US5035363A Expired / Lapsed US ⏱️ 0.0 years remaining

Ultrasonic grinding of explosives

Assignee: Northrop Grumman Innovation Systems LLC
•
Filing: 1990-07-06
•
Granted: 1991-07-30
•
Expires: 2010-07-06
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract The particle size of energetic explosive materials is reduced by slurrying the particulate explosive materials in an inert liquid such as water or an aqueous solution, and subjecting the slurry to intense acoustic cavitation from an ultrasonic generator for a short time. The particulate explosive materials are rapidly ground to a small particle size while minimizing the danger of detonation.

Inventors

  • 👤 Carlos Somoza

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 02:48
CPC Classifications
B; B02; B02C; B02C23/00; B02C23/18; B02C19/00; B02C19/18

Claims Analysis

Total Claims: 12
Claim 1
Independent Claim 71 words
A method for reducing the particle size of particulate explosive material, comprising: adding said particulate explosive material to an inert liquid to form a slurry thereof; subjecting said slurrry to treatment proximate an ultrasonic generator wherein acoustic cavitation in said inert liquid abrades and grinds said particulate explosive material to a reduced particle size, without detonation thereof; and separating said particulate explosive material of reduced particle size from said inert liquid.
Claim 2
Independent Claim 71 words
A method for reducing the particle size of particulate explosive material, comprising: adding said particulate explosive material to an inert liquid to form a slurry thereof; subjecting said slurrry to treatment proximate an ultrasonic generator wherein acoustic cavitation in said inert liquid abrades and grinds said particulate explosive material to a reduced particle size, without detonation thereof; and separating said particulate explosive material of reduced particle size from said inert liquid.
Claim 3
Dependent Claim 15 words
The method of claim 1, wherein said inert liquid is water or an aqueous solution.
Claim 4
Dependent Claim 17 words
The method of claim 1, wherein said ultrasonic generator is operated at a frequency of 14-60 KHz.
Claim 5
Dependent Claim 17 words
The method of claim 1, wherein said ultrasonic generator is operated at a frequency of 14-30 KHz.
Claim 6
Dependent Claim 26 words
The method of claim 1, wherein said ultrasonic generator is operated at a power output intensity of at least 70 watts/square centimeter of generator tip area.
Claim 7
Dependent Claim 28 words
The method of claim 1, wherein said ultrasonic generator is operated at a power output intensity of 70 to 120 watts per square centimeter of generator tip area.
Claim 8
Dependent Claim 17 words
The method of claim 1, wherein said aqueous liquid includes an additive for increasing the grinding rate.
Claim 9
Dependent Claim 30 words
The method of claim 1, comprising the further step of cooling said slurry before and/or during said passage proximate and ultrasonic generator to maintain a temperature below 50 degrees C.
Claim 10
Dependent Claim 14 words
The method of claim 1, wherein said explosive material comprises RDX, HMX, or CPX.
Claim 11
Independent Claim 91 words
A method for reducing the particle size of a particulate explosive material, comprising: adding said particulate explosive material to an inert aqueous liquid to form a slurry thereof; passing said slurry in a continuous stream past an ultrasonic generator wherein acoustic cavitation in said inert aqueous liquid abrades and grinds said particulate explosive material to a reduced particle size without detonation thereof; discharging a stream of said particulate material of reduced particle size to a separation means; and separating said particulate material of reduced particle size from said inert aqueous liquid.
Claim 12
Independent Claim 91 words
A method for reducing the particle size of a particulate explosive material, comprising: adding said particulate explosive material to an inert aqueous liquid to form a slurry thereof; passing said slurry in a continuous stream past an ultrasonic generator wherein acoustic cavitation in said inert aqueous liquid abrades and grinds said particulate explosive material to a reduced particle size without detonation thereof; discharging a stream of said particulate material of reduced particle size to a separation means; and separating said particulate material of reduced particle size from said inert aqueous liquid.

References Cited (Backward Citations)

US2204059A Cited
US3770721A Cited
US3239502A Cited
US3351585A Cited
US3600477A Cited
US4156593A Cited
US4572439A Cited
US4767064A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1994-07-29 1995-01-28 1995-07-30 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1998-07-29 1999-01-28 1999-07-30 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2002-07-29 2003-01-28 2003-07-30 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag