a wavelength of about 150 nm-380 nm, (b) at a density of at least 10 4 w/cm 2 , and (c) at a fluence lower than the threshold to form a predetermined pattern thereon.
Claim 25
Independent Claim 75 words
A method of recording information comprising providing a molded article composed of an aromatic polymer or a polymer composition containing said aromatic polyer as a recording materials; irradiating a surface of said molded article (a) with an ultraviolet laser beam having a wavelength of about 150 nm-380 nm, (b) at a density of at least 10 4 w/cm 2 , and (c) at a fluence lower than the threshold to form a predetermined pattern thereon.
Claim 26
Independent Claim 93 words
A method of recording information comprising providing a molded article composed of an aromatic polymer or a polymer composition containing said aromatic polymer as a recording material; irradiating a surface of said molded article (a) with an ultraviolet laser beam having a wavelength of about 150 nm-380 nm, (b) at a density of at least 10 4 w/cm 2 , (c) at a fluence which is 300% or less of the threshold, and (d) so that the surface portions irradiated with the ultraviolet laser beam are discolored to form a predetermined pattern thereon.
Claim 27
Independent Claim 93 words
A method of recording information comprising providing a molded article composed of an aromatic polymer or a polymer composition containing said aromatic polymer as a recording material; irradiating a surface of said molded article (a) with an ultraviolet laser beam having a wavelength of about 150 nm-380 nm, (b) at a density of at least 10 4 w/cm 2 , (c) at a fluence which is 300% or less of the threshold, and (d) so that the surface portions irradiated with the ultraviolet laser beam are discolored to form a predetermined pattern thereon.
Claim 28
Dependent Claim 60 words
A process for producing a molded article with a modified or etched surface, which process is characterized by irradiating the surface of a molded article composed of a linear polymer composition constituted by a recurring unit containing at least one polycyclic condensed aromatic ring or diphenyl ring, with an ultraviolet light having a wavelength of about 150 nm-about 380 nm.
Claim 29
Dependent Claim 60 words
A process for producing a molded article with a modified or etched surface, which process is characterized by irradiating the surface of a molded article composed of a linear polymer composition constituted by a recurring unit containing at least one polycyclic condensed aromatic ring or diphenyl ring, with an ultraviolet light having a wavelength of about 150 nm-about 380 nm.
Claim 30
Dependent Claim 81 words
A process for producing a polyethylene terephthalate molded article having a modified or discolored surface condition as a result of the irradiation with an ultraviolet laser beam, which process is characterized by irradiating the surface of a molded article of an at least uniaxially drawn polyethylene terephthalate (a') with an ultraviolet laser beam having a wavelength of 220 nm-380 nm, (b) at a density of at least 10 4 w/cm 2 , and (c) at a fluence lower than the threshold.
Claim 31
Dependent Claim 81 words
A process for producing a polyethylene terephthalate molded article having a modified or discolored surface condition as a result of the irradiation with an ultraviolet laser beam, which process is characterized by irradiating the surface of a molded article of an at least uniaxially drawn polyethylene terephthalate (a') with an ultraviolet laser beam having a wavelength of 220 nm-380 nm, (b) at a density of at least 10 4 w/cm 2 , and (c) at a fluence lower than the threshold.
Claim 32
Dependent Claim 25 words
The process for producing a molded article, set forth in claim 1 or 2, wherein the aromatic polymer is an aromatic polycarbonate or a polystyrene.

References Cited (Backward Citations)

US4417948A Cited
US4568632A Cited
US4414059A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1995-12-29 1996-06-29 1996-12-29 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1999-12-29 2000-06-29 2000-12-29 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2003-12-29 2004-06-29 2004-12-29 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag