US5156985A Expired / Lapsed US ⏱️ 0.0 years remaining

Method for making a charge transfer semiconductor device having an oblong trench

Assignee: Panasonic Holdings Corp
•
Filing: 1991-05-08
•
Granted: 1992-10-20
•
Expires: 2011-05-08
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract In making trench type semiconductor CCD by using oblique ion-injections into an oblong trench groove in a semiconductor substrate region for injecting impurity atoms, an injection angle alpha for injecting a first conductivity type impurity to form isolation region into the side walls and also for injecting a second conductivity type impurity to form a charge transfer region thereon is selected less than pi /4, and another injection angle beta for injecting the same impurity into the end wall to form the end part of the isolation region and a third injection angle gamma for injecting the second conductivity type impurity thereon into the end wall to form the end part of the charge transfer region are selected: <IMAGE>

Inventors

  • 👤 Takahiro Yamada
  • 👤 Tadashi Sugaya

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 15:27
CPC Classifications
H; H10; H10D; H10D44/00; H10D44/01; H10D44/041; H10F; H10F39/00; H10F39/10; H10F39/12; H10F39/15; H10F39/153; H10P; H10P30/00; H10P30/20; H10P30/222

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 239 words
Method for making a semiconductor device comprising the steps of: etching a semiconductor substrate to form an oblong trench groove having an end wall; forming an electric isolation region comprising the steps of: obliquely ion-injecting impurity atoms of a first conductivity type at an injection angle α into a first side wall which is parallel to an oblong direction of said trench groove, said injection angle α being selected for injecting only into said first side wall; obliquely ion-injecting impurity atoms of said first conductivity type at said injection angle α into a second side wall which is parallel to said oblong direction but disposed opposite said first side wall; and obliquely ion-injecting impurity atoms of said first conductivity type at an injection angle β in the direction of said end wall and in the direction of a bottom face; forming a charge transfer region comprising the steps of: obliquely ion-injecting impurity atoms of a second conductivity type at an injection angle α into said first side wall; obliquely ion-injecting impurity atoms of said second conductivity type at said injection angle pat α into said second side wall; and obliquely ion-injecting impurity atoms of said second conductivity type at an injection angle γ into said end wall and also into said bottom face; forming insulation films on the wall faces of said trench groove; and forming plural charge transfer electrodes on the wall faces covered by said insulation films.
Claim 2
Dependent Claim 239 words
Method for making a semiconductor device comprising the steps of: etching a semiconductor substrate to form an oblong trench groove having an end wall; forming an electric isolation region comprising the steps of: obliquely ion-injecting impurity atoms of a first conductivity type at an injection angle α into a first side wall which is parallel to an oblong direction of said trench groove, said injection angle α being selected for injecting only into said first side wall; obliquely ion-injecting impurity atoms of said first conductivity type at said injection angle α into a second side wall which is parallel to said oblong direction but disposed opposite said first side wall; and obliquely ion-injecting impurity atoms of said first conductivity type at an injection angle β in the direction of said end wall and in the direction of a bottom face; forming a charge transfer region comprising the steps of: obliquely ion-injecting impurity atoms of a second conductivity type at an injection angle α into said first side wall; obliquely ion-injecting impurity atoms of said second conductivity type at said injection angle pat α into said second side wall; and obliquely ion-injecting impurity atoms of said second conductivity type at an injection angle γ into said end wall and also into said bottom face; forming insulation films on the wall faces of said trench groove; and forming plural charge transfer electrodes on the wall faces covered by said insulation films.
Claim 3
Independent Claim 114 words
A method for making a semiconductor device comprising the steps of: etching a semiconductor substrate to form an oblong trench groove having an end wall; obliquely ion-injecting impurity atoms of a first conductivity type, at an injection angle α of less than π/4, to the side walls of said oblong trench groove disposed in oblong direction; obliquely ion-injecting impurity atoms of said first conductivity type at an injection angle β to said end wall of said trench groove; and obliquely ion-injecting impurity atoms of a second conductivity type which is opposite to said first conductivity type at an injection angle γ to said end wall, said injection angles holding the relation: β+γ=π/2 and β≦γ.
Claim 4
Independent Claim 114 words
A method for making a semiconductor device comprising the steps of: etching a semiconductor substrate to form an oblong trench groove having an end wall; obliquely ion-injecting impurity atoms of a first conductivity type, at an injection angle α of less than π/4, to the side walls of said oblong trench groove disposed in oblong direction; obliquely ion-injecting impurity atoms of said first conductivity type at an injection angle β to said end wall of said trench groove; and obliquely ion-injecting impurity atoms of a second conductivity type which is opposite to said first conductivity type at an injection angle γ to said end wall, said injection angles holding the relation: β+γ=π/2 and β≦γ.
Claim 5
Independent Claim 459 words
A method for making a semiconductor device comprising the steps of: etching a semiconductor substrate to form an oblong trench groove having an end wall; forming an electric isolation region comprising the steps of: obliquely ion-injecting impurity atoms of a first conductivity type at an injection angle α with an impurity dose Npi(α) into a first side wall which is parallel to an oblong direction of said trench groove, said injection angle α being only in the direction of said first side wall; obliquely ion-injecting impurity atoms of said first conductivity type at said injection angle α with said impurity dose Npi(α) into a second side wall which is parallel to said oblong direction but disposed opposite said first side wall; obliquely ion-injecting impurity atoms of said first conductivity type at an injection angle β with an impurity dose Npi(β) into said end wall and also into the bottom face; and activating said impurity atoms of said first conductivity type injected into said first side wall and said second side wall thereby to produce impurity doses Npi(α,x) at the depth x from the surface of said side walls and also to produce impurity doses Npi(β,x) at the depth x from the surface of said end wall and said bottom face, wherein impurity doses Npi(α,x)·sin α of said side walls, impurity dose Npi(β,x)·sin β of said end wall and impurity dose Npi(β,x)·cos β of said bottom face are defined by the following relation: Npi(β,x)·sin β≦Npi(β,x)·cos β≦Npi(α,x)·sin α; forming a charge transfer region comprising the steps: obliquely ion-injecting impurity atoms of a second conductivity type which is opposite to said first conductivity type at said injection angle α with an impurity dose Nni(α) into said first side wall; obliquely ion-injecting impurity atoms of said second conductivity type at said injection angle α with said impurity does Nni(α) into said second side wall; obliquely ion-injecting impurity atoms of said second conductivity type at an injection angle γ with an impurity dose Nni(γ) into said end wall and also into said bottom face; and activating said impurity atoms of said second conductivity type injected into said first side wall and said second side wall thereby to produce impurity doses Nni(α,y) at depth y from a surface of said side walls and also to produce impurity doses Nni(γ,y) at depth y from a surface of said end wall and said bottom face, wherein impurity doses Nni(γ,y)·sin α of said side walls, impurity dose Nni(γ,y)·sin π of said end wall and impurity dose Nni(γ,y)·cos π of said bottom face are defined by the following relation: Nni(γ,y)·cos τ≦Nni(α,y)·sin α≦Nni(γ,y)·sin λ; forming insulation films on the wall faces of said trench groove; and forming plural charge transfer electrodes on the wall faces covered by said insulation films.
Claim 6
Independent Claim 459 words
A method for making a semiconductor device comprising the steps of: etching a semiconductor substrate to form an oblong trench groove having an end wall; forming an electric isolation region comprising the steps of: obliquely ion-injecting impurity atoms of a first conductivity type at an injection angle α with an impurity dose Npi(α) into a first side wall which is parallel to an oblong direction of said trench groove, said injection angle α being only in the direction of said first side wall; obliquely ion-injecting impurity atoms of said first conductivity type at said injection angle α with said impurity dose Npi(α) into a second side wall which is parallel to said oblong direction but disposed opposite said first side wall; obliquely ion-injecting impurity atoms of said first conductivity type at an injection angle β with an impurity dose Npi(β) into said end wall and also into the bottom face; and activating said impurity atoms of said first conductivity type injected into said first side wall and said second side wall thereby to produce impurity doses Npi(α,x) at the depth x from the surface of said side walls and also to produce impurity doses Npi(β,x) at the depth x from the surface of said end wall and said bottom face, wherein impurity doses Npi(α,x)·sin α of said side walls, impurity dose Npi(β,x)·sin β of said end wall and impurity dose Npi(β,x)·cos β of said bottom face are defined by the following relation: Npi(β,x)·sin β≦Npi(β,x)·cos β≦Npi(α,x)·sin α; forming a charge transfer region comprising the steps: obliquely ion-injecting impurity atoms of a second conductivity type which is opposite to said first conductivity type at said injection angle α with an impurity dose Nni(α) into said first side wall; obliquely ion-injecting impurity atoms of said second conductivity type at said injection angle α with said impurity does Nni(α) into said second side wall; obliquely ion-injecting impurity atoms of said second conductivity type at an injection angle γ with an impurity dose Nni(γ) into said end wall and also into said bottom face; and activating said impurity atoms of said second conductivity type injected into said first side wall and said second side wall thereby to produce impurity doses Nni(α,y) at depth y from a surface of said side walls and also to produce impurity doses Nni(γ,y) at depth y from a surface of said end wall and said bottom face, wherein impurity doses Nni(γ,y)·sin α of said side walls, impurity dose Nni(γ,y)·sin π of said end wall and impurity dose Nni(γ,y)·cos π of said bottom face are defined by the following relation: Nni(γ,y)·cos τ≦Nni(α,y)·sin α≦Nni(γ,y)·sin λ; forming insulation films on the wall faces of said trench groove; and forming plural charge transfer electrodes on the wall faces covered by said insulation films.

References Cited (Backward Citations)

US4374455A Cited
US4580331A Cited
JPS6312162A Cited
JPS63227036A Cited
JPH0278272A Cited
US5029321A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1995-10-20 1996-04-20 1996-10-20 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1999-10-20 2000-04-20 2000-10-20 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2003-10-20 2004-04-20 2004-10-20 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag