Abstract

Abstract A quickly curable unsaturated polyester composition with high surface quality contains an unsaturated polyester, a vinyl monomer, either an alkane polyol polyacrylate or an alkane polyol polymethylacrylate, a thermoplastic resin, and one or more curing catalysts selected from t-butylperoxy benzoate, t-butylperoxy octoate and 2,5-dimethyl-2,5-di(benzoilperoxy) hexane. Molding compounds are obtained by impregnating glass fibers with such composition and molded products obtained by curing such molding material have improved surface smoothness.

Inventors

  • 👤 Takashi Shibata
  • 👤 Koichi Akiyama
  • 👤 Sanzi Aoki
  • 👤 Yasuhiro Mishima
  • 👤 Hisayuki Iwai
  • 👤 Ken Hatta

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 23:36
CPC Classifications
C; C08; C08L; C08L67/00; C08L67/06

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 118 words
A quickly curable unsaturated polyester composition with high surface quality, comprising an unsaturated polyester as a first component, a monovinyl monomer as a second component, a third component selected from the group consisting of alkane polyol polyacrylate and alkane polyol polymethacrylate, a thermoplastic resin that can function as a low profile additive as a fourth component, and at least one hardening catalyst selected from the group consisting of t-butylperoxy benzoate, t-butylperoxy octoate and 2,5-dimethyl-2,5-di(benzoilperoxy)hexane, said composition containing 20-40 weight parts of said first component, 40-60 weight parts of said second component, 1-15 weight parts of said third component, and 10-30 weight parts of said fourth component such that the total of said weight parts is 100 weight parts.
Claim 2
Dependent Claim 118 words
A quickly curable unsaturated polyester composition with high surface quality, comprising an unsaturated polyester as a first component, a monovinyl monomer as a second component, a third component selected from the group consisting of alkane polyol polyacrylate and alkane polyol polymethacrylate, a thermoplastic resin that can function as a low profile additive as a fourth component, and at least one hardening catalyst selected from the group consisting of t-butylperoxy benzoate, t-butylperoxy octoate and 2,5-dimethyl-2,5-di(benzoilperoxy)hexane, said composition containing 20-40 weight parts of said first component, 40-60 weight parts of said second component, 1-15 weight parts of said third component, and 10-30 weight parts of said fourth component such that the total of said weight parts is 100 weight parts.
Claim 3
Dependent Claim 135 words
A molding material comprising glass fibers and a quickly curable unsaturated polyester composition with high surface quality impregnating said glass fibers, said unsaturated polyester composition comprising an unsaturated polyester as a first component, a monovinyl monomer as a second component, a third component selected from the group consisting of alkane polyol polyacrylate and alkane polyol polymethacrylate, a thermoplastic resin that can function as a low profile additive as a fourth component, and at least one hardening catalyst selected from the group consisting of t-butylperoxy benzoate, t-butylperoxy octoate and 2,5-dimethyl-2,5-di(benzoilperoxy)hexane, said unsaturated polyester composition containing 20-40 weight parts of said first component, 40-60 weight parts of said second component, 1-15 weight parts of said third component, and 10-30 weight parts of said fourth component such that the total of said weight parts is 100 weight parts.
Claim 4
Dependent Claim 135 words
A molding material comprising glass fibers and a quickly curable unsaturated polyester composition with high surface quality impregnating said glass fibers, said unsaturated polyester composition comprising an unsaturated polyester as a first component, a monovinyl monomer as a second component, a third component selected from the group consisting of alkane polyol polyacrylate and alkane polyol polymethacrylate, a thermoplastic resin that can function as a low profile additive as a fourth component, and at least one hardening catalyst selected from the group consisting of t-butylperoxy benzoate, t-butylperoxy octoate and 2,5-dimethyl-2,5-di(benzoilperoxy)hexane, said unsaturated polyester composition containing 20-40 weight parts of said first component, 40-60 weight parts of said second component, 1-15 weight parts of said third component, and 10-30 weight parts of said fourth component such that the total of said weight parts is 100 weight parts.
Claim 5
Dependent Claim 142 words
A molded product obtained by hardening a molding material which comprises glass fibers and a quickly curable unsaturated polyester composition with high surface quality impregnating said glass fibers, said unsaturated polyester composition comprising an unsaturated polyester as a first component, a monovinyl monomer as a second component, a third component selected from the group consisting of alkane polyol polyacrylate and alkane polyol polymethacrylate, a thermoplastic resin that can function as a low profile additive as a fourth component, and at least one hardening catalyst selected from the group consisting of t-butylperoxy benzoate, t-butylperoxy octoate and 2,5-dimethyl-2,5-di(benzoilperoxy)hexane, said unsaturated polyester composition containing 20-40 weight parts of said first component, 40-60 weight parts of said second component, 1-15 weight parts of said third component, and 10-30 weight parts of said fourth component such that the total of said weight parts is 100 weight parts.
Claim 6
Dependent Claim 142 words
A molded product obtained by hardening a molding material which comprises glass fibers and a quickly curable unsaturated polyester composition with high surface quality impregnating said glass fibers, said unsaturated polyester composition comprising an unsaturated polyester as a first component, a monovinyl monomer as a second component, a third component selected from the group consisting of alkane polyol polyacrylate and alkane polyol polymethacrylate, a thermoplastic resin that can function as a low profile additive as a fourth component, and at least one hardening catalyst selected from the group consisting of t-butylperoxy benzoate, t-butylperoxy octoate and 2,5-dimethyl-2,5-di(benzoilperoxy)hexane, said unsaturated polyester composition containing 20-40 weight parts of said first component, 40-60 weight parts of said second component, 1-15 weight parts of said third component, and 10-30 weight parts of said fourth component such that the total of said weight parts is 100 weight parts.

References Cited (Backward Citations)

US4100229A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1994-12-30 1995-07-01 1995-12-31 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1998-12-30 1999-07-01 1999-12-31 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2002-12-30 2003-07-01 2003-12-31 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag