Patent US2191361A successfully refreshed from Google Patents.
Patent US5132505A successfully refreshed from Google Patents.
← Back to Patent Explorer
US5132505A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of cleaving a brittle plate and device for carrying out the method

Assignee: US Philips Corp
•
Filing: 1991-03-04
•
Granted: 1992-07-21
•
Expires: 2011-03-04
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method and a device for cleaving a plate of a brittle material, such as, for example, glass, by means of a radiation beam repeatedly moving over the plate. The radiation beam is repeatedly passed over a desired track until the plate has been cleaved along a desired line of rupture of the plate.

Inventors

  • 👤 Maarten H. Zonneveld
  • 👤 Jacobus N. Dekker
  • 👤 Gerrit C. Verkade
  • 👤 Ireneus H. T. Fierkens
  • 👤 Theodorus J. M. J. van Gennip

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-06 14:02
CPC Classifications
G; G02; G02F; G02F1/00; G02F1/01; G02F1/13; G02F1/133; G02F1/1333; G02F1/133351; B; B23; B23K; B23K26/00; B23K26/08; B23K26/082; B23K26/0821; B23K26/36; B23K26/40; B28; B28D; B28D1/00; B28D1/22; B28D1/221; C; C03; C03B; C03B33/00; C03B33/09; C03B33/091; B23K2103/00; B23K2103/50

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 159 words
A method of cleaving a brittle plate in which a radiation beam originating from a source of radiation is passed over a desired track of the plate, which beam produces thermomechanical stresses in the plate and causes, starting from a crack initiation, a crack to be formed along a desired line of rupture, characterized in that the radiation beam is passed repeatedly over the track until the plate has been cleaved along the desired line of rupture, and characterized in that a first radiation beam is passed repeatedly over a first desired track of a first glass plate belonging to a number of liquid crystal display devices and a second radiation beam is passed repeatedly over a second desired track of a second glass plate belonging to the liquid crystal display devices until the plates have been cleaved along a first and a second desired line of rupture, respectively, which are located between two adjacent liquid crystal display devices.
Claim 2
Independent Claim 159 words
A method of cleaving a brittle plate in which a radiation beam originating from a source of radiation is passed over a desired track of the plate, which beam produces thermomechanical stresses in the plate and causes, starting from a crack initiation, a crack to be formed along a desired line of rupture, characterized in that the radiation beam is passed repeatedly over the track until the plate has been cleaved along the desired line of rupture, and characterized in that a first radiation beam is passed repeatedly over a first desired track of a first glass plate belonging to a number of liquid crystal display devices and a second radiation beam is passed repeatedly over a second desired track of a second glass plate belonging to the liquid crystal display devices until the plates have been cleaved along a first and a second desired line of rupture, respectively, which are located between two adjacent liquid crystal display devices.
Claim 3
Dependent Claim 33 words
A method as claimed in claim 1, characterized in that the first and second lines of rupture, viewed in a projection on one of the plates, are located at a certain relative distance.
Claim 4
Independent Claim 74 words
A method of cleaving a brittle plate comprising the steps of (a) locating an initial crack at an edge surface of a brittle plate, (b) producing thermomechanical stresses in said plate along a track starting from said initial crack by repeatedly passing a radiation beam over said track, and (c) continuing said step of repeatedly passing said radiation beam along said track until a crack is formed cleaving said plate along a rupture line.
Claim 5
Independent Claim 74 words
A method of cleaving a brittle plate comprising the steps of (a) locating an initial crack at an edge surface of a brittle plate, (b) producing thermomechanical stresses in said plate along a track starting from said initial crack by repeatedly passing a radiation beam over said track, and (c) continuing said step of repeatedly passing said radiation beam along said track until a crack is formed cleaving said plate along a rupture line.
Claim 6
Dependent Claim 69 words
A method according to claim 3, wherein said rupture line extends from one side of said plate to another side of said plate, wherein said step of repeated passing said radiation beam is carried out to only a given distance from said another side, and wherein cleaving of said plate along said rupture line is thereafter completed within the part of said plate kept free of said radiation beam.
Claim 7
Independent Claim 72 words
A device for cleaving a plate comprising (a) laser means for producing a laser beam, (b) focussing means for focussing said laser beam, (c) rotatable mirror means for repeatedly passing said laser beam over a track on a surface of a brittle plate until a crack is provided to cleave said plate along a rupture line, and (d) screening means for shielding a part of said rupture line from said laser beam.
Claim 8
Independent Claim 72 words
A device for cleaving a plate comprising (a) laser means for producing a laser beam, (b) focussing means for focussing said laser beam, (c) rotatable mirror means for repeatedly passing said laser beam over a track on a surface of a brittle plate until a crack is provided to cleave said plate along a rupture line, and (d) screening means for shielding a part of said rupture line from said laser beam.

References Cited (Backward Citations)

US3453097A Cited
US3543979A Cited
US4546231A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1995-07-21 1996-01-20 1996-07-21 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1999-07-21 2000-01-20 2000-07-21 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2003-07-21 2004-01-20 2004-07-21 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag