Patent US5089354A successfully refreshed from Google Patents.
← Back to Patent Explorer
US5089354A Expired / Lapsed US ⏱️ 0.0 years remaining

Wear-resistant, anti-seizing copper alloy composite materials

Assignee: Chuetsu Metal Works Co Ltd
•
Filing: 1990-12-11
•
Granted: 1992-02-18
•
Expires: 2010-12-11
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A copper alloy composite material which comprises a copper alloy matrix and at least one additive selected from solid materials having self-lubricity and wear-resistant materials and uniformly dispersed in the alloy matrix is described. The composite material has improved wear resistance and anti-seizing properties.

Inventors

  • 👤 Kunio Nakashima
  • 👤 Ryouichi Ishigane
  • 👤 Takayuki Tanaka
  • 👤 Ken-ichi Ichida

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 18:44
CPC Classifications
C; C22; C22C; C22C32/00; C22C32/0089; F; F16; F16C; F16C33/00; F16C33/02; F16C33/04; F16C33/06; F16C33/12; F16C33/121; Y; Y10; Y10T; Y10T428/00; Y10T428/12; Y10T428/12014; Y10T428/12028; Y10T428/12049; Y10T428/12056

Claims Analysis

Total Claims: 22
Claim 1
Independent Claim 87 words
A shaped, copper alloy material which has been prepared by hot working a mixture of powders encapsulated in a hermetically sealed metal jacket so as to apply compression and stretching actions on said mixture to effect uniform dispersion thereof, said mixture of powders consisting essentially of from about 0.1 to 10 wt% of additive material powder and the balance is copper alloy powder, said additive material powder being selected from the group consisting of solid materials having self-lubricating properties, solid materials having wear-resistant properties and mixtures thereof.
Claim 2
Dependent Claim 87 words
A shaped, copper alloy material which has been prepared by hot working a mixture of powders encapsulated in a hermetically sealed metal jacket so as to apply compression and stretching actions on said mixture to effect uniform dispersion thereof, said mixture of powders consisting essentially of from about 0.1 to 10 wt% of additive material powder and the balance is copper alloy powder, said additive material powder being selected from the group consisting of solid materials having self-lubricating properties, solid materials having wear-resistant properties and mixtures thereof.
Claim 3
Dependent Claim 21 words
A copper alloy composite material according to claim 1, wherein said additive material powder is a solid material having self-lubricating properties.
Claim 4
Dependent Claim 51 words
A copper alloy composite material according to claim 2, wherein the solid material having self-lubricating properties is a member selected from the group consisting of graphite, lead, MoS 2 , WS and mixtures thereof and is used in an amount of from 0.1 to 10 wt% based on the composite material.
Claim 5
Dependent Claim 33 words
A copper alloy composite material according to claim 2, wherein the solid material having self-lubricating properties is in the form of a powder having a particle size of from 0.1 to 500 micrometers.
Claim 6
Dependent Claim 36 words
A copper alloy composite material according to claim 1, wherein said additive material powder is a wear-resistant solid material and is contained in an amount of from 0.1 to 10 wt% based on the composite material.
Claim 7
Dependent Claim 34 words
A copper alloy composite material according to claim 5, wherein the wear-resistant solid material is a ceramic material in the form of a powder having a particle size of from 0.1 to 500 micrometers.
Claim 8
Dependent Claim 40 words
A copper alloy composite material according to claim 6, wherein the ceramic material is a member selected from the group consisting of SiC, BN, SiN, Al 2 O 3 , Cr 2 O 3 , SiO 2 and mixtures thereof.
Claim 9
Dependent Claim 47 words
A copper alloy composite material according to claim 1, wherein said additive material powder is a mixture of a solid material having self-lubricating properties and a wear-resistant solid material and is used in a total amount of from 0.1 to 10 wt% based on the composite material.
Claim 10
Dependent Claim 27 words
A copper alloy composite material according to claim 8, wherein the mixture is the form of powder each having a size of from 0.1 to 500 micrometers.
Claim 11
Dependent Claim 42 words
A copper alloy composite material according to claim 8, wherein the solid material having self-lubricating properties is a member selected from the group consisting of graphite, lead, MoS 2 , WS and mixtures thereof and the wear-resistant material is a ceramic material.
Claim 12
Dependent Claim 29 words
A copper alloy composite material as claimed in claim 1, wherein the encapsulated mixture of powders is hot worked and plastically molded into a desired shape by hot extrusion.
Claim 13
Dependent Claim 29 words
A copper alloy composite material as claimed in claim 1, wherein the encapsulated mixture of powders is hot worked and plastically molded into a desired shape by hot foregoing.
Claim 14
Dependent Claim 62 words
A copper alloy composite material encapsulated by a hermetically sealed metal jacket, said composite material consisting essentially of a mixture of from about 0.1 to 10 wt% of additive material powder and the balance is copper alloy powder, said additive material powder being selected from the group consisting of solid materials having self-lubricating properties, solid materials having wear-resistant properties and mixtures thereof.
Claim 15
Dependent Claim 62 words
A copper alloy composite material encapsulated by a hermetically sealed metal jacket, said composite material consisting essentially of a mixture of from about 0.1 to 10 wt% of additive material powder and the balance is copper alloy powder, said additive material powder being selected from the group consisting of solid materials having self-lubricating properties, solid materials having wear-resistant properties and mixtures thereof.
Claim 16
Dependent Claim 70 words
A copper alloy composite material which is a mixture of powders consisting essentially of from about 0.1 to 10 wt% of additive material powder having a particle size of from 0.1 to 500 micrometers and the balance is copper alloy powder, said additive material powder being selected from the group consisting of SiC, BN, SiN, Al 2 O 3 , Cr 2 O 3 , SiO 2 and mixtures thereof.
Claim 17
Dependent Claim 70 words
A copper alloy composite material which is a mixture of powders consisting essentially of from about 0.1 to 10 wt% of additive material powder having a particle size of from 0.1 to 500 micrometers and the balance is copper alloy powder, said additive material powder being selected from the group consisting of SiC, BN, SiN, Al 2 O 3 , Cr 2 O 3 , SiO 2 and mixtures thereof.
Claim 18
Independent Claim 98 words
A method of preparing a copper alloy composite material which comprises preparing a mixture of powders consisting essentially of from about 0.1 to 10 wt% of additive material powder and the balance is copper alloy powder, said additive material powder being selected from the group consisting of solid materials having self-lubricating properties, solid materials having wear-resistant properties and mixtures thereof, encapsulating said mixture of powders in a hermetically sealed metal jacket and then hot working said jacket containing said mixture of powders so as to apply compression and stretching actions on said mixture to effect uniform dispersion thereof.
Claim 19
Independent Claim 98 words
A method of preparing a copper alloy composite material which comprises preparing a mixture of powders consisting essentially of from about 0.1 to 10 wt% of additive material powder and the balance is copper alloy powder, said additive material powder being selected from the group consisting of solid materials having self-lubricating properties, solid materials having wear-resistant properties and mixtures thereof, encapsulating said mixture of powders in a hermetically sealed metal jacket and then hot working said jacket containing said mixture of powders so as to apply compression and stretching actions on said mixture to effect uniform dispersion thereof.
Claim 20
Dependent Claim 26 words
A method as claimed in claim 15 wherein the encapsulated mixture of powders is hot worked and plastically molded into a desired shape by hot extrusion.
Claim 21
Dependent Claim 26 words
A method as claimed in claim 15 wherein the encapsulated mixture of powders is hot worked and plastically molded into a desired shape by hot forgoing.
Claim 22
Dependent Claim 25 words
A method as claimed in claim 15 including the step of removing the metal jacket from the mixture of powder after said hot working step.

References Cited (Backward Citations)

US4935056A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1995-02-17 1995-08-19 1996-02-18 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1999-02-17 1999-08-19 2000-02-18 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2003-02-17 2003-08-19 2004-02-18 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag