Abstract

Abstract A tough, wear resistant body is provided. The body includes hard carbide particles embedded in and bonded with a first casted ferrous matrix material such as steel or cast iron. The body may be embedded in and bonded with a second steel matrix to form a wear resistant composite. The second steel matrix has a melting point at least 200 degrees F. greater than the melting point of the first ferrous matrix, thereby facilitating a metallurgical bond between the surface of the wear resistant body and the second steel matrix. The composite structure is particularly suitable for earthmoving and other severe mechanical applications.

Inventors

  • 👤 James P. Materkowski

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-27 11:57
CPC Classifications
B; B22; B22D; B22D19/00; B22D19/14; E; E02; E02F; E02F9/00; E02F9/28; E02F9/2808; E02F9/285; Y; Y10; Y10T; Y10T428/00; Y10T428/12; Y10T428/12486; Y10T428/12493; Y10T428/12535; Y10T428/12576; Y10T428/12771; Y10T428/12861; Y10T428/12951; Y10T428/12958; Y10T428/12965; Y10T428/12972

Claims Analysis

Total Claims: 17
Claim 1
Independent Claim 86 words
A tough, wear resistant body comprising: (a) at least one layer of a carbide material selected from the group consisting of tungsten carbide, titanium carbide, tantalum carbide, niobium carbide, zirconium carbide, vanadium carbide, hafnium carbide, molybdenum carbide, chromium carbide, boron carbide, silicon carbide, their mixtures, solid solutions, and cemented composites; (b) a casted steel matrix material, wherein said carbide material is embedded in and bonded to said casted steel matrix; and (c) wherein said steel matrix has a carbon equivalent value of between 1.5 and 2.5.
Claim 2
Dependent Claim 86 words
A tough, wear resistant body comprising: (a) at least one layer of a carbide material selected from the group consisting of tungsten carbide, titanium carbide, tantalum carbide, niobium carbide, zirconium carbide, vanadium carbide, hafnium carbide, molybdenum carbide, chromium carbide, boron carbide, silicon carbide, their mixtures, solid solutions, and cemented composites; (b) a casted steel matrix material, wherein said carbide material is embedded in and bonded to said casted steel matrix; and (c) wherein said steel matrix has a carbon equivalent value of between 1.5 and 2.5.
Claim 3
Dependent Claim 21 words
The wear resistant body according to claim 1, wherein said carbide material has an average particle size greater than 4 mesh.
Claim 4
Dependent Claim 23 words
The wear resistant body according to claim 2, wherein said carbide material has an average particle size between 4 mesh and 3/8 inch.
Claim 5
Dependent Claim 27 words
The wear resistant body according to claim 2, wherein said carbide material is in the form of crushed parts, powder or pressed bodies having an irregular shape.
Claim 6
Dependent Claim 24 words
The wear resistant body according to claim 1, wherein said steel matrix has a hardness value of between 35 and 45 R c .
Claim 7
Dependent Claim 23 words
The wear resistant body according to claim 1, wherein said steel matrix has a melting point of between 2400 and 2600 degrees F.
Claim 8
Dependent Claim 17 words
The wear resistant body according to claim 1, wherein said steel matrix is more than 90% dense.
Claim 9
Dependent Claim 119 words
A tough, wear resistant composite body comprising: (a) at least one layer of a carbide material selected from the group consisting of tungsten carbide, titanium carbide, tantalum carbide, niobium carbide, zirconium carbide, vanadium carbide, hafnium carbide, molybdenum carbide, chromium carbide, boron carbide, silicon carbide, their mixtures, solid solutions, and cemented composites; (b) a first casted steel matrix material, wherein said carbide material is embedded in and bonded to said first casted steel matrix to form a wear resistant body; and (c) a second steel matrix, having a melting point at least 200 degrees F. greater than the melting point of said first steel matrix, wherein said wear resistant body is embedded in and bonded to said second steel matrix.
Claim 10
Dependent Claim 119 words
A tough, wear resistant composite body comprising: (a) at least one layer of a carbide material selected from the group consisting of tungsten carbide, titanium carbide, tantalum carbide, niobium carbide, zirconium carbide, vanadium carbide, hafnium carbide, molybdenum carbide, chromium carbide, boron carbide, silicon carbide, their mixtures, solid solutions, and cemented composites; (b) a first casted steel matrix material, wherein said carbide material is embedded in and bonded to said first casted steel matrix to form a wear resistant body; and (c) a second steel matrix, having a melting point at least 200 degrees F. greater than the melting point of said first steel matrix, wherein said wear resistant body is embedded in and bonded to said second steel matrix.
Claim 11
Dependent Claim 19 words
The wear resistant composite according to claim 8, wherein said second steel matrix substantially surrounds said wear resistant body.
Claim 12
Dependent Claim 27 words
The wear resistant composite according to claim 8, wherein said carbide material is in the form of crushed parts, powder or pressed bodies having an irregular shape.
Claim 13
Dependent Claim 28 words
The wear resistant composite according to claim 8, wherein said second steel matrix is a low carbon steel having a carbon content of less than 1.0 wt. %.
Claim 14
Dependent Claim 25 words
The wear resistant composite according to claim 11, wherein said second steel matrix has a hardness value of between 40 and 50 R c .
Claim 15
Dependent Claim 26 words
The wear resistant composite according to claim 11, wherein said low carbon second steel matrix has a melting point of between 2700 and 2800 degrees F.
Claim 16
Dependent Claim 18 words
The wear resistant composite according to claim 8, wherein said second steel matrix is more than 90% dense.
Claim 17
Dependent Claim 17 words
The wear resistant body according to claim 1, wherein said steel matrix is an austenitic manganese steel.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1994-11-18 1995-05-20 1995-11-19 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1998-11-18 1999-05-20 1999-11-19 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2002-11-18 2003-05-20 2003-11-19 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag