Abstract

Abstract Interlaminar grafting of coatings, particularly grafting of a lubricious outer coating upon an anchor coating supported upon glass or plastic, for example, to provide anti-fogging or lubricating characteristics. The method is characterized by its ability to anchor permanently the highly lubricious coating to the glass or plastic.

Inventors

  • 👤 Gregory Halpern
  • 👤 Charles Campbell
  • 👤 Ellington M. Beavers
  • 👤 Huk Y. Chen

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-25 19:38
CPC Classifications
C; C08; C08G; C08G18/00; C08G18/06; C08G18/08; C08G18/28; C08G18/40; C08G18/62; C08G18/6216; C08G18/622; C08G18/6225; C08G18/6229; C08G18/64; C08G18/6484; C08G18/70; C08G18/72; C08G18/728; C08J; C08J7/00; C08J7/04; C08J7/0427; C08J7/043; C08J7/054; C08J2475/00

Claims Analysis

Total Claims: 11
Claim 1
Independent Claim 112 words
Method of interlaminar grafting of continuous coatings upon an object, the coatings being different and not mutually soluble, the method comprising the steps of: a) first coating the object with a solution containing an acrylic polymer and a solvent; b) removing the solvent, so as to form a first continuous film which manifests a high degree of adhesion to the object; c) second coating the object with an aqueous solution of sodium hyaluronate; d) removing water from said second coating, so as to form a second continuous film; and e) heating said first and second films, so as to effect interlaminar grafting between the films, wherein both films retain their individual integrity.
Claim 2
Dependent Claim 112 words
Method of interlaminar grafting of continuous coatings upon an object, the coatings being different and not mutually soluble, the method comprising the steps of: a) first coating the object with a solution containing an acrylic polymer and a solvent; b) removing the solvent, so as to form a first continuous film which manifests a high degree of adhesion to the object; c) second coating the object with an aqueous solution of sodium hyaluronate; d) removing water from said second coating, so as to form a second continuous film; and e) heating said first and second films, so as to effect interlaminar grafting between the films, wherein both films retain their individual integrity.
Claim 3
Dependent Claim 18 words
Method of interlaminar grafting of coatings upon an object as in claim 1 wherein the object is plastic.
Claim 4
Dependent Claim 129 words
Method of interlaminar grafting of continuous coatings upon an object, the coatings being different and not mutually soluble, the method comprising the steps of: a) first coating the object with a solution of an acrylic co-polymer of ethylmethacrylate and isocyanatoethyl methacrylate; b) removing the solvent so as to form a first continuous film which manifests a high degree of adhesion to the object; c) second coating the object with an aqueous solution of sodium hyaluronate; d) removing water from said second coating so as to form a second continuous film; and e) heating said first and second films so as to effect interlaminar grafting in which isocyanate groups in said first film react with hydroxyl groups in said second film of hyaluronate, wherein both films retain their individual integrity.
Claim 5
Dependent Claim 129 words
Method of interlaminar grafting of continuous coatings upon an object, the coatings being different and not mutually soluble, the method comprising the steps of: a) first coating the object with a solution of an acrylic co-polymer of ethylmethacrylate and isocyanatoethyl methacrylate; b) removing the solvent so as to form a first continuous film which manifests a high degree of adhesion to the object; c) second coating the object with an aqueous solution of sodium hyaluronate; d) removing water from said second coating so as to form a second continuous film; and e) heating said first and second films so as to effect interlaminar grafting in which isocyanate groups in said first film react with hydroxyl groups in said second film of hyaluronate, wherein both films retain their individual integrity.
Claim 6
Dependent Claim 20 words
Method of interlaminar grafting of coatings upon an object as in claim 3, wherein the object is an intra-ocular lens.
Claim 7
Dependent Claim 165 words
Method of interlaminar grafting of continuous coatings upon an object, the coatings being different and not mutually soluble, the method comprising the steps of: a) first coating the object with a solution in methoxypropyl acetate prepared from: i) a copolymer of ethyl methacrylate, butylacrylate and hydroxyethyl methacrylate, and ii) polyisocyanate in sufficient quantity to represent 1.25 equivalents of isocyanate per hydroxyl equivalent in said polymer; b) heating so as to evaporate solvent and enable formation of a prepolymer so as to form a first continuous film which manifests a high degree of adhesion to the object; c) second coating the object with an aqueous solution of sodium hyaluronate; d) removing water from the said second coating aqueous solution so as to form a second continuous film; and e) heating said first and second films, so as to effect interlaminar grafting such that the hydroxyl groups in said second film hyaluronate react with said first film isocyanate groups, and wherein both films retain their individual integrity.
Claim 8
Dependent Claim 165 words
Method of interlaminar grafting of continuous coatings upon an object, the coatings being different and not mutually soluble, the method comprising the steps of: a) first coating the object with a solution in methoxypropyl acetate prepared from: i) a copolymer of ethyl methacrylate, butylacrylate and hydroxyethyl methacrylate, and ii) polyisocyanate in sufficient quantity to represent 1.25 equivalents of isocyanate per hydroxyl equivalent in said polymer; b) heating so as to evaporate solvent and enable formation of a prepolymer so as to form a first continuous film which manifests a high degree of adhesion to the object; c) second coating the object with an aqueous solution of sodium hyaluronate; d) removing water from the said second coating aqueous solution so as to form a second continuous film; and e) heating said first and second films, so as to effect interlaminar grafting such that the hydroxyl groups in said second film hyaluronate react with said first film isocyanate groups, and wherein both films retain their individual integrity.
Claim 9
Dependent Claim 26 words
Method of interlaminar grafting of coatings upon an object as in claim 5, wherein said second coating is a solution of 0.1% to 2% sodium hyaluronate.
Claim 10
Dependent Claim 22 words
Method of interlaminar grafting of coatings upon an object as in claim 5, wherein said hydroxyethyl methacrylate is 10 to 25 mole-percent.
Claim 11
Dependent Claim 36 words
Method of interlaminar grafting of coatings upon an object as in claim 5, wherein said polyisocyanate is added in sufficient quantity to represent 1.1 to 2 equivalents of isocyanate per hydroxyl equivalent in said acrylic copolymer.

References Cited (Backward Citations)

US4280954A Cited
US4487865A Cited
US4500676A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1994-08-05 1995-02-04 1995-08-06 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1998-08-05 1999-02-04 1999-08-06 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2002-08-05 2003-02-04 2003-08-06 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag