High temperature superconducting memory storage device and cryotron

Assignee: EIDP Inc
•
Filing: 1988-03-09
•
Granted: 1991-12-03
•
Expires: 2008-03-09
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Binary memory storage devices and cryotrons utilizing superconducting crystals exhibiting an onset of superconductivity and a relatively weak flux exclusion at a temperature T1 and the onset of relatively strong flux exclusion at T2, where T1>T2>77K, are controlled by dc magnetic fields. The preferred superconducting crystals have the formula Bi 2 Sr 3-z Ca z Cu 2 O 8+w wherein z is from about 0.1 to about 0.9 and w is greater than zero but less than about 1.

Inventors

  • 👤 Thomas R. Askew
  • 👤 Richard B. Flippen
  • 👤 Munirpallam A. Subramanian

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 13:41
CPC Classifications
H; H10; H10N; H10N60/00; H10N60/30; H10N60/35; G; G11; G11C; G11C11/00; G11C11/21; G11C11/44; H10N60/80; H10N60/85; H10N60/855; H10N60/857; Y; Y10; Y10S; Y10S505/00; Y10S505/70; Y10S505/701; Y10S505/775; Y10S505/776; Y10S505/782

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 96 words
A binary memory storage device comprising a crystal of a compound having the formula Bi.sub.2 Sr.sub.3-z Ca.sub.z Cu.sub.2 O.sub.8+w wherein z is from about 0.4 to about 0.8 and o<w<l, means for cooling said crystal to a temperature between about 77K and about 96K, means for applying and removing a dc magnetic field of about 10 Oe (800 A/m) to about 200 Oe to said crystal, means for applying an alternating magnetic field having a maximum strength of about 1 Oe to said crystal, and means for detecting the amount of flux excluded by said crystal.
Claim 2
Dependent Claim 96 words
A binary memory storage device comprising a crystal of a compound having the formula Bi.sub.2 Sr.sub.3-z Ca.sub.z Cu.sub.2 O.sub.8+w wherein z is from about 0.4 to about 0.8 and o<w<l, means for cooling said crystal to a temperature between about 77K and about 96K, means for applying and removing a dc magnetic field of about 10 Oe (800 A/m) to about 200 Oe to said crystal, means for applying an alternating magnetic field having a maximum strength of about 1 Oe to said crystal, and means for detecting the amount of flux excluded by said crystal.
Claim 3
Dependent Claim 19 words
The binary memory storage device of claim 1 wherein said dc magnetic field is about 30 Oe (2400 A/m).
Claim 4
Dependent Claim 76 words
A cryotron comprising a crystal of a compound having the formula Bi 2 Sr 3-z Ca z Cu 2 O 8+w wherein z is from about 0.4 to about 0.8 and o<w<l, means for passing an electrical current through said crystal, means for cooling said crystal to a temperature between about 77K and about 96K, and means for applying and removing a dc magnetic field of about 10 Oe to about 200 Oe to said crystal.
Claim 5
Dependent Claim 76 words
A cryotron comprising a crystal of a compound having the formula Bi 2 Sr 3-z Ca z Cu 2 O 8+w wherein z is from about 0.4 to about 0.8 and o<w<l, means for passing an electrical current through said crystal, means for cooling said crystal to a temperature between about 77K and about 96K, and means for applying and removing a dc magnetic field of about 10 Oe to about 200 Oe to said crystal.
Claim 6
Dependent Claim 14 words
The cryotron of claim 3 wherein said dc magnetic field is about 30 Oe.

References Cited (Backward Citations)

US4164030A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1994-12-02 1995-06-03 1995-12-03 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1998-12-02 1999-06-03 1999-12-03 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2002-12-02 2003-06-03 2003-12-03 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag