Abstract
Abstract A fluorine-containing elastomer capable of giving a primary vulcanization product with a good permanent set through peroxide vulcanization is produced by homopolymerization or copolymerization of a fluorine-containing olefin having 2 to 8 carbon atoms in the presence of an iodine and bromine-containing compound represented by the general formula RBrnIm, wherein R represents a fluorohydrocarbon group, a chlorofluorohydrocarbon group, a chlorohydrocarbon group or a hydrocarbon group, and n and m are integers of 1 and 2, and a small amount of perfluoro(unsaturated compound) which is iodotrifluoroethylene, perfluoro(bromoalkylvinylether) or perfluoro(iodoalkylvinylether).
Inventors
- 👤 Masatoshi Abe
- 👤 Haruyoshi Tatsu
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-02 06:40
CPC Classifications
C; C08; C08F; C08F214/00; C08F214/18; C08F214/184; C08F214/16
Claims Analysis
Total Claims: 6
Claim 1
Independent Claim
75 words
A process for producing a peroxide-vulcanizable, fluorine-containing elastomer, which comprises homopolymerizing or copolymerizing a fluorine-containing olefin having 2 to 8 carbon atoms in the presence of an iodine and bromine-containing compound represented by the general formula: RBrnIm wherein R is a fluorohydrocarbon group, a chlorofluorohydrocarbon group, a chlorohydrocarbon group or a hydrocarbon group, and n and m are integers of 1 and 2, and perfluoro-(unsaturated compound) selected from the group consisting of perfluoro(bromoalkylvinylether) and perfluoro(iodoalkylvinylether).
Claim 2
Dependent Claim
75 words
A process for producing a peroxide-vulcanizable, fluorine-containing elastomer, which comprises homopolymerizing or copolymerizing a fluorine-containing olefin having 2 to 8 carbon atoms in the presence of an iodine and bromine-containing compound represented by the general formula: RBrnIm wherein R is a fluorohydrocarbon group, a chlorofluorohydrocarbon group, a chlorohydrocarbon group or a hydrocarbon group, and n and m are integers of 1 and 2, and perfluoro-(unsaturated compound) selected from the group consisting of perfluoro(bromoalkylvinylether) and perfluoro(iodoalkylvinylether).
Claim 3
Dependent Claim
38 words
A process according to claim 1, wherein the iodine and bromine-containing compound is used in an amount of about 0.001% to about 5% by weight in terms of iodine and bromine to be combined in the fluorine-containing elastomer.
Claim 4
Dependent Claim
26 words
A process according to claim 1, wherein the perfluoro-(unsaturated compound) is used in a ratio about 0.001% to about 5% by mole to the fluorine-containing olefin.
Claim 5
Dependent Claim
32 words
A process according to claim 1, wherein the homopolymerizing or copolymerizing is carried out at a temperature of about -30° C. to about 150° C. in the presence of a polymerization initiator.
Claim 6
Dependent Claim
33 words
A process according to claim 1, wherein the homopolymerizing or copolymerizing is carried out at a temperature of about 0° C. to about 50° C. in the presence of a Redox polymerization initiator.
References Cited (Backward Citations)
US4745165A
Cited
EP0211251B1
Cited
US4774302A
Cited
US5041508A
Cited
US5037914A
Cited
US4973633A
Cited
US5032655A
Cited
US4948853A
Cited
US4973634A
Cited
US4948852A
Cited
US5077359A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1995-09-29 | 1996-03-30 | 1996-09-29 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1999-09-29 | 2000-03-30 | 2000-09-29 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2003-09-29 | 2004-03-30 | 2004-09-29 | $7700.00 | Window Closed / Lapsed |