Abstract

Abstract An improved lightweight, ablative coating that may be spray applied and cured without the development of appreciable shrinkage cracks. The ablative mixture consists essentially of phenolic microballoons, hollow glass spheres, glass fibers, ground cork, a flexibilized resin binder, and an activated colloidal clay.

Inventors

  • 👤 William G. Simpson
  • 👤 Max H. Sharpe
  • 👤 William E. Hill

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-02 10:17
CPC Classifications
C; C08; C08J; C08J9/00; C08J9/32; C08J2363/00; Y; Y10; Y10S; Y10S521/00; Y10S521/907

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 86 words
A composition, consisting essentially of: approximately one-hundred (100) parts by weight of twenty-five (25) to sixty-five (65) percent by weight of phenolic microspheres, zero (0) to twenty (20) percent by weight of hollow glass spheres, four (4) to ten (10) percent by weight of glass fibers, twenty-five (25) to fifty (50) percent by weight of a flexibilized epoxy resin binder, and two (2) to six (6) percent by weight of an activated colloidal clay; and two-hundred (200) to four-hundred (400) parts by weight of a solvent.
Claim 2
Dependent Claim 86 words
A composition, consisting essentially of: approximately one-hundred (100) parts by weight of twenty-five (25) to sixty-five (65) percent by weight of phenolic microspheres, zero (0) to twenty (20) percent by weight of hollow glass spheres, four (4) to ten (10) percent by weight of glass fibers, twenty-five (25) to fifty (50) percent by weight of a flexibilized epoxy resin binder, and two (2) to six (6) percent by weight of an activated colloidal clay; and two-hundred (200) to four-hundred (400) parts by weight of a solvent.
Claim 3
Dependent Claim 111 words
A composition, consisting essentially of: approximately one-hundred (100) parts by weight of twenty (20) to fifty-five (55) percent by weight of phenolic microspheres, zero (0) to twenty (20) percent by weight of hollow glass spheres, four (4) to ten (10) percent by weight of glass fibers, two (2) to four (4) percent by weight of ground cork, twenty-five (25) to forty-five (45) percent by weight of a epoxy-modified polyurethane resin binder, and two (2) to six (6) percent by weight of an activated colloidal clay; one (1) to ten (10) parts by weight of an aromatic amine curing agent; and two-hundred (200) to four-hundred (400) parts by weight of a solvent.
Claim 4
Dependent Claim 111 words
A composition, consisting essentially of: approximately one-hundred (100) parts by weight of twenty (20) to fifty-five (55) percent by weight of phenolic microspheres, zero (0) to twenty (20) percent by weight of hollow glass spheres, four (4) to ten (10) percent by weight of glass fibers, two (2) to four (4) percent by weight of ground cork, twenty-five (25) to forty-five (45) percent by weight of a epoxy-modified polyurethane resin binder, and two (2) to six (6) percent by weight of an activated colloidal clay; one (1) to ten (10) parts by weight of an aromatic amine curing agent; and two-hundred (200) to four-hundred (400) parts by weight of a solvent.
Claim 5
Dependent Claim 96 words
A composition, consisting essentially of: approximately one-hundred (100) parts by weight of twenty-nine (29) to thirty-seven (37) percent by weight of phenolic microspheres, eleven (11) to fifteen (15) percent by weight of hollow glass spheres, four (4) to six (6) percent by weight of glass fibers, two (2) to four (4) percent by weight of ground cork, thirty-eight (38) to forty-eight (48) percent by weight of a flexibilized epoxy resin binder, and two (2) to six (6) percent by weight of activated colloidal clay; and two-hundred (200) to four-hundred (400) parts by weight of a solvent.
Claim 6
Dependent Claim 96 words
A composition, consisting essentially of: approximately one-hundred (100) parts by weight of twenty-nine (29) to thirty-seven (37) percent by weight of phenolic microspheres, eleven (11) to fifteen (15) percent by weight of hollow glass spheres, four (4) to six (6) percent by weight of glass fibers, two (2) to four (4) percent by weight of ground cork, thirty-eight (38) to forty-eight (48) percent by weight of a flexibilized epoxy resin binder, and two (2) to six (6) percent by weight of activated colloidal clay; and two-hundred (200) to four-hundred (400) parts by weight of a solvent.

References Cited (Backward Citations)

US3457215A Cited
US3755223A Cited
US4031059A Cited
US4077921A Cited
US4839394A Cited
US4772495A Cited
US4837250A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1994-11-11 1995-05-13 1995-11-12 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1998-11-11 1999-05-13 1999-11-12 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2002-11-11 2003-05-13 2003-11-12 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag