Patent US5133957A successfully refreshed from Google Patents.
← Back to Patent Explorer
US5133957A Expired / Lapsed US ⏱️ 0.0 years remaining

Composition and method for desensitizing dentin

Assignee: Bisco Inc
•
Filing: 1991-09-18
•
Granted: 1992-07-28
•
Expires: 2011-09-18
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Hypersensitive dentin or cementum is treated by applying thereto two copolymerizable monomers which are polymerized in place and function to desensitize the hypersensitive areas. The first copolymerizable monomer used in the invention is the reaction product of N-phenylglycine or N- (p-tolyl)glycine and glycidyl methacrylate (NPG-GMA or NTG-GMA). The second copolymerizable monomer is selected from certain compounds produced by the reaction of an acid anhydride with excess hydroxyethyl methacrylate, e.g., biphenyl dimethacrylate. In a preferred embodiment, the mixture of monomers also contains a photosensitizer, such as camphoroquinone, which makes the mixture photocurable in addition to self-curable.

Inventors

  • 👤 Byoung I. Suh
  • 👤 Martin Hamer

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 05:25
CPC Classifications
A; A61; A61K; A61K6/00; A61K6/60; A61K6/62; A61K6/20; A61K6/40; Y; Y10; Y10S; Y10S522/00; Y10S522/908

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 219 words
A method of desensitizing hypersensitive dentin or cementum comprising applying to said dentin or cementum effective amounts of hydrophilic copolymerizable monomers A and B in solution in a water-displacing organic solvent, said monomers being applied simultaneously in a single solution or consecutively in separate solutions, and polymerizing said monomers to form an adhesive protective film thereon, monomer A being selected from the group consisting of the reaction products of N-phenyl glycine or N-(p-tolyl) glycine with glycidyl methacrylate, and alkali metal salts thereof, monomer B being selected from the group having the formulas ##STR11## wherein R is oxygen or --CH 2 ) n and n is 0, 1, or 2; ##STR12## wherein R 1 is N or --CH═ and m is 1 or 2; ##STR13## wherein X is ##STR14## R 2 and R 3 are the same or different, and are selected from hydrogen and C 1 -C 3 alkyl, and p is 0 or 1; ##STR15## wherein R 4 is --CH 2 ) n and n is 1 or 2; ##STR16## wherein one of Y 1 and Y 2 and one of Y 3 and Y 4 is hydrogen and the other is ##STR17## and ##STR18## wherein one of Y 1 and Y 2 and one of Y 3 and Y 4 is hydrogen and the other is ##STR19##
Claim 2
Independent Claim 219 words
A method of desensitizing hypersensitive dentin or cementum comprising applying to said dentin or cementum effective amounts of hydrophilic copolymerizable monomers A and B in solution in a water-displacing organic solvent, said monomers being applied simultaneously in a single solution or consecutively in separate solutions, and polymerizing said monomers to form an adhesive protective film thereon, monomer A being selected from the group consisting of the reaction products of N-phenyl glycine or N-(p-tolyl) glycine with glycidyl methacrylate, and alkali metal salts thereof, monomer B being selected from the group having the formulas ##STR11## wherein R is oxygen or --CH 2 ) n and n is 0, 1, or 2; ##STR12## wherein R 1 is N or --CH═ and m is 1 or 2; ##STR13## wherein X is ##STR14## R 2 and R 3 are the same or different, and are selected from hydrogen and C 1 -C 3 alkyl, and p is 0 or 1; ##STR15## wherein R 4 is --CH 2 ) n and n is 1 or 2; ##STR16## wherein one of Y 1 and Y 2 and one of Y 3 and Y 4 is hydrogen and the other is ##STR17## and ##STR18## wherein one of Y 1 and Y 2 and one of Y 3 and Y 4 is hydrogen and the other is ##STR19##
Claim 3
Dependent Claim 39 words
The method of claim 1 wherein said monomers are applied as a single solution containing 1-50% by weight of monomers A and B the weight ratio of monomer A to monomer B being within the range 1:1 to 1:50.
Claim 4
Dependent Claim 33 words
The method of claim 2 wherein said solution contains 10-30% by weight of monomers A and B, the weight ratio of monomer A to monomer B being within the range 1:5 to 1:20.
Claim 5
Dependent Claim 24 words
The method of claim 1 wherein said solvent is selected from organic solvents miscible with at least 25% by of water at ambient temperature.
Claim 6
Dependent Claim 18 words
The method of claim 3 wherein said solvent is selected from acetone and C 1 -C 4 alkanols.
Claim 7
Dependent Claim 27 words
The method of claim 1 wherein at least one of said solutions contains in addition an effective amount of a photosensitizer whereby said monomers are rendered photocurable.
Claim 8
Dependent Claim 10 words
The method of claim 6 wherein said photosensitizer is camphoroquinone.
Claim 9
Dependent Claim 29 words
The method of claim 1 wherein said hypersensitive dentin and cementum are pretreated with a conditioning agent comprising 1 to 50% phosphoric acid prior to application of said monomers.
Claim 10
Dependent Claim 16 words
The method of claim 8 wherein said conditioning agent comprises 5 to 15% of phosphoric acid.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1995-07-28 1996-01-27 1996-07-28 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1999-07-28 2000-01-27 2000-07-28 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2003-07-28 2004-01-27 2004-07-28 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag