Abstract

Abstract I disclose a method for upgrading low-grade uintaite to high-grade uintaite having a desired meltpoint. It comprises dissolving the uintaite in a medium polarity solvent, mixing the dissolved uintaite with a nonpolar saturated hydrocarbon solvent at a volume-to-volume ratio that determines the meltpoint of the upgraded uintaite product, separating residual asphaltenes from the mixture, and recovering the medium polarity solvent and nonpolar saturated hydrocarbon to produce an upgraded uintaite having the desired meltpoint.

Inventors

  • 👤 Robert M. Carlson

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 03:17
CPC Classifications
C; C10; C10G; C10G1/00; C10G1/04

Claims Analysis

Total Claims: 12
Claim 1
Independent Claim 171 words
A method for upgrading uintaite to produce an upgraded uintaite product, comprising: (a) dissolving uintaite feed in a medium polarity solvent to produce a first mixture; (b) mixing said first mixture with a nonpolar saturated hydrocarbon solvent at a volume ratio of said first mixture to said nonpolar saturated hydrocarbon solvent to produce a second mixture comprising alight phase and a solid phase; (c) separating said solid phase containing residual asphaltenes from said second mixture to produce a light phase product; and (d) heating the light phase product of step (c) to recover said medium polarity solvent and said nonpolar saturated hydrocarbon solvent to produce an upgraded uintaite product having a lower meltpoint than the starting uintaite; wherein the relative proportion of said medium polarity solvent containing dissolved uintaite feed and said nonpolar solvent in said second mixture of step (b) is selected so that the meltpoint of said upgraded uintaite product of step (d) is about 30° C. to about 170° F. lower than the meltpoint of the unitaite feed.
Claim 2
Independent Claim 171 words
A method for upgrading uintaite to produce an upgraded uintaite product, comprising: (a) dissolving uintaite feed in a medium polarity solvent to produce a first mixture; (b) mixing said first mixture with a nonpolar saturated hydrocarbon solvent at a volume ratio of said first mixture to said nonpolar saturated hydrocarbon solvent to produce a second mixture comprising alight phase and a solid phase; (c) separating said solid phase containing residual asphaltenes from said second mixture to produce a light phase product; and (d) heating the light phase product of step (c) to recover said medium polarity solvent and said nonpolar saturated hydrocarbon solvent to produce an upgraded uintaite product having a lower meltpoint than the starting uintaite; wherein the relative proportion of said medium polarity solvent containing dissolved uintaite feed and said nonpolar solvent in said second mixture of step (b) is selected so that the meltpoint of said upgraded uintaite product of step (d) is about 30° C. to about 170° F. lower than the meltpoint of the unitaite feed.
Claim 3
Dependent Claim 40 words
A method, according to claim 1, further comprising: (e) dissolving the product of step (d) and a fraction of said solid phase recovered instep (c) in a medium polarity solvent in a weight ratio to produce a second uintaite product.
Claim 4
Dependent Claim 52 words
A method, according to claim 1, further comprising: (f) mixing the product of step (d) with a uintaite feed; (g) dissolving the uintaite mixture of step (f) in a medium polarity solvent; and (h) heating the mixture of step (g) to recover said medium polarity solvent to produce a second uintaite product.
Claim 5
Dependent Claim 26 words
A method, according to claim 1, 2, or 3, wherein said nonpolar saturated hydrocarbon solvent is selected from the group consisting of pentane, hexane and heptane.
Claim 6
Dependent Claim 33 words
A method, according to claim 1, wherein said nonpolar saturated hydrocarbon solvent is present in a ratio of at least 5 to 1 hydrocarbon solvent to medium polarity solvent containing dissolved uintaite feed.
Claim 7
Dependent Claim 15 words
A method, according to claim 5, wherein said ratio is at least 10 to 1.
Claim 8
Dependent Claim 15 words
A method, according to claim 6, wherein said ratio is at least 20 to 1.
Claim 9
Independent Claim 155 words
A method for upgrading uintaite, comprising: (a) dissolving uintaite feed in a refinery distillation cut comprising an aromatic hydrocarbon selected from the group consisting of benzene, toluene an xylene to produce a uintaite solution; (b) mixing the solution of step (a) with a nonpolar saturated hydrocarbon solvent comprising hexane, wherein said solvent is present in a ratio of about 20:1 solvent to solution to produce a mixture; (c) separating residual solid asphaltenes form the mixture of step (b) to produce a light phase; (d) heating the light phase of step (c) to recover said refinery distillation cut and said nonpolar saturated hydrocarbon solvent to produce a solid maltene fraction having a meltpoint of about 30° to 170° F. lower than the meltpoint of said uintaite feed, and (e) dissolving the maltene fraction of step (d) and a fraction of said asphaltenes recovered in step (c) in a medium polarity solvent to produce a uintaite product.
Claim 10
Independent Claim 155 words
A method for upgrading uintaite, comprising: (a) dissolving uintaite feed in a refinery distillation cut comprising an aromatic hydrocarbon selected from the group consisting of benzene, toluene an xylene to produce a uintaite solution; (b) mixing the solution of step (a) with a nonpolar saturated hydrocarbon solvent comprising hexane, wherein said solvent is present in a ratio of about 20:1 solvent to solution to produce a mixture; (c) separating residual solid asphaltenes form the mixture of step (b) to produce a light phase; (d) heating the light phase of step (c) to recover said refinery distillation cut and said nonpolar saturated hydrocarbon solvent to produce a solid maltene fraction having a meltpoint of about 30° to 170° F. lower than the meltpoint of said uintaite feed, and (e) dissolving the maltene fraction of step (d) and a fraction of said asphaltenes recovered in step (c) in a medium polarity solvent to produce a uintaite product.
Claim 11
Independent Claim 135 words
A method for upgrading uintaite, comprising: (a) dissolving uintaite feed in a medium polarity solvent comprising toluene to produce a solution; (b) mixing the solution of step (a) with a nonpolar saturated hydrocarbon solvent; (c) separating residual asphaltenes from the product of step (b) to produce a light phase; (d) dissolving a feed uintaite in a medium polarity solvent comprising toluene; (e) mixing the light phase of step (c) with the solution of step (d) at a volume ratio of said light phase to said dissolved feed uintaite to produce a uintaite mixture; (f) heating the mixture of step (e) to recover said medium polarity solvent and said nonpolar saturated hydrocarbon solvent to produce an ungraded uintaite product having a meltpoint of about 30° to 170° F. lower than the meltpoint of said uintaite feed.
Claim 12
Independent Claim 135 words
A method for upgrading uintaite, comprising: (a) dissolving uintaite feed in a medium polarity solvent comprising toluene to produce a solution; (b) mixing the solution of step (a) with a nonpolar saturated hydrocarbon solvent; (c) separating residual asphaltenes from the product of step (b) to produce a light phase; (d) dissolving a feed uintaite in a medium polarity solvent comprising toluene; (e) mixing the light phase of step (c) with the solution of step (d) at a volume ratio of said light phase to said dissolved feed uintaite to produce a uintaite mixture; (f) heating the mixture of step (e) to recover said medium polarity solvent and said nonpolar saturated hydrocarbon solvent to produce an ungraded uintaite product having a meltpoint of about 30° to 170° F. lower than the meltpoint of said uintaite feed.

References Cited (Backward Citations)

US2775292A Cited
US3558408A Cited
US3791956A Cited
US3929193A Cited
US4164466A Cited
US4312747A Cited
US4374015A Cited
US4539093A Cited
US4548701A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1994-09-09 1995-03-11 1995-09-10 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1998-09-09 1999-03-11 1999-09-10 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2002-09-09 2003-03-11 2003-09-10 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag